公开(公告)号:AU2016307760B2
公开(公告)日:2018-07-12
申请号:AU2016307760
申请日:2016-07-22
Applicant: CORNING INC
Inventor: DEMARTINO STEVEN EDWARD , FABIAN MICHELLE DAWN , KOHLI JEFFREY TODD , LYON JENNIFER LYNN , SMITH CHARLENE MARIE , TANG ZHONGZHI
Abstract: Embodiments of this disclosure pertain to a strengthened glass article including a first surface and a second surface opposing the first surface defining a thickness (t) of about less than about 1.1 mm, a compressive stress layer extending from the first surface to a depth of compression (DOC) of about 0.1-t or greater, such that when the glass article fracture, it breaks into a plurality of fragments having an aspect ratio of about 5 or less. In some embodiments, the glass article exhibits an equibiaxial flexural strength of about 20 kgf or greater, after being abraded with 90-grit SiC particles at a pressure of 25 psi for 5 seconds. Devices incorporating the glass articles described herein and methods for making the same are also disclosed.
-
公开(公告)号:AU2016253615B2
公开(公告)日:2018-05-31
申请号:AU2016253615
申请日:2016-11-03
Applicant: CORNING INC
Inventor: DEMARTINO STEVEN EDWARD , SCHAUT ROBERT ANTHONY
Abstract: A strengthened glass container or vessel such as, but not limited to, vials for holding pharmaceutical products or vaccines in a hermetic and/or sterile state. The strengthened glass container undergoes a strengthening process that produces compression at the surface and tension within the container wall. The strengthening process is designed such that the tension within the wall is great enough to ensure catastrophic failure of the container, thus rendering the product unusable, should sterility be compromised by a through-wall crack. The tension is greater than a threshold central tension, above which catastrophic failure of the container is guaranteed, thus eliminating any potential for violation of pharmaceutical integrity.
-
公开(公告)号:AU2018200466A1
公开(公告)日:2018-02-08
申请号:AU2018200466
申请日:2018-01-19
Applicant: CORNING INC
Inventor: FADEEV ANDREI GENNADYEVICH , CHANG THERESA , BOOKBINDER DANA CRAIG , PAL SANTONA , SAHA CHANDAN KUMAR , DEMARTINO STEVEN EDWARD , TIMMONS CHRISTOPHER LEE , PEANASKY JOHN STEPHEN
Abstract: A coated pharmaceutical package comprising: a glass body comprising a first surface and a second surface opposite the first surface, wherein the glass body is a glass container formed from a borosilicate glass composition and the first surface is an exterior surface of the glass container; and a low-friction coating positioned on at least a portion of the first surface of the glass body, the low-friction coating comprising: a polymer selected from the group consisting of polyimides, fluoropolymers, silsesquioxane-based polymers, and silicone resins; and a coupling agent layer disposed between the polymer and the first surface of the glass body, wherein the coefficient of friction of the portion of the coated pharmaceutical package with the low-friction coating is at least 20% less than a coefficient of friction of a surface of an uncoated pharmaceutical package formed from the same glass composition.
-
公开(公告)号:AU2016206304B2
公开(公告)日:2018-02-08
申请号:AU2016206304
申请日:2016-07-20
Applicant: CORNING INC
Inventor: FADEEV ANDREI GENNADYEVICH , CHANG THERESA , BOOKBINDER DANA CRAIG , PAL SANTONA , SAHA CHANDAN KUMAR , DEMARTINO STEVEN EDWARD , TIMMONS CHRISTOPHER LEE , PEANASKY JOHN STEPHEN
Abstract: A coated pharmaceutical package comprising: a glass body comprising a first surface and a second surface opposite the first surface, wherein the glass body is a glass container and the first surface is an exterior surface of the glass container; and a low-friction coating positioned on at least a portion of the first surface of the glass body, the low-friction coating comprising a polymer chemical composition, wherein: the coated pharmaceutical package is thermally stable at a temperature of at least about 260'C for 30 minutes; the low-friction coating has a mass loss of less than about 5% of its mass when heated from a temperature of 1 50 C to 350 C at a ramp rate of about 10 C/minute; and the coefficient of friction of the portion of the coated pharmaceutical package with the low-friction coating is at least 20% less than a coefficient of friction of a surface of an uncoated pharmaceutical package formed from a same glass composition.
