公开(公告)号:JP2010042987A
公开(公告)日:2010-02-25
申请号:JP2009168695
申请日:2009-07-17
Inventor: HAMAI TOSHIMASA , SHIMODA MASARO , OKUBO MAKOTO , TANIGUCHI TAKAO , TOMIFUJI TAKESHI , NOMURA MASATO
CPC classification number: C04B24/166 , C04B24/16 , C04B28/02 , C04B40/0039 , C04B2201/05 , C04B2103/408
Abstract: PROBLEM TO BE SOLVED: To provide a high-early-strength agent for hydraulic composition with excellent improved effect of short-term strength. SOLUTION: The high-early-strength agent for hydraulic composition is composed of a compound (a) which is obtained by reacting (A) one or more substances selected from polyhydric alcohols having functionality of 3-20 and alkylene oxide addition products of polyhydric alcohols having functionality of 3-20 with (B) a sulfating agent. An additive composition for hydraulic composition containing the compound (a) is also disclosed. COPYRIGHT: (C)2010,JPO&INPIT
Abstract translation: 要解决的问题:提供具有优异的短期强度效果的用于水硬性组合物的高强度剂。 解决方案:用于水硬性组合物的高强度剂由化合物(a)组成,该化合物通过(A)一种或多种选自官能度为3-20的多元醇和烯化氧加成产物 具有3-20官能度的多元醇与(B)硫酸化剂反应。 还公开了含有化合物(a)的水硬性组合物用添加剂组合物。 版权所有(C)2010,JPO&INPIT
-
公开(公告)号:JP2010042986A
公开(公告)日:2010-02-25
申请号:JP2009168694
申请日:2009-07-17
Inventor: SHIMODA MASARO , HAMAI TOSHIMASA , OKUBO MAKOTO , TOMIFUJI TAKESHI , NOMURA MASATO
IPC: C04B7/52 , C04B7/00 , C04B24/16 , C04B103/52
Abstract: PROBLEM TO BE SOLVED: To provide a method for producing a hydraulic powder, whereby safety of a pulverizing aid can be assured, the time required for achieving a desired particle diameter can be shortened due to high pulverizing efficiency and the hydraulic powder capable of increasing strength of a resulting hydraulic composition can be obtained. SOLUTION: The hydraulic powder is produced via a step of pulverizing a hydraulic compound in the presence of a compound (a) obtained by reacting (A) at least one chosen from a polyhydric alcohol and an alkylene oxide adduct thereof with (B) a sulfating agent. COPYRIGHT: (C)2010,JPO&INPIT
Abstract translation: 解决的问题:为了提供一种制造水硬性粉末的方法,由此可以确保粉碎助剂的安全性,由于高的粉碎效率和能够使水硬性粉末能够达到期望的粒径所需的时间可以缩短 可获得所得水硬性组合物强度的增加。 溶液:通过在(A)至少一种选自多元醇和其氧化烯加合物中的(B)与(B)的反应得到的化合物(a)的存在下,将水硬性化合物粉碎的工序, )硫酸化剂。 版权所有(C)2010,JPO&INPIT
-
公开(公告)号:JP2003335830A
公开(公告)日:2003-11-28
申请号:JP2002144073
申请日:2002-05-20
Inventor: SAWAI MINORU , OKUBO MAKOTO
Abstract: PROBLEM TO BE SOLVED: To provide a sufficiently strong foam having suitable resilience and, concurrently, high rebound resilience. SOLUTION: The foam has a storage elastic modulus of 17-25 MPa as determined from its dynamic viscoelasticity at 10 Hz and 25°C, and records 0.01-0.14 in tanδ. Soles including the foam and shoes using the soles are manufactured. COPYRIGHT: (C)2004,JPO
Abstract translation: 要解决的问题:提供具有合适弹性和同时具有高回弹性的足够强的泡沫。 解决方案:泡沫体的储能弹性模量为17-25MPa,由其在10Hz和25℃下的动态粘弹性测定,在tanδ中记录0.01-0.14。 制造包括泡沫和鞋底的鞋底。 版权所有(C)2004,JPO
-
公开(公告)号:JP2003306522A
公开(公告)日:2003-10-31
申请号:JP2002110404
申请日:2002-04-12
Inventor: SAWAI MINORU , OKUBO MAKOTO
IPC: C08G18/00 , C08G101/00
Abstract: PROBLEM TO BE SOLVED: To provide a foam having sufficient strength and combining soft and good touch and reduced resilience. SOLUTION: The foam has a density of 0.1 g/cm 3 or higher, a storage elastic modulus, obtained by the dynamic viscoelasticity at a frequency of 10 Hz and 25°C of 5-20 MPa and a tanδ of 0.16-0.5. A sole having the foam and a shoe having the sole are also provided. COPYRIGHT: (C)2004,JPO
Abstract translation: 要解决的问题:提供具有足够强度并结合柔软和良好触感并降低弹性的泡沫。 解决方案:泡沫体的密度为0.1g / cm 3 / SP以上,通过在10Hz和25℃的频率下的动态粘弹性得到的储存弹性模量为5-20 MPa,tanδ为0.16-0.5。 还提供了具有泡沫的鞋底和具有鞋底的鞋。 版权所有(C)2004,JPO
-
公开(公告)号:JP2003119236A
公开(公告)日:2003-04-23
申请号:JP2001311482
申请日:2001-10-09
Applicant: KAO CORP
Inventor: SAWAI MINORU , OKUBO MAKOTO
IPC: C08G18/10 , C08G18/76 , C08G101/00
Abstract: PROBLEM TO BE SOLVED: To provide a polyurethane foam elastomer low in impact resilience but sufficiently strong when used singly and a method for manufacturing the same. SOLUTION: The elastomer is manufactured by reaction of a composition I containing a compound A having two or more active hydrogens and an isocyanate prepolymer II in the presence of a foaming agent, and is 0.2-1.0 g/cm in density, 20% or less in modulus of repulsion elasticity when 10 mm in thickness, and 1-90 in hardness (Asker C). The manufacturing method is such that the composition I and the prepolymer II react with each other as mentioned above for manufacturing an elastomer having the above-mentioned properties.
