PAI-PTM 부직포에 탄화수소계 고분자 전해질을 함침시켜 제조한 복합막 및 이의 용도
    52.
    发明公开
    PAI-PTM 부직포에 탄화수소계 고분자 전해질을 함침시켜 제조한 복합막 및 이의 용도 有权
    包含非挥发性PAI-PTM和磺化聚(亚乙基醚)的复合膜作为基于碳氢化合物的电解质及其用途

    公开(公告)号:KR1020150126504A

    公开(公告)日:2015-11-12

    申请号:KR1020140053501

    申请日:2014-05-02

    CPC classification number: Y02P70/56 H01M8/1027 C08J5/22 H01M8/02 H01M8/10

    Abstract: 본발명은폴리(아미드-코-이미드)(poly(amide-co-imide); PAI) 수지및 폴리(트리멜리틱언하이드라이드클로라이드-코-4,4'-메틸렌디아닐린)(poly(trimellitic anhydride chloride-co-4,4'-methylenedianiline); PTM) 수지혼합물을포함하는용액을전기방사하여제조한 PAI-PTM 부직포및 이에함침시킨탄화수소계고분자전해질을포함하는복합막(composite membrane), 상기복합막을구비한막-전극접합체(membrane-electrode assembly; MEA) 및상기막-전극접합체를구비한연료전지에관한것이다.

    Abstract translation: 本发明涉及通过静电纺丝含有聚(酰胺 - 酰亚胺)(PAI)树脂和聚(偏苯三酸酐氯化物 - 共-4,4'-亚甲基二苯胺)(PTM))的溶液制备的PAI-PTM无纺布, 树脂化合物和包含浸渍在其中的烃类聚合物电解质的复合膜,包含复合膜的膜 - 电极组件(MEA)和包括MEA的燃料电池。

    부분 가지형 블록 공중합체를 포함하는 이온전도성 고분자 및 이의 용도
    53.
    发明授权
    부분 가지형 블록 공중합체를 포함하는 이온전도성 고분자 및 이의 용도 有权
    包含部分支化的多嵌段共聚物的离子导电聚合物及其用途

    公开(公告)号:KR101546816B1

    公开(公告)日:2015-08-25

    申请号:KR1020120126980

    申请日:2012-11-09

    Abstract: 본발명은부분가지형블록공중합체를포함하는이온전도성고분자; 이의제조방법; 상기이온전도성고분자를포함하는이온전도체; 상기이온전도체를전해질막또는분리막으로사용한전지에관한것이다. 구체적으로는상기부분가지형블록공중합체는친수성제1 고분자로된 제1 블록; 주사슬상에곁가지를형성하는분기점(branching point)을형성하도록양 말단에각각 2개이상의반응기를갖는소수성제2 고분자로부터유래된제2 블록; 및선택적으로소수성제3 고분자로된 제3 블록을포함한다.

    Abstract translation: 本发明涉及包含部分支化的嵌段共聚物的离子导电聚合物; 其制备方法; 包括离子导电聚合物的离子导体; 包括离子导电聚合物的电解质膜; 包括电解膜的膜 - 电极组件和包含该电解质膜的电池组; 以及包含离子导电聚合物的氧化还原液流电池用分离膜和包含该离子导电性聚合物的氧化还原液流电池。 具体地说,部分支化的嵌段共聚物包括:包含亲水性第一聚合物的第一嵌段; 衍生自在其两端分别具有两个或更多个反应性基团的疏水性第二聚合物的第二嵌段,以形成在主链上形成侧枝的分支点; 和任选的包含疏水性第三聚合物的第三嵌段。 部分支链嵌段共聚物形式的离子导电聚合物可制备具有相同或相似离子交换容量(IEC)的导电性和优异物理性能如断裂拉伸强度伸长率等的聚合物膜, 与以直链嵌段共聚物形式的常规离子导电聚合物相比,吸水率和/或尺寸变化程度相当。 由于具有这样优异的物理性能,聚合物膜可以用作燃料电池的膜 - 电极组件,并且包含其的分离膜的氧化还原液流电池可以表现出优异的电池性能并且甚至保持高的放电充电容量保持率 反复充放电多次。

    고분자 전해질용 막-전극 어셈블리의 제조방법 및 그로부터 제조되는 막-전극 어셈블리
    55.
    发明公开
    고분자 전해질용 막-전극 어셈블리의 제조방법 및 그로부터 제조되는 막-전극 어셈블리 有权
    因此,用于聚合物电解质和膜 - 电极组件的膜 - 电极组装的制造方法

    公开(公告)号:KR1020120126302A

    公开(公告)日:2012-11-21

    申请号:KR1020110043992

    申请日:2011-05-11

    Abstract: PURPOSE: A manufacturing method of membrane-electrode assembly for polyelectrolyte and a membrane-electrode assembly manufactured from the same are provided to resolve problems generated by deterioration of electrolyte membrane. CONSTITUTION: A manufacturing method of membrane-electrode assembly for polyelectrolyte comprises the following steps: forming a catalyst layer by coating a release film with catalyst slurry in which catalyst, proton-conducting polymer and dispersion medium and drying thereof; laminating the catalyst layer formed on the release film on both sides of a transmitted film for the catalyst layer to direct in the electrolyte film direction; and transferring the catalyst layer to the electrolyte film by hot-pressing the laminated body. [Reference numerals] (AA) Catalyst slurry coating; (BB) Catalyst layers laminating; (CC) Hot pressing(T=50-200 deg. Celsius, P=5-75 kgf/cm^2); (DD) Release film removal; (EE) Introductory remark; (FF) Release film; (GG) Catalyst layer; (HH) Electrolyte film; (II) Second release film; (JJ) Silicon rubber layer; (KK) Steel plate; (LL) Dry; (S1) Forming the catalyst layer on the release film; (S2) Laminating on both sides of the electrolyte film; (S3) Transcribing the catalyst layer to the electrolyte film; (S4) Removing the release film and solvent

    Abstract translation: 目的:提供一种聚电解质膜电极接合体的制造方法及其制造的膜 - 电极接合体,以解决由电解质膜的劣化而产生的问题。 构成:聚电解质膜电极组件的制造方法包括以下步骤:通过用其中催化剂,质子传导性聚合物和分散介质及其干燥的催化剂浆料涂布脱模膜形成催化剂层; 将形成在剥离膜上的催化剂层层叠在用于催化剂层的透射膜两侧,以引导电解质膜方向; 并通过热压层叠体将催化剂层转移到电解质膜。 (附图标记)(AA)催化剂淤浆涂布; (BB)层压催化剂层; (CC)热压(T = 50-200摄氏度,P = 5-75kgf / cm 2); (DD)剥离膜去除; (EE)介绍性意见; (FF)脱膜; (GG)催化剂层; (HH)电解质膜; (二)二次剥离膜; (JJ)硅橡胶层; (KK)钢板; (LL)干; (S1)在剥离膜上形成催化剂层; (S2)在电解质膜的两面层压; (S3)将催化剂层转印到电解质膜上; (S4)除去脱模膜和溶剂