公开(公告)号:KR1020010046313A
公开(公告)日:2001-06-15
申请号:KR1019990050026
申请日:1999-11-11
Applicant: 현대자동차주식회사
Inventor: 정순준
IPC: C08L23/10
CPC classification number: C08L23/10 , C08F10/06 , C08F2500/18 , C08K3/013 , C08K3/26 , C08K9/08 , C08L23/16
Abstract: PURPOSE: A polypropylene resin composition having excellent plating characteristics and adhesive strength by proving polarity to polypropylene resin with an amine group having reactivity is provided, which is suitable for plating parts of an exterior and interior trim of an automobile and reduces manufacturing cost. CONSTITUTION: This polypropylene resin composition comprises 50 to 80% by weight of a polypropylene homopolymer and a polypropylene copolymer, 5 to 30% by weight of ethylene/propylene rubber containing 50 to 90% by weight of ethylene, 5 to 30% by weight of calcium carbonate grafted with 0.1 to 12% by weight of unsaturated carbonic acid or derivatives thereof after the coating of an amine-containing polymer and 5 to 40% by weight of an inorganic filler.
Abstract translation: 目的:提供一种聚丙烯树脂组合物,其具有优异的电镀特性和粘合强度,通过向具有反应性的胺基的聚丙烯树脂提供极性,其适用于汽车的内外饰件的电镀部件并降低制造成本。 构成:该聚丙烯树脂组合物包含50〜80重量%的聚丙烯均聚物和聚丙烯共聚物,5〜30重量%的含有50〜90重量%乙烯的乙烯/丙烯橡胶,5〜30重量% 在涂覆含胺聚合物和5〜40重量%的无机填料后,接枝0.1〜12重量%的不饱和碳酸或其衍生物的碳酸钙。
-
公开(公告)号:KR100236475B1
公开(公告)日:2000-01-15
申请号:KR1019970064826
申请日:1997-11-29
Applicant: 현대자동차주식회사
Inventor: 정순준
IPC: C09D127/06 , C09D5/34 , C09K3/10
Abstract: 본 발명은 폴리비닐클로라이드(PVC) 페이스트에 가소제, 충진제, 첨가제 및 개질제 등이 함유된 PVC 바디실러 조성물에 관한 것으로서, 본 발명의 조성물은 차체 강판의 중첩부에 도포되어 중도 및 상도 도막에서 발생하는 황변현상을 억제하는 우수한 황변방지용 PVC 바디실러 조성물이다.
-
公开(公告)号:KR100232625B1
公开(公告)日:1999-12-01
申请号:KR1019970044746
申请日:1997-08-30
IPC: C08L25/00
CPC classification number: C08L55/02 , C08L25/12 , C08L35/06 , C08L51/003 , C08L51/04 , C08L2205/02 , C08L2666/02
Abstract: 본 발명은 내약품성 및 내열성이 우수한 스티렌계 수지 조성물에 관한 것이다. 구체적으로, 본 발명은 말레이미드 화합물, 아크릴레이트 공중합체 및 오일 성분 등을 포함하여 내약품성 및 내열성이 우수하므로 자동차 부품으로 방향제, 브레이크 오일, 엔진 오일 및 가솔린 등 여러 약품이 접하는 부위에 유용하게 사용될 수 있는 스티렌계 수지 조성물에 관한 것으로서, 상기 수지 조성물은 특히 방향제에 의한 환경응력균열 저항성이 탁월하다.
-
公开(公告)号:KR1020170115345A
公开(公告)日:2017-10-17
申请号:KR1020160042884
申请日:2016-04-07
Applicant: 현대자동차주식회사 , 기아자동차주식회사 , 금호미쓰이화학 주식회사
CPC classification number: C08J9/125 , C08G18/12 , C08G18/30 , C08G18/4825 , C08G18/4837 , C08G18/632 , C08G18/6552 , C08G18/7621 , C08G18/7657 , C08G18/7664 , C08G2101/0008 , C08G2101/0058 , C08G2101/0083 , C08G2350/00 , C08J2203/10 , C08J2375/04 , C08G18/10 , C08G18/4072
Abstract: 본발명은정적, 동적안락감이향상된자동차시트패드제조용폴리우레탄조성물에관한것으로, 구체적으로폴리에테르폴리올(a1) 및폴리머폴리올(a2)이소정량혼합된폴리올혼합물(A), 톨루엔디이소시아네이트(Toluene diisocyanate)의사용없이메틸렌디페닐이소시아네이트(M-MDI)과폴리메틸렌디페닐디이소시아네이트(P-MDI)의이소시아네이트혼합물(b1)에특정범위의중량평균분자량을가지는폴리에스테르폴리올(b2)과중합하여얻은이소시아네이트화합물, 및첨가제로이루어진폴리우레탄제조용조성물및 이에의해제조된자동차시트패드인성형품에관한것이다.
