43.
    发明专利
    未知

    公开(公告)号:DE69633662D1

    公开(公告)日:2004-11-25

    申请号:DE69633662

    申请日:1996-03-14

    Abstract: A method for producing a formed product of deproteinized natural rubber latex capable of reducing a content of an allergen in a natural rubber latex material to a level sufficient to keep the latex from being harmful to the human body without decreasing yields of the product and deteriorating formability of the latex. In the method, cleaning removal of a non-rubber content is carried out after each of protein decomposition, prevulcanization and forming. An aqueous alkali solution, ammonia, water containing free chlorine in an amount of 0.005 to 0.02% by weight or alcohol-water mixed liquid containing alcohol in an amount of 5 to 80% by weight is used as cleaning liquid for the cleaning removal. The method is suitably applied to production of a natural rubber product such as a rubber glove, a condom, a catheter, a foam rubber material and the like.

    46.
    发明专利
    未知

    公开(公告)号:ES2106404T3

    公开(公告)日:1997-11-01

    申请号:ES94107308

    申请日:1994-05-10

    Abstract: A process for producing raw rubber from a deproteinized natural rubber is disclosed, which comprises coagulating rubber particles in the deproteinized natural rubber latex by: (1) adding a nonionic surfactant having a cloud point of from 20 to 100 DEG C and a molecular weight of 300 or more to the deproteinized natural rubber latex and heating the latex to a temperature not lower than the cloud point of the nonionic surfactant; or (2) adding a coagulation assistant selected from the group consisting of: (a) an anionic surfactant, (b) an amphoteric surfactant, (c) a nonionic surfactant, (d) a nonionic or amphoteric oligomer or polymer, and (e) an anionic oligomer or polymer, to the deproteinized natural rubber latex; and then recovering the coagulated rubber particles. According to the process of the present invention, raw rubber containing substantially no metal ion can be produced with a high efficiency.

    47.
    发明专利
    未知

    公开(公告)号:BR9509816A

    公开(公告)日:1997-09-30

    申请号:BR9509816

    申请日:1995-11-22

    Applicant: KAO CORP

    Abstract: PCT No. PCT/JP95/02382 Sec. 371 Date May 22, 1997 Sec. 102(e) Date May 22, 1997 PCT Filed Nov. 22, 1995 PCT Pub. No. WO96/16539 PCT Pub. Date Jun. 6, 1996An adjuvant composition for agricultural chemicals comprising at least one sorbitan/fatty acid ester surfactant (A) and at least one surfactant (B) selected from the group consisting of resin acid surfactants and anionic oligomer or polymer type quaternary ammonium salt surfactants can be used for various crops in safety without causing injury thereof to the crops, and can enhance the efficacies of various agricultural chemicals.

    48.
    发明专利
    未知

    公开(公告)号:DE69404740D1

    公开(公告)日:1997-09-11

    申请号:DE69404740

    申请日:1994-05-10

    Abstract: A process for producing raw rubber from a deproteinized natural rubber is disclosed, which comprises coagulating rubber particles in the deproteinized natural rubber latex by: (1) adding a nonionic surfactant having a cloud point of from 20 to 100 DEG C and a molecular weight of 300 or more to the deproteinized natural rubber latex and heating the latex to a temperature not lower than the cloud point of the nonionic surfactant; or (2) adding a coagulation assistant selected from the group consisting of: (a) an anionic surfactant, (b) an amphoteric surfactant, (c) a nonionic surfactant, (d) a nonionic or amphoteric oligomer or polymer, and (e) an anionic oligomer or polymer, to the deproteinized natural rubber latex; and then recovering the coagulated rubber particles. According to the process of the present invention, raw rubber containing substantially no metal ion can be produced with a high efficiency.

    Process for producing raw rubber
    50.
    发明专利

    公开(公告)号:AU666267B2

    公开(公告)日:1996-02-01

    申请号:AU6307094

    申请日:1994-05-12

    Abstract: A process for producing raw rubber from a deproteinized natural rubber is disclosed, which comprises coagulating rubber particles in the deproteinized natural rubber latex by: (1) adding a nonionic surfactant having a cloud point of from 20 to 100 DEG C and a molecular weight of 300 or more to the deproteinized natural rubber latex and heating the latex to a temperature not lower than the cloud point of the nonionic surfactant; or (2) adding a coagulation assistant selected from the group consisting of: (a) an anionic surfactant, (b) an amphoteric surfactant, (c) a nonionic surfactant, (d) a nonionic or amphoteric oligomer or polymer, and (e) an anionic oligomer or polymer, to the deproteinized natural rubber latex; and then recovering the coagulated rubber particles. According to the process of the present invention, raw rubber containing substantially no metal ion can be produced with a high efficiency.