Abstract:
A method of manufacturing an optical waveguide preform includes providing a first process gas atmosphere to a soot preform contained in a vessel. The first atmosphere is held in the vessel for a first reacting time sufficient to at least partially dope or dry the soot preform. The vessel is then at least partially refilled with a second doping or drying atmosphere. The second doping or drying atmosphere is held in the vessel for a second reacting time sufficient to further dope or dry the soot preform.