Abstract translation: 另外,本发明的静态的,动态的舒适根据制造聚氨酯组合物,特别是聚醚多元醇(a1)和聚合物多元醇(a2)混合多元醇混合物(A)的异丙基量,甲苯二异氰酸酯(甲苯二异氰酸酯作为汽车座垫增强 无伪二苯基二异氰酸酯(M-MDI)和聚亚甲基二苯基甲烷二异氰酸酯(P-MDI异氰酸酯的混合物(B1)具有在特定范围的重均分子量的聚酯多元醇(b2)))亚甲基异氰酸酯得到的重合并 一种化合物和一种添加剂,以及由其制造的汽车座垫的模制品。
-
公开(公告)号:KR1020170111861A
公开(公告)日:2017-10-12
申请号:KR1020160038069
申请日:2016-03-30
CPC classification number: C08G18/14 , C08G18/165 , C08G18/1833 , C08G18/2063 , C08G18/244 , C08G18/4804 , C08G18/4829 , C08G18/7607 , C08G18/7621 , C08G18/7671 , C08G77/46 , C08G2101/0008 , C08G2101/005 , C08G2101/0083 , C08G18/4808 , C08G18/18 , C08G18/72 , C08J9/04 , C08J9/38
Abstract: 본발명은자체적으로난연성능을보유하고있음으로써별도의난연첨가제를첨가하지않아도되는난연성슬래브스톡폴리우레탄폼 조성물에관한것이다. 본발명에따른폴리우레탄폼 조성물은폴리올성분으로서분자량범위가서로다른폴리에테르폴리올을포함하면서동시에이소시아네이트지수를 70 ~ 95로낮춤으로써폼 자체적으로난연성을보유하게되어별도의난연제를첨가하지않아도되는획기적인효과를얻고있고, 또한종래의난연성슬래브스톡폴리우레탄폼조성물이난연제를첨가함으로써발생되는물성저하의문제까지도해결하는효과가있다.
Abstract translation: 本发明涉及阻燃块状聚氨酯泡沫组合物,其具有其自身的阻燃性能并且不需要添加单独的阻燃添加剂。 根据本发明由聚氨酯泡沫组合物,以及包括该分子量范围内的不同的聚醚多元醇作为在同一时间降低至95,在70的异氰酸酯指数是具有阻燃性的形式本身的突破,其不需要添加单独的阻燃剂的多元醇成分 而传统的阻燃块状聚氨酯泡沫组合物还具有解决降低添加阻燃剂所产生的物理性能的问题的效果。
-
公开(公告)号:KR101704137B1
公开(公告)日:2017-02-08
申请号:KR1020140178625
申请日:2014-12-11
Applicant: 현대자동차주식회사 , 롯데케미칼 주식회사
Abstract: 본발명은장섬유강화열가소성수지(LFT) 층사이에, 탄소섬유직조체, 유리섬유직조체또는탄소-유리섬유혼성직조체가적절히조합되어적층된하이브리드직조층이삽입되어있는구조를이루고있고, 직조간의간격조절, 탄소섬유와유리섬유의함량조절, 직조체의적층개수조절등을통하여요구되는물성보강효과와저비중효과를동시에만족시키는하이브리드복합재와이의제조방법, 그리고상기하이브리드복합재를소재로사용한자동차시트프레임에관한것이다.
Abstract translation: 本发明涉及混合复合材料及其制造方法以及使用该混合复合材料的汽车座椅框架。 根据本发明,混合复合材料具有在长纤维增强热塑性树脂层之间插入混合编织层的结构,其中混合编织层包括碳纤维编织体,玻璃纤维编织物 身体或碳玻璃纤维混合编织体适当组合和层压。 此外,混合复合材料通过调节编织纤维之间的间隙,碳纤维和玻璃纤维的含量以及层叠机织物的数量,可以满足低密度效果和材料性能的增强效果。
-
公开(公告)号:KR100828789B1
公开(公告)日:2008-05-09
申请号:KR1020060063164
申请日:2006-07-05
Applicant: 현대자동차주식회사
IPC: C09D175/06 , C09D175/04 , C09D5/28
CPC classification number: C08G18/42 , C08G18/44 , C08G18/6659 , C08G18/706 , C09D175/06
Abstract: 본 발명은 박막형 수성 소프트 질감도료에 관한 것으로서, 상세하게는 기존의 수성 소프트 질감도료의 도막물성(내마모성, 부착성 등) 및 소프트한 질감은 그대로 유지하면서, 도료의 도막두께를 35 ~ 40 미크론에서 20 ~ 25 미크론으로 감소시켜 박막화함으로써, 도료사용량 감소에 따른 원가절감 및 냄새개선, 뿐만 아니라 부품표면에 새겨진 엠보의 구현성을 향상시킬 수 있는 박막형 수성 소프트 질감도료에 관한 것이다.