-
公开(公告)号:AU2013352514B2
公开(公告)日:2017-03-16
申请号:AU2013352514
申请日:2013-11-22
Applicant: CORNING INC
Inventor: CHANG THERESA , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , FADEEV ANDREI GENNADYEVICH , MORENA ROBERT MICHAEL , PAL SANTONA , PEANASKY JOHN STEPHEN , SCHAUT ROBERT ANTHONY , TIMMONS CHRISTOPHER LEE , VENKATARAMAN NATESAN , VERKLEEREN RONALD LUCE
IPC: B32B17/06 , B65D1/40 , B65D23/08 , B65D25/14 , C03C17/00 , C03C17/30 , C03C17/32 , C03C17/42 , C03C21/00 , C09D179/08
Abstract: The glass containers described herein have at least two performance attributes selected from resistance to delamination, improved strength, and increased damage resistance. In one embodiment, a glass container may include a body having an inner surface, an outer surface and a wall thickness extending between the outer surface and the inner surface. At least the inner surface of the body may have a delamination factor less than or equal to 10. A tenacious inorganic coating may be positioned around at least a portion of the outer surface of the body. The outer surface of the body with the tenacious inorganic coating may have a coefficient of friction less than or equal to 0.7.
-
公开(公告)号:AU2015218474B2
公开(公告)日:2016-09-15
申请号:AU2015218474
申请日:2015-08-26
Applicant: CORNING INC
Inventor: DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , DRAKE MELINDA ANN , MORENA ROBERT MICHAEL , PAL SANTONA , SCHAUT ROBERT ANTHONY
Abstract: A glass composition comprising: from about 70 mol.% to about 80 mol.% SiO2; from about 4 mol.% to about 8 mol.% alkaline earth oxide, the alkaline earth oxide comprising CaO and from about 3 mol.% to about 7 mol.% MgO; X mol.% A120 3 , wherein X is from about 5 to about 7; and Y mol.% alkali oxide, wherein the alkali oxide comprises Na20 in an amount greater than 8 mol.%, and the glass composition is free of boron and compounds of boron.
-
公开(公告)号:AU2013282411B2
公开(公告)日:2016-08-04
申请号:AU2013282411
申请日:2013-06-28
Applicant: CORNING INC
Inventor: ADIB KAVEH , BOOKBINDER DANA CRAIG , CHANG THERESA , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , DRAKE MELINDA ANN , FADEEV ANDREI GENNADYEVICH , HAMILTON JAMES PATRICK , MORENA ROBERT MICHAEL , PAL SANTONA , PEANASKY JOHN STEPHEN , SAHA CHANDAN KUMAR , SCHAUT ROBERT ANTHONY , SCHIEFELBEIN SUSAN LEE , TIMMONS CHRISTOPHER LEE
Abstract: Delamination resistant glass containers with heat-tolerant coatings are disclosed. In one embodiment, a glass container may include a glass body having an interior surface, an exterior surface and a wall thickness extending from the exterior surface to the interior surface. At least the interior surface of the glass body is delamination resistant. The glass container may further include a heat-tolerant coating positioned on at least a portion of the exterior surface of the glass body. The heat- tolerant coating may be thermally stable at temperatures greater than or equal to 260°C for 30 minutes.
