公开(公告)号:JP2011068831A
公开(公告)日:2011-04-07
申请号:JP2009223024
申请日:2009-09-28
Applicant: Jx Nippon Oil & Energy Corp , Jx日鉱日石エネルギー株式会社
Inventor: NAKAYAMA TOSHIO , MUROUCHI SATOSHI
CPC classification number: B29C45/00 , B29K2067/00 , B29K2105/0079 , C08K3/04 , C08K3/22 , C08K3/36 , C08K2201/009 , C09K19/3809 , C08L67/03
Abstract: PROBLEM TO BE SOLVED: To provide a resin composition for camera modules capable of reducing generation of dust (dropping of particles) during manufacturing of cameras, during use of cameras and during driving of camera modules, and having high surface hardness and excellent balance between heat resistance, rigidity and moldability and surface exfoliation characteristics, with no operation failure of automatic focus control, etc.
SOLUTION: A liquid crystal polyester resin composition is used, which contains (A) 49.5-69.5 pts.mass of a liquid crystal polyester, (B) 30.0-50.0 pts.mass of powder in an indefinite or spherical shape with a primary particle diameter of ≤5 μm and having a Mohs hardness of ≥5, and (C) 0.5-5.0 pts.mass of a carbon black based on the whole composition as 100 pts.mass.
COPYRIGHT: (C)2011,JPO&INPITAbstract translation: 要解决的问题:提供一种相机模块用树脂组合物,其能够在相机的制造期间,在照相机的使用期间和在相机模块的驱动期间减少灰尘的产生(颗粒的掉落),并且具有高的表面硬度和优异的 耐热性,刚性和成型性以及表面剥离特性之间的平衡,无自动聚焦控制的操作故障等。解决方案:使用液晶聚酯树脂组合物,其包含(A)49.5-69.5质点 液晶聚酯,(B)30.0-50.0粒子,一次粒径≤5μm,莫氏硬度≥5的不定形或球形粉末,(C)0.5-5.0质量份 的基于整个组合物的炭黑为100质量份。 版权所有(C)2011,JPO&INPIT
-
公开(公告)号:JP2017527648A
公开(公告)日:2017-09-21
申请号:JP2016575945
申请日:2015-07-01
Applicant: ヘンケル・アクチェンゲゼルシャフト・ウント・コムパニー・コマンディットゲゼルシャフト・アウフ・アクチェンHenkel AG & Co. KGaA , ヘンケル・アクチェンゲゼルシャフト・ウント・コムパニー・コマンディットゲゼルシャフト・アウフ・アクチェンHenkel AG & Co. KGaA
Inventor: ヘルガ・ガルマン , デニス・バンクマン , マルセル・フランケン , イェンス・グロイトル
IPC: C09J175/04 , B65D65/40 , C09J11/04
CPC classification number: C09J175/04 , B32B7/12 , B32B15/04 , B32B27/40 , B32B2553/00 , C08G18/10 , C08G18/12 , C08G18/4018 , C08G18/42 , C08G18/4816 , C08G18/4829 , C08G18/7671 , C08K3/26 , C08K2003/265 , C08K2201/005 , C08K2201/009 , C09D175/04 , C09J175/06 , C09J175/08 , C08K9/06
Abstract: 本発明は、ポリウレタン接着剤、特に、積層フィルム用のポリウレタン接着剤であって、前記PU接着剤が、接着剤の総重量に対して、5〜50重量%の、好ましくは10〜40重量%の、特に好ましくは20〜30重量%の、少なくとも1種の固体粒子状フィラーを含んでなり、少なくとも1種のフィラーのフィラー粒子の少なくとも90%が4μm以下の粒子径を有し、少なくとも1種のフィラーが3以下のモース硬度を有するポリウレタン接着剤に関する。また、本発明は、フィルムを接着するための前記接着剤の使用、複合フィルムの製造方法、および前記接着剤を用いて接着された複合フィルムに関する。
-
公开(公告)号:JPWO2013191207A1
公开(公告)日:2016-05-26
申请号:JP2014521489
申请日:2013-06-19