-
公开(公告)号:JP2000103958A
公开(公告)日:2000-04-11
申请号:JP27478998
申请日:1998-09-29
Applicant: KAO CORP
Inventor: OKUBO MAKOTO , FUKUMOTO KAZUHISA , TAKEMURA KAZUNARI
Abstract: PROBLEM TO BE SOLVED: To obtain a polyurethane excellent in safety, obtained by using raw materials having no corrosivity on a metal, capable of maintaining the strength possessed by the original resin for a long term, manifesting stable electroconductive properties at the time just after the molding and with time, and useful for an additive for safety shoes. SOLUTION: This polyurethane contains (A) a quarternary ammonium alkyl sulfate, preferably a one of the formula (R1 is a 6-24C alkyl; R2 and R2' are each H or a 1-4C alkyl; R3 is a 1-4C alkyl; R4 is a 1-24C alkyl), e.g. N-ethyl-N,N- dimethyl-N-stearylammonium ethyl sulfate, and (B) a salt of trifluoromethanesulfonic acid (e.g. lithium trifluoromethanesulfonate). For example, the weight ratio of components A to B is preferably regulated so as to be (20:1)-(1:1), and the polyurethane preferably contains 0.5-9 wt.% component A and 0.02-1 wt.% component B.
-
公开(公告)号:JPH1180329A
公开(公告)日:1999-03-26
申请号:JP24708497
申请日:1997-09-11
Applicant: KAO CORP
Inventor: SAWAI MINORU , OKUBO MAKOTO , MORI MASAHIRO
IPC: C08J9/02 , C08G18/10 , C08G18/42 , C08G63/12 , C08G101/00
Abstract: PROBLEM TO BE SOLVED: To provide a method for producing a low-density polyurethane foam having good appearance and feel and excellent in mechanical strength such as tensile strength and tear strength. SOLUTION: This polyurethane foam is obtained by reaction between a polyisocyanate component and a polyol component followed by expansion; wherein the polyol component contains a polyester polyol which is prepared by polycondensation reaction between an acid component comprising isophthalic acid and an aliphatic polybasic acid and a polyhydric alcohol, and the polyester polyol is liquid at 40 deg.C and has a viscosity of
-
公开(公告)号:JPH10182780A
公开(公告)日:1998-07-07
申请号:JP34811496
申请日:1996-12-26
Applicant: KAO CORP
Inventor: OKUBO MAKOTO , NOMURA TAKAYUKI , MORII MASAYOSHI , ISAYAMA YASUTOSHI
IPC: C08G18/32 , C08G18/60 , C08G101/00
Abstract: PROBLEM TO BE SOLVED: To provide a method by which a rigid polyurethane foam excellent in dimensional stability at low temperatures can be produced. SOLUTION: A tertiary amino-alcohol represented by formula I [R1 denotes a 1-24C straight-chain or branched alkyl group, etc.; (m) denotes a number of 3-50 on the weight average; R2 denotes a 2-20C straight-chain or branched alkylene group, etc.] is used as at least a part of an active hydrogen-containing compound and a reaction is carried out in the presence of a compound represented by formula II R3 (X)n [R3 is an (n)-valent hydrocarbon group; X denotes the same or different anionic eliminable group; (n) is an integer of >=2] when reacting an isocyanate compound with the active hydrogen-containing compound and producing a rigid polyurethane resin.
-
-
-
-
-
-
-