公开(公告)号:US11332594B2
公开(公告)日:2022-05-17
申请号:US17031188
申请日:2020-09-24
Applicant: BASF SE
Inventor: Frank Prissok , Frank Braun
IPC: C08J9/16 , C08J9/232 , C08J9/18 , A43B13/04 , A43B13/18 , A43B17/14 , C08G18/48 , C08L75/04 , B29B9/06 , B29B9/12 , B29B9/14 , B29B9/16 , A43B13/02 , C08G18/10 , C08G18/76 , C08J3/12 , C08J9/14 , C08G101/00 , C08K3/32
Abstract: Expandable thermoplastic polyurethane comprising blowing agent, wherein the Shore hardness of the thermoplastic polyurethane is from A 44 to A 84.
-
公开(公告)号:US20210403669A1
公开(公告)日:2021-12-30
申请号:US17472632
申请日:2021-09-11
Applicant: BASF SE
Inventor: Frank Prissok , Frank Braun
IPC: C08J9/16 , C08J9/232 , C08J9/18 , A43B13/04 , A43B13/18 , A43B17/14 , C08G18/48 , C08L75/04 , B29B9/06 , B29B9/12 , B29B9/14 , B29B9/16 , A43B13/02 , C08G18/10 , C08G18/76 , C08J3/12 , C08J9/14
Abstract: A process can be used for recycling foams based on thermoplastic polyurethane.
-
公开(公告)号:US20210380805A1
公开(公告)日:2021-12-09
申请号:US17286827
申请日:2019-10-22
Applicant: BASF SE
Inventor: Frank Prissok , Florian Puch , Elmar Poeselt
Abstract: A thermoplastic polyamide can be obtained through the reaction of at least the components (i), (ii), and (iii), where a catalyst having a Lewis base component is used in the reaction. Component (i) is a composition containing a polymeric compound having two carboxylic acid moieties; component (ii) is a dicarboxylic acid composition containing at least one dicarboxylic acid; and component (iii) is a diisocyanate composition containing at least one diisocyanate. A process can be used for producing the thermoplastic polyamide and a method for the use thereof. A tandem reactive extruder can be used for the reaction.
-
公开(公告)号:US11142621B2
公开(公告)日:2021-10-12
申请号:US15837344
申请日:2017-12-11
Applicant: BASF SE
Inventor: Frank Prissok , Frank Braun
IPC: C08J9/16 , C08J9/232 , C08J9/18 , A43B13/04 , A43B13/18 , A43B17/14 , C08G18/48 , C08L75/04 , B29B9/06 , B29B9/12 , B29B9/14 , B29B9/16 , A43B13/02 , C08G18/10 , C08G18/76 , C08J3/12 , C08J9/14 , C08G101/00 , C08K3/32
Abstract: Expandable thermoplastic polyurethane comprising blowing agent, wherein the Shore hardness of the thermoplastic polyurethane is from A 44 to A 84.
-
公开(公告)号:US11124620B2
公开(公告)日:2021-09-21
申请号:US17031164
申请日:2020-09-24
Applicant: BASF SE
Inventor: Frank Prissok , Frank Braun
IPC: C08J9/16 , C08J9/232 , C08J9/18 , A43B13/04 , A43B13/18 , A43B17/14 , C08G18/48 , C08L75/04 , B29B9/06 , B29B9/12 , B29B9/14 , B29B9/16 , A43B13/02 , C08G18/10 , C08G18/76 , C08J3/12 , C08J9/14 , C08G101/00 , C08K3/32
Abstract: Expandable thermoplastic polyurethane comprising blowing agent, wherein the Shore hardness of the thermoplastic polyurethane is from A 44 to A 84.
