公开(公告)号:KR100380441B1
公开(公告)日:2003-04-26
申请号:KR1020000062383
申请日:2000-10-23
Applicant: 현대자동차주식회사
Inventor: 조봉래
IPC: C22C38/44
Abstract: PURPOSE: Provided is Si-Cr free carburizing steel composition with excellent durability and mechanical properties such as fatigue strength for transmission gear. CONSTITUTION: In a carburizing steel composition mainly composed of Fe, the steel composition comprises C 0.17-0.23 wt.%, Si 0.01 wt.% or less, Mn 0.30-0.5 wt.%, P 0.01 wt.% or less, S 0.015 wt.%% or less, Ni 1.55-2.0 wt.%%, Cr 0.01 wt.% or less, Mo 0.9-1.1 wt.%, Nb 0.015-0.1 wt.%, Vd 0.01-0.05 wt.%, trace amount of Ti and Al.
Abstract translation: 用途:提供具有优异的耐久性和传动装置的疲劳强度等机械特性的Si-Cr自由渗碳钢成分。 构成:在主要由Fe组成的渗碳钢组合物中,钢组成包含C 0.17-0.23重量%,Si 0.01重量%或更少,Mn 0.30-0.5重量%,P 0.01重量%或更少,S 0.015 ,Ni:1.55-2.0重量%,Cr:0.01重量%以下,Mo:0.9-1.1重量%,Nb:0.015-0.1重量%,Vd:0.01-0.05重量%,微量 的Ti和Al。
-
公开(公告)号:KR1020030013961A
公开(公告)日:2003-02-15
申请号:KR1020010048262
申请日:2001-08-10
Applicant: 현대자동차주식회사
Inventor: 조봉래
IPC: C23C8/20
Abstract: PURPOSE: A method for reducing thermal deformation of cementation heat treatment parts is provided to reduce the deformation range of the parts after heat treatment by passing the parts through sub-zero treatment process before cementation after forming parts such as gears for automobile transmission. CONSTITUTION: The method comprises hot or cold forging process for a material to be formed, cooling process, heat treatment process before forming, forming process, cementation heat treatment process and postforming process, wherein the method further comprises a sub-zero treatment process between the forming process and the cementation heat treatment process in which the rapidly cooled article is maintained for a certain period of time after rapidly cooling a formed article to a liquid nitrogen temperature of about -196 deg.C before heat treating the formed material after forming of the material.
Abstract translation: 目的:提供一种降低胶结热处理部件热变形的方法,通过在汽车变速器齿轮等部件形成后,通过零部件通过零下处理工艺,减少热处理后部件的变形范围。 构成:该方法包括要形成的材料的热或冷锻造工艺,冷却过程,成形之前的热处理工艺,成型工艺,胶结热处理工艺和后成型工艺,其中所述方法还包括: 在将成型体快速冷却至约-196℃的液氮温度之后将快速冷却的物品保持一定时间的固化热处理工艺,在形成后形成的材料之前, 材料。
-
公开(公告)号:KR1020020056059A
公开(公告)日:2002-07-10
申请号:KR1020000085343
申请日:2000-12-29
Applicant: 현대자동차주식회사
Inventor: 조봉래
IPC: C21D9/32
Abstract: PURPOSE: A surface hardening method of automotive transmission gear for micronizing grain size and improving bending fatigue property is provided. CONSTITUTION: In a surface hardening method of automotive transmission gear, the present invention is characterized in that after conventional vacuum decarburization and gas quenching operations, automotive transmission gear is reheated in the temperature range of 820-850°C for 20-30 minutes, and then gas quenching or oil quenching is conducted. Gas quenching operation is characterized by using a reductive gas selected from N2, H2 and He.
