Abstract: The polymerized phosphate salt anticorrosive is produced by mixing 60-90 wt.% NaH2PO4, 0-10 wt.% Na2H2PO4, 0-20 wt.% zinc carbonate (ZnCO3), 1-5 wt.% calcium carbonate (CaCO3), 1-5 wt.% aluminium oxide (Al2O3) and 0-5 wt.% silica, drying the mixture, heating it at 800-1000 deg.C and 10 deg.C/min heating rate, and polymerizing it at 850 deg.C for 0.5-1 hr. The anticorrosive has a good anticorrosion effect, and is useful for drinking and