-
公开(公告)号:US10941263B2
公开(公告)日:2021-03-09
申请号:US15307134
申请日:2015-04-14
Applicant: BASF SE
Inventor: Frank Prissok , Michael Harms , Martin Vallo
IPC: C08J7/04 , C08J9/36 , C08G18/48 , C08G18/32 , C08J9/228 , C08G18/66 , B05D1/02 , B05D1/18 , B05D1/28 , C08G18/76 , C09D175/04
Abstract: The present invention relates to coated shaped articles comprising at least one shaped article comprising foamed beads comprising at least one polyurethane (A) and at least one coating comprising at least one polyurethane (B), wherein polyurethane (A) and polyurethane (B) are each constructed from at least one polyol and at least one polyisocyanate and wherein not less than 50 wt % of the polyol component used for constructing polyurethane (A) and polyurethane (B) is identical and not less than 50 wt % of the at least one polyisocyanate component used for constructing polyurethane (A) and polyurethane (B) is identical. The present invention further relates to processes for producing the coated shaped articles of the present invention and also to the method of using the coated shaped articles of the present invention for various applications.
-
公开(公告)号:US10329370B2
公开(公告)日:2019-06-25
申请号:US14890847
申请日:2014-05-08
Applicant: BASF SE
Inventor: Frank Prissok , Andre Kamm
IPC: C08G18/00 , C08G18/10 , C08G18/20 , C09D175/04
Abstract: The present invention relates to a method for producing at least one resin, which comprises mixing at least one polyisocyanate with at least one polyepoxide, the reaction taking place in the presence of a catalyst system based on at least one metal-free Lewis base having at least one nitrogen atom, and also to resins obtainable by a method of the invention, and to the use of a resin obtainable by a method of the invention, or of a resin of the invention, for producing seals, for producing components for rotor blades, boat hulls, or vehicle body parts, or for coatings.
-
公开(公告)号:US10279516B2
公开(公告)日:2019-05-07
申请号:US14897746
申请日:2014-06-11
Applicant: BASF SE
Inventor: Christian Däschlein , Peter Gutmann , Frank Prissok , Uwe Keppeler , Jürgen Ahlers
IPC: B29C44/34 , B29B9/06 , C08J9/16 , B29B9/12 , B29C44/04 , C08J9/00 , C08J9/12 , C08J9/34 , B29B7/88 , B29B7/90 , B29B9/14 , B29C47/00 , B29C47/86 , B29K21/00 , B29K77/00 , B29K105/00 , B29K105/16
Abstract: A process for producing expanded pellets from a thermoplastic elastomer having an elongation at break of more than 100% measured to DIN EN ISO 527-2, comprising: (a) pressing a polymer melt comprising a blowing agent through a perforated disk (18) controlled to a temperature between 150° C. and 280° C. and into a pelletizing chamber (26), (b) using a cutting device (20) to comminute the polymer melt pressed through the perforated disk (18) into individual expanding pellets, (c) discharging the pellets from the pelletizing chamber (26) using a liquid stream (36), wherein the blowing agent comprises CO2 and/or N2 and the amount of blowing agent in the polymer melt is from 0.5 to 2.5 wt %, the pelletizing chamber (26) is traversed by a stream of liquid at a temperature between 5° C. and 90° C. and the pressure of 0.1 bar to 20 bar above ambient pressure such that the pellets are expanded in the pressurized liquid by the blowing agent, producing expanded pellets having an uninterrupted skin.
-
公开(公告)号:US09562131B2
公开(公告)日:2017-02-07
申请号:US13969837
申请日:2013-08-19
Applicant: BASF SE
Inventor: Frank Prissok , Julio Albuerne , Christian Renner
IPC: C08G18/18 , C08G18/20 , C08G18/32 , C08G18/34 , C08G101/00
CPC classification number: C08G18/1825 , C08G18/1833 , C08G18/1858 , C08G18/2027 , C08G18/3206 , C08G18/341 , C08G2101/0025 , C08G2101/005
Abstract: The present invention relates to a process for producing a thermoformable rigid polyurethane-polyamide foam having a closed-cell content of less than 70%, which comprises mixing (a) an organic polyisocyanate with (b) one or more polymeric compounds having two or more isocyanate-reactive hydrogen atoms, (c) optionally crosslinking and/or chain-extending agents, (d) one or more carboxylic acids having a functionality of 2 or more, (e) a catalyst comprising a Lewis base component, and (f) optionally auxiliaries and additives to form a reaction mixture and reacting this reaction mixture to form the rigid polyurethane-polyamide foam. The present invention further relates to a thermoformable rigid polyurethane-polyamide foam obtained by such a process and also to the use of such a thermoformable rigid polyurethane-polyamide foam for interior lining or engine compartment lining of motor vehicles.