Abstract translation: 目的:提供一种用于微粒化和改善弯曲疲劳性能的汽车传动齿轮的表面硬化方法。 构成:在汽车传动齿轮的表面硬化方法中,本发明的特征在于,在常规的真空脱碳和气体淬火操作之后,将汽车传动齿轮在820-850℃的温度范围内再加热20-30分钟, 然后进行气体淬火或油淬。 气体淬火操作的特征在于使用选自N2,H2和He的还原气体。
-
公开(公告)号:KR1020010018102A
公开(公告)日:2001-03-05
申请号:KR1019990033921
申请日:1999-08-17
Applicant: 현대자동차주식회사
Abstract: PURPOSE: A bronze based sintered material for bush of an exhaust gas recirculation valve is provided to decrease a coefficient of thermal expansion and improve lubricating properties and indentation hardness by adding certain amounts of C and Fe to an existing bronze based sintered material alloy material base in a bronze based sintered material for bush of an exhaust gas recirculation valve. CONSTITUTION: A bronze based sintered material for bush of an exhaust gas recirculation valve contains a main material of Cu, 0.8 to 1.5 wt.% of C, 1.0 to 1.8 wt.% of Fe, 8.0 to 11.0 wt.% of Sn, and 3 wt.% of other impurities. The bronze based sintered material for bush of an exhaust gas recirculation valve has a density of 6.8 to 7.2 g/mm3. A bronze based sintered material for bush of an exhaust gas recirculation valve solves problems of breakaway or burning and heat cracks due to insufficient indentation strength and demonstrates original exhaust gas recirculation function, thereby doubling effect of smoke improvement.
Abstract translation: 目的:提供一种用于废气再循环阀衬套的青铜基烧结材料,以通过向现有的青铜基烧结材料合金材料基底添加一定量的C和Fe来降低热膨胀系数,并提高润滑性能和压痕硬度 用于排气再循环阀衬套的青铜基烧结材料。 构成:用于废气再循环阀衬套的青铜基烧结材料包含Cu的主要材料,C:0.8-1.5重量%,C:1.0-1.8重量%,Sn:8.0-1.11重量%,Sn: 3重量%的其他杂质。 用于废气再循环阀衬套的青铜基烧结材料的密度为6.8至7.2g / mm 3。 用于废气再循环阀衬套的青铜基烧结材料解决了由于压痕强度不足而导致的分离或燃烧和热裂纹问题,并表现出原有的废气再循环功能,从而提高烟气的双重效果。
-
公开(公告)号:KR1019990019266A
公开(公告)日:1999-03-15
申请号:KR1019970042621
申请日:1997-08-29
Applicant: 현대자동차주식회사
Inventor: 조봉래
IPC: B60H1/00
Abstract: 본 발명은 자동차용 공조장치에 관한 것으로, 자동차 실내의 쾌적함을 유지하기 위하여 실내로 공급되는 에어컨의 냉기나 히터의 온기의 공급을 위한 공조장치의 구조를 단순하도록 일체화하여 설치공간의 확보가 용이하며 공기의 누설에 따른 손실을 최대한 방지할 수 있도록 하기 위하여 제1댐퍼에 의하여 해당부위로 공기를 선택적으로 공급하는 분출구가 상측에 구비되며 하측에는 외부의 공기를 흡입하여 송풍구를 통하여 공급하는 송풍기가 구비되는 케이스 본체와, 상기 케이스 본체 내부의 상기 제1댐퍼의 하측에는 통로의 개폐와 공기의 통과를 제어하는 제2댐퍼 및 상기 제2댐퍼에 의하여 공기의 유입이 제어되는 히터가 구비되고 상기 제2댐퍼의 하측에는 통로의 개폐와 공기의 통과를 제어하는 제3댐퍼 및 상가 제3댐피에 의하여 공기의 유� �이 제어되는 증발기를 구비하여 상기 송풍기에 의하여 케이스본체의 내부로 유입되는 공기를 제2댐퍼 및 제3댐퍼에 의하여 히터 및 증발기로 유입되는 것을 제어하며 제1댐퍼에 의하여 해당부위로 공급되도록 한 자동차용 공조장치에 관한 것이다.
-
公开(公告)号:KR1019970011544A
公开(公告)日:1997-03-27
申请号:KR1019950026741
申请日:1995-08-26
Applicant: 현대자동차주식회사
Inventor: 조봉래
IPC: F16H7/08
Abstract: 본 발명은 컴푸레서 장착용 구조물(10)에 관한 것이다. 힌지축(22)을 중심으로 제2브래킷(14)을 소정의 지점으로 선회시키고나서, 제1브래킷(12)의 구멍(20)과 제2브래킷(14)의 궁형 슬로트(18)를 관통하여 보울트를 통과시키고 반대쪽에서 너트로 조임으로써, 벨트의 장력조절이 이루어지게 된다.
-
-
-
-
-