41.
    发明专利
    未知

    公开(公告)号:NO952801D0

    公开(公告)日:1995-07-14

    申请号:NO952801

    申请日:1995-07-14

    Applicant: BAXTER INT

    Abstract: A polymer based composition for fabricating into articles is described. The composition comprises: a polypropylene in an amount by weight from 40-90% of the composition and having a melting temperature greater than 130 DEG C; a radio frequency susceptible polymer in an amount by weight from 5-50% of the composition and having a dielectric loss greater than 0.05 at 1-60 MHz and ambient temperature to 250 DEG C, the susceptible polymer being selected from (1) polymers containing at least one segment selected from the group consisting of urethanes, esters, ureas, imides, sulfones, and amides, and (2) ethylene copolymers having 50-85% ethylene content copolymerized with at least one monomer selected from the group consisting of acrylic acid, methacrylic acid, ester derivatives of acrylic acid with alcohols having 1-10 carbons, vinyl acetate, and vinyl alcohol; a compatibilizing polymer in an amount by weight from 5-30% of the composition, the compatibilizing polymer conferring compatibility between the radio frequency susceptible polymer, and the polypropylene, the compatibilizing polymer being a styrenic block copolymer with hydrocarbon soft segments, and wherein the composition has an optical haze value of less than 30% for the composition processed into a film of about 0.299 mm in thickness measured in accordance to ASTM D-1003, a mechanical modulus of less than 2758x10 Pa when measured according to ASTM D-882 and the composition exhibits no strain whitening after being strained at moderate speeds of about 50 cm per minute to about 100% elongation.

    43.
    发明专利
    未知

    公开(公告)号:DE69921396D1

    公开(公告)日:2004-12-02

    申请号:DE69921396

    申请日:1999-01-25

    Applicant: BAXTER INT

    Abstract: A steam sterilizable monolayer medical tubing comprising a blend of a melt strength enhancing agent of a homopolymer or copolymer of polypropylene having free-end long chain branches of propylene units, a melt flow index of greater than 10 and in an amount of 1-10% by weight and a second component selected from the group of (i) a selectively hydrogenated block copolymer of a vinyl aromatic hydrocarbon and a conjugated diene and (ii) a selectively hydrogenated block copolymer of a vinyl aromatic hydrocarbon and a conjugated diene to which has been grafted, an alpha, beta-olenfically unsaturated monocarboxylic or dicarboxylic acid reagent.

    50.
    发明专利
    未知

    公开(公告)号:BR9405786A

    公开(公告)日:1996-03-26

    申请号:BR9405786

    申请日:1994-11-16

    Applicant: BAXTER INT

    Abstract: A polymer based composition for fabricating into articles is described. The composition comprises: a polypropylene in an amount by weight from 40-90% of the composition and having a melting temperature greater than 130 DEG C; a radio frequency susceptible polymer in an amount by weight from 5-50% of the composition and having a dielectric loss greater than 0.05 at 1-60 MHz and ambient temperature to 250 DEG C, the susceptible polymer being selected from (1) polymers containing at least one segment selected from the group consisting of urethanes, esters, ureas, imides, sulfones, and amides, and (2) ethylene copolymers having 50-85% ethylene content copolymerized with at least one monomer selected from the group consisting of acrylic acid, methacrylic acid, ester derivatives of acrylic acid with alcohols having 1-10 carbons, vinyl acetate, and vinyl alcohol; a compatibilizing polymer in an amount by weight from 5-30% of the composition, the compatibilizing polymer conferring compatibility between the radio frequency susceptible polymer, and the polypropylene, the compatibilizing polymer being a styrenic block copolymer with hydrocarbon soft segments, and wherein the composition has an optical haze value of less than 30% for the composition processed into a film of about 0.299 mm in thickness measured in accordance to ASTM D-1003, a mechanical modulus of less than 2758x10 Pa when measured according to ASTM D-882 and the composition exhibits no strain whitening after being strained at moderate speeds of about 50 cm per minute to about 100% elongation.