박막, 수성, 소프트 질감도료, 내마모성, 부착성, 엠보-
公开(公告)号:KR1020080010044A
公开(公告)日:2008-01-30
申请号:KR1020060069999
申请日:2006-07-25
Abstract: A thermoplastic resin composition is provided to improve weather resistance, to lower smell and to enhance mechanical characteristics such as impact strength, thereby improving the suitability to an interior material of automobiles. A thermoplastic resin composition comprises 5-30 wt% of an acrylonitrile-ethylene-styrene copolymer; 5-30 wt% of an acrylonitrile-butadiene-styrene(ABS) copolymer; and 50-80 wt% of a styrene-acrylonitrile copolymer. Preferably the acrylonitrile-ethylene-styrene copolymer is prepared by reacting 10-45 wt% of a solvent, 40-60 wt% of a styrene-based monomer, 10-30 wt% of an acrylonitrile-based monomer, 5-12 wt% of an ethylene-propylene-based rubber, 0.5-5 wt% of a styrene-butadiene-styrene rubber, 0.01-0.1 wt% of an initiator; and 0.01-1 wt% of a molecular weight controller.
Abstract translation: 提供一种热塑性树脂组合物以改善耐候性,降低气味并增强机械特性如冲击强度,从而提高对汽车内部材料的适用性。 热塑性树脂组合物包含5-30重量%的丙烯腈 - 乙烯 - 苯乙烯共聚物; 5-30重量%的丙烯腈 - 丁二烯 - 苯乙烯(ABS)共聚物; 和50-80重量%的苯乙烯 - 丙烯腈共聚物。 优选地,丙烯腈 - 乙烯 - 苯乙烯共聚物通过使10-45重量%的溶剂,40-60重量%的苯乙烯基单体,10-30重量%的丙烯腈 - 基单体,5-12重量% 的乙烯 - 丙烯基橡胶,0.5-5重量%的苯乙烯 - 丁二烯 - 苯乙烯橡胶,0.01-0.1重量%的引发剂; 和0.01-1重量%的分子量控制剂。
-
公开(公告)号:KR1020080004316A
公开(公告)日:2008-01-09
申请号:KR1020060063164
申请日:2006-07-05
Applicant: 현대자동차주식회사
IPC: C09D175/06 , C09D175/04 , C09D5/28
CPC classification number: C08G18/42 , C08G18/44 , C08G18/6659 , C08G18/706 , C09D175/06
Abstract: A thin-wall waterborne soft feel paint is provided to reduce film thickness from 35-40 micron to 20-25 micron while retaining film physical properties and soft texture of the conventional waterborne soft feel paint. A thin-wall waterborne soft feel paint includes 15-20wt% of polyester polyol, 5-10wt% of polycarbonate polyol, 5-12wt% of a non-yellowing isocyanate resin as a hardener, 0.3-2wt% of a hydrophilic resin, 35-55wt% of deionized water, 2-5wt% of a pigment as an additive, 0.5-2wt% of a photostabilizer, 0.3-2wt% of a thickener, 3-7wt% of a photosensitizer, and 2-5wt% of an aliphatic organic solvent. The paint embodies film physical properties and soft textures in the film thickness level of 20-25 micron.
Abstract translation: 提供薄壁水性柔软油漆,以将膜厚度从35-40微米降低到20-25微米,同时保持传统水性柔软油漆的物理性能和柔软的质感。 薄壁水性柔软油漆包括15-20重量%的聚酯多元醇,5-10重量%的聚碳酸酯多元醇,5-12重量%的作为硬化剂的非黄变异氰酸酯树脂,0.3-2重量%的亲水性树脂,35 -55重量%的去离子水,2-5重量%的颜料作为添加剂,0.5-2重量%的光稳定剂,0.3-2重量%的增稠剂,3-7重量%的光敏剂和2-5重量%的脂族 有机溶剂。 该漆具有薄膜的物理性质和柔软的质感,膜厚度为20-25微米。
-
公开(公告)号:KR100757590B1
公开(公告)日:2007-09-10
申请号:KR1020060106538
申请日:2006-10-31
Applicant: 현대자동차주식회사 , 주식회사 엘지화학 , 에코플라스틱 주식회사
Abstract: A soft thermoplastic resin composition is provided to lower the coefficient of linear thermal expansion and the specific gravity and to improve impact resistance. A soft thermoplastic resin composition comprises 5-50 wt% of at least one kind of olefin-based thermoplastic elastomer selected from the group consisting of a partially crosslinked olefin-based thermoplastic elastomer and a totally crosslinked olefin-based thermoplastic elastomer; 1-40 wt% of an alpha-olefin-based copolymer rubber, an olefin-based copolymer rubber or a styrene-based copolymer rubber; 30-60 wt% of a polypropylene rubber having a melt index of 60-90 g/10 min; and 10-30 wt% of an inorganic filler having an average diameter of 0.1-15 micrometers.
Abstract translation: 提供软的热塑性树脂组合物以降低线性热膨胀系数和比重,并提高耐冲击性。 柔软的热塑性树脂组合物包含5-50重量%的至少一种选自部分交联的烯烃类热塑性弹性体和全部交联的烯烃类热塑性弹性体的烯烃类热塑性弹性体; 1-40重量%的α-烯烃基共聚物橡胶,烯烃基共聚物橡胶或苯乙烯基共聚物橡胶; 30-60重量%的熔体指数为60-90克/ 10分钟的聚丙烯橡胶; 和10-30重量%的平均直径为0.1-15微米的无机填料。
-
-
-
-
-
-
-
-
-