Abstract translation: 本发明涉及一种具有小于70%的闭孔含量的可热成形的硬质聚氨酯 - 聚酰胺泡沫体的制造方法,该方法包括将(a)有机多异氰酸酯与(b)一种或多种具有两个或多个 异氰酸酯反应性氢原子,(c)任选交联和/或增链剂,(d)一种或多种官能度为2或更大的羧酸,(e)包含路易斯碱组分的催化剂,和(f) 任选的助剂和添加剂以形成反应混合物并使该反应混合物反应形成刚性聚氨酯 - 聚酰胺泡沫体。 本发明还涉及通过这种方法获得的可热成型的刚性聚氨酯 - 聚酰胺泡沫,并且还涉及使用这种可热成型的硬质聚氨酯 - 聚酰胺泡沫用于机动车辆的内衬或发动机隔间衬里。
-
公开(公告)号:US20150174808A1
公开(公告)日:2015-06-25
申请号:US14391870
申请日:2013-04-12
Applicant: BASF SE
Inventor: Hans Rudolph , Rainer Klostermann , Torben Kaminsky , Bernd Lohaus , Jürgen Ahlers , Bernhard Schmied , Peter Gutmann , Klaus Hahn , Frank Prissok , Elke Marten , Christian Däschlein
IPC: B29C47/00
CPC classification number: B29C47/0011 , B29B9/065 , B29B9/12 , B29B9/14 , B29B9/16 , B29C44/3461 , B29K2075/00 , B29L2031/00 , C08G18/0895 , C08G18/6674 , C08G18/7671 , C08J9/122 , C08J9/141 , C08J9/16 , C08J9/34 , C08J2201/03 , C08J2203/06 , C08J2203/14 , C08J2203/182 , C08J2300/22 , C08J2367/00 , C08J2375/04 , C08J2377/00
Abstract: The invention relates to a process for production of expanded pellets from a polymer melt comprising a blowing agent, said process comprising the steps of: a) pressing the polymer melt comprising a blowing agent through a perforated disk controlled to a temperature between 150° C. and 280° C. and into a pelletizing chamber, b) using a cutting device to comminute the polymer melt pressed through the temperature-controlled perforated disk into individual expanding pellets, c) discharging the pellets from the pelletizing chamber using a liquid stream, wherein the blowing agent comprises CO2 or N2 or a combination of CO2 and N2 and the pelletizing chamber is traversed by a stream of liquid which is controlled to a temperature between 10° C. and 60° C. and the pressure of which is from 0.7 bar to 20 bar above ambient pressure, the pressure and temperature for the liquid in the pelletizing chamber and also the temperature for the perforated disk being chosen such that the pellets are expanded in the pressurized liquid by the blowing agent they contain so as to produce expanded pellets having an uninterrupted skin.
Abstract translation: 本发明涉及一种由包含发泡剂的聚合物熔体制备发泡颗粒的方法,所述方法包括以下步骤:a)将包含发泡剂的聚合物熔体通过控制在150℃之间的多孔板压制 和280℃,并且进入造粒室,b)使用切割装置将通过温度控制的多孔盘压制的聚合物熔体粉碎成单独的膨胀颗粒,c)使用液体流将颗粒从造粒室排出,其中 发泡剂包括CO 2或N 2或CO 2和N 2的组合,并且造粒室通过液体流穿过,该液流被控制在10℃和60℃之间的温度,其压力为0.7巴 在环境压力以上20巴以下,选择造粒室中的液体的压力和温度以及多孔盘的温度,使得颗粒为exp 通过它们包含的发泡剂将其加压在加压液体中以产生具有不间断皮肤的发泡颗粒。
-
-
-
-
-
-
-
-
-