CPC classification number: C08K7/24 , C08K3/22 , C08K3/346 , C08K3/38 , C08K2003/2227 , C08K2003/382 , C08K2201/009 , C08L81/02
Abstract: 20〜80質量%のポリアリーレンスルフィド樹脂(A)と、合計で10〜50質量%のモース硬度が5以上の高放熱性フィラー(B)とモース硬度が5未満の高放熱性フィラー(C)と平均粒径が8μm以下でかつモース硬度が2以下の粘土鉱物(D)と、10〜40質量%の繊維状強化材(E)とを必須成分とし、前記ポリアリーレンスルフィド樹脂をマトリックスとして前記高放熱性フィラー(B)と、前記高放熱性フィラー(C)と、前記粘土鉱物(D)と、前記繊維状強化材(E)が分散してなる高放熱性ポリアリーレンスルフィド樹脂組成物を提供する。当該樹脂組成物は熱伝導性および機械的強度に優れる。
Abstract translation: 20向聚亚芳基硫醚树脂(A),并且在5个或更多高散热填料(B)和具有小于5(C)的莫氏硬度高散热填料的总10〜50质量%的莫氏硬度的80%(重量) 和平均粒径为8微米或更小和2或更小的粘土矿物(D)和10的莫氏硬度与纤维增强材料(E)作为必须成分的40重量%,其特征在于,所述聚芳硫醚树脂作为基体 高的热辐射填料(B),和高的散热填料(C),其中,所述粘土矿物(D),高的热辐射聚芳硫醚树脂组合物,其中所述纤维增强材料(E)分散 提供。 该树脂组合物具有优异的热导率和机械强度。
-
公开(公告)号:JP5486889B2
公开(公告)日:2014-05-07
申请号:JP2009223024
申请日:2009-09-28
Applicant: Jx日鉱日石エネルギー株式会社
IPC: C08L67/03 , B29C45/00 , C08K3/04 , C08K3/10 , C08K7/18 , G02B7/02 , G03B9/08 , G03B17/00 , H04N5/225
CPC classification number: B29C45/00 , B29K2067/00 , B29K2105/0079 , C08K3/04 , C08K3/22 , C08K3/36 , C08K2201/009 , C09K19/3809 , C08L67/03
Abstract: A liquid crystal polyester resin composition for camera modules is used, the composition including, based on 100 parts by mass of the composition as a whole, (A) 49.5 to 69.5 parts by mass of a liquid crystal polyester, (B) 30.0 to 50.0 parts by mass of an irregular form or spherical powder having a Mohs hardness of 5 or higher and a primary particle diameter of 5 mum or less, and (C) 0.5 to 5.0 parts by mass of carbon black. The use of the resin composition allows a reduction in the amount of dust generated (particles falling off) during the production of the camera, the use of the camera, and the operation of the camera modules. The resin composition has high surface hardness, is excellent in balance between heat resistance, stiffness, moldability, and resistance to falling of particles off a surface, and causes no malfunction during autofocus control.
-
公开(公告)号:JP2004059629A
公开(公告)日:2004-02-26
申请号:JP2002216569
申请日:2002-07-25
Applicant: Sumitomo Rubber Ind Ltd , 住友ゴム工業株式会社
Inventor: HORIGUCHI TAKUYA , MINAKOSHI AKIRA
IPC: B60C1/00 , B60C11/14 , C08K3/00 , C08K5/5415 , C08K7/02 , C08K7/14 , C08L3/00 , C08L9/00 , C08L21/00
CPC classification number: B60C11/14 , B60C1/0016 , C08K3/013 , C08K7/14 , C08K2201/009 , C08L3/00 , C08L21/00 , C08L2666/26
Abstract: PROBLEM TO BE SOLVED: To provide a rubber composition capable of sufficiently improving on-ice-and-snow grip performance and wet grip performance; and a pneumatic tire using the same.