-
公开(公告)号:MX2015006888A
公开(公告)日:2015-09-16
申请号:MX2015006888
申请日:2013-11-22
Applicant: CORNING INC
Inventor: MORENA ROBERT MICHAEL , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , SCHAUT ROBERT ANTHONY , FADEEV ANDREI GENNADYEVICH , CHANG THERESA , PEANASKY JOHN STEPHEN , PAL SANTONA , VENKATARAMAN NATESAN , VERKLEEREN RONALD LUCE
IPC: B32B17/06 , C03C17/00 , B65D1/40 , B65D25/14 , C03C17/30 , C03C17/32 , C03C17/42 , C03C21/00 , C09D179/08
Abstract: Los contenedores de vidrio descritos en la presente tienen por lo menos dos atributos de rendimiento seleccionados de resistencia a la delaminación, resistencia mejorada y mayor resistencia al daño; en una modalidad, un contenedor de vidrio que tiene resistencia a la delaminación y fuerza mejorada puede incluir un cuerpo que tiene una superficie interior, una superficie exterior y un grosor de pared que se extiende entre la superficie exterior y la superficie interior; por lo menos la superficie interior del cuerpo puede tener un factor de delaminación menor o igual que 10; el contenedor de vidrio también puede incluir una capa tensada compresivamente que se extiende desde la superficie exterior del cuerpo hacia el grosor de la pared; la capa tensada compresivamente puede tener un esfuerzo de compresión de superficie mayor o igual que 150 MPa.
-
69.
公开(公告)号:MX2014015932A
公开(公告)日:2015-07-17
申请号:MX2014015932
申请日:2013-06-28
Applicant: CORNING INC
Inventor: DRAKE MELINDA ANN , MORENA ROBERT MICHAEL , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , SCHAUT ROBERT ANTHONY , CHANG THERESA , BOOKBINDER DANA CRAIG , SAHA CHANDAN KUMAR , TIMMONS CHRISTOPHER LEE , PEANASKY JOHN STEPHEN , ADIB KAVEH , HAMILTON JAMES PATRICK , SCHIEFELBEIN SUSAN LEE , FADEEV ANDREI GENNADYEVICH , PAL SANTONA
Abstract: Los contenedores de vidrio resistentes a la deslaminación con los recubrimientos tolerantes al calor se describen; en una modalidad, un contenedor de vidrio puede incluir un cuerpo de vidrio que tiene una superficie interior, una superficie exterior y un espesor de pared que se extiende desde la superficie exterior a la superficie interior; al menos la superficie interior del cuerpo de vidrio es resistente a la deslaminación; el contenedor de vidrio además puede incluir un recubrimiento tolerante al calor colocado sobre al menos una porción de la superficie exterior del cuerpo de vidrio; el recubrimiento tolerante al calor puede ser térmicamente estable a temperaturas mayores o iguales a 260 °C por 30 minutos.
-
公开(公告)号:SG11201504033TA
公开(公告)日:2015-06-29
申请号:SG11201504033T
申请日:2013-11-22
Applicant: CORNING INC
Inventor: CHANG THERESA , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , FADEEV ANDREI GENNADYEVICH , MORENA ROBERT MICHAEL , PAL SANTONA , PEANASKY JOHN STEPHEN , SCHAUT ROBERT ANTHONY , TIMMONS CHRISTOPHER LEE , VENKATARAMAN NATESAN , VERKLEEREN RONALD LUCE
IPC: C03C17/00 , B32B17/06 , B65D1/40 , B65D25/14 , C03C17/30 , C03C17/32 , C03C17/42 , C03C21/00 , C09D179/08
Abstract: The glass containers described herein have at least two performance attributes selected from resistance to delamination, improved strength, and increased damage resistance. In one embodiment, a glass container may include a body having an inner surface, an outer surface and a wall thickness extending between the outer surface and the inner surface. At least the inner surface of the body may have a delamination factor less than or equal to 10. A tenacious inorganic coating may be positioned around at least a portion of the outer surface of the body. The outer surface of the body with the tenacious inorganic coating may have a coefficient of friction less than or equal to 0.7.
-
-
-
-
-
-
-
-
-