SOLUTION: The rubber composition is prepared by compounding (A) 100 pts.wt. diene rubber with (B) 2-20 pts.wt. short fibers having an average fiber length of 10-100 μm and an average fiber length of 0.01-4 mm, (C) 1-10 pts.wt. particles having a Mohs hardness of 5 or higher and an average particle size of 500 μm or less, and (D) 1-15 pts.wt. starch/plasticizer composite. The pneumatic tire has a tread made from the rubber composition.
COPYRIGHT: (C)2004,JPOAbstract translation: 要解决的问题:提供能够充分提高冰 - 雪和抓地性能和湿抓地性能的橡胶组合物; 以及使用该轮胎的充气轮胎。 解决方案:通过配合(A)100重量份制备橡胶组合物。 二烯橡胶与(B)2-20重量份 平均纤维长度为10-100μm,平均纤维长度为0.01-4mm,(C)1-10重量份的短纤维 莫氏硬度为5以上,平均粒径为500μm以下的粒子,(D)1-15重量份。 淀粉/增塑剂复合材料。 充气轮胎具有由橡胶组合物制成的胎面。 版权所有(C)2004,JPO
-
公开(公告)号:TW201111439A
公开(公告)日:2011-04-01
申请号:TW099119285
申请日:2010-06-14
Applicant: 傑斯日本石油能源公司
CPC classification number: B29C45/00 , B29K2067/00 , B29K2105/0079 , C08K3/04 , C08K3/22 , C08K3/36 , C08K2201/009 , C09K19/3809 , C08L67/03
Abstract: 本發明係提供一種相機模組用樹脂組成物,其係於相機生產過程中、使用中及相機模組之驅動中,甚少發生微塵(粉末脫落),表面硬度高,耐熱性、剛性、成形性與表面脫落物特性的均衡性優異,未有自動焦點調整之動作不良等。本發明使用一種液晶聚酯樹脂組成物,其係組成物全體設為100質量部,包含:(A)液晶聚酯49.5~69.5質量部;(B)莫氏硬度5以上且一次粒徑5μ
Abstract in simplified Chinese: 本发明系提供一种相机模块用树脂组成物,其系于相机生产过程中、使用中及相机模块之驱动中,甚少发生微尘(粉末脱落),表面硬度高,耐热性、刚性、成形性与表面脱落物特性的均衡性优异,未有自动焦点调整之动作不良等。本发明使用一种液晶聚酯树脂组成物,其系组成物全体设为100质量部,包含:(A)液晶聚酯49.5~69.5质量部;(B)莫氏硬度5以上且一次粒径5μ
-
公开(公告)号:KR101766085B1
公开(公告)日:2017-08-08
申请号:KR1020150176374
申请日:2015-12-10
Inventor: 김율구
CPC classification number: C09D127/18 , B05D5/083 , B05D2601/20 , C08K3/04 , C08K2201/005 , C08K2201/009 , C09D5/00 , F02F3/10
Abstract: 비드밀링을통해다이아몬드분말을유기용매에분산시켜분산용액을제조하는분산단계; 분산용액에실란용액을혼합시켜혼합용액을제조하는혼합단계; 혼합용액에 PTFE(Polytetrafluoroethylene)입자의크기가 0.1~6㎛인 PTFE용액을첨가하여코팅용액을제조하는첨가단계; 제조된코팅용액을피스톤스커트표면에코팅하여복수의딤플(Dimple)이분포된코팅층을형성시키는코팅단계; 및코팅층을건조시킨후 열처리하는경화단계;를포함하는 PTFE 코팅용액코팅방법이소개된다.
Abstract translation: 分散步骤,通过珠磨将金刚石粉末分散在有机溶剂中以产生分散溶液; 将分散溶液与硅烷溶液混合以制备混合溶液; 加入步骤加入到PTFE,PTFE的大小(聚四氟乙烯)0.1〜6㎛颗粒在混合溶液中以制备涂布溶液的溶液; 将所制备的涂覆溶液涂覆在活塞裙部的表面上以形成分布有多个凹坑的涂层的涂覆步骤; 以及干燥涂层然后进行热处理的固化步骤。
-
公开(公告)号:KR1020170023932A
公开(公告)日:2017-03-06
申请号:KR1020177000184
申请日:2015-07-01
Applicant: 헨켈 아게 운트 코. 카게아아
IPC: C09J11/02 , C09J175/04 , B32B37/12 , B32B7/12 , B32B27/08
CPC classification number: C09J175/04 , B32B7/12 , B32B15/04 , B32B27/40 , B32B2553/00 , C08G18/10 , C08G18/12 , C08G18/4018 , C08G18/42 , C08G18/4816 , C08G18/4829 , C08G18/7671 , C08K3/26 , C08K2003/265 , C08K2201/005 , C08K2201/009 , C09D175/04 , C09J175/06 , C09J175/08 , C08K9/06 , C09J11/02 , B32B27/08 , B32B37/12 , B32B2439/70 , B32B2439/80
Abstract: 본발명은, 특히필름을라미네이팅하기위한, 폴리우레탄접착제에관한것이다. 폴리우레탄 (PU) 접착제는 - 접착제의총 중량에대해 - 5 내지 50 wt%, 바람직하게는 10 내지 40 wt%, 특히 20 내지 30 wt% 의적어도하나의고체입자필러를함유한다. 적어도하나의필러의필러입자의적어도 90% 가 4 μm 이하의입자크기를갖고, 적어도하나의필러재료는 3 이하의모스 (Mohs) 경도를갖는다. 본발명은또한필름을접착시키기위한상기접착제의용도, 복합필름을제조하기위한방법, 및상기언급된접착제를사용하여접착된복합필름에관한것이다.
Abstract translation: 本发明涉及聚氨酯粘合剂,特别是用于层压膜。 PU粘合剂含有至少一种固体颗粒填料的5至50重量%,优选10至40重量%,特别是基于粘合剂总重量的20至30重量%。 所述至少一种填充材料的至少90%的填料颗粒具有4μm或更小的粒度,并且所述至少一种填料材料的莫氏硬度为3以下。 本发明还涉及粘合剂用于粘合膜的用途,复合膜的制造方法以及使用上述粘合剂粘合的复合膜。
-
公开(公告)号:KR1020150023805A
公开(公告)日:2015-03-05
申请号:KR1020157001360
申请日:2013-08-09
Applicant: 다이킨 고교 가부시키가이샤
CPC classification number: C08K9/02 , C08L27/12 , C08K3/04 , C08K2201/009 , C08K2201/011
Abstract: 본 발명은 인장 강도 및 내굴곡성이 우수한 성형품을 얻기 위한 불소 수지 조성물을 제공하는 것을 목적으로 한다. 본 발명은 불소 수지 및 불소화 나노 다이아몬드를 포함하고, 불소화 나노 다이아몬드가 불소 수지의 0.001 내지 5질량%인 것을 특징으로 하는 불소 수지 조성물이다.
-
公开(公告)号:KR1020150023573A
公开(公告)日:2015-03-05
申请号:KR1020147037156
申请日:2013-06-18
Applicant: 사빅 글로벌 테크놀러지스 비.브이.
Inventor: 얀선베르나르드뉘스요하네스파울뤼스 , 스테인담빌헬뮈스요하네스다니엘 , 파위엔브룩로버르트
CPC classification number: C08L69/00 , C08G64/04 , C08G64/16 , C08K5/5313 , C08K2201/009 , C08L33/12 , C08L55/02 , C08L67/04 , C08L83/10
Abstract: 본 개시는 이소소르바이드/레조르시놀/비스페놀-A 폴리카보네이트 터폴리머를 포함하는 제1 폴리카보네이트 성분, 선택적인 제2 폴리카보네이트 성분, 및 1종 이상의 충격 개질제를 포함하는 열가소성 폴리카보네이트 조성물에 관한 것이다. 본 명세서에 개시된 폴리카보네이트 조성물은 다른 특성들 중에서 향상된 노치형 아이조드 충격 강도, 인장 탄성률, 인장 강도, 및 다축 충격 강도를 가진다.
-
-
-
-
-
-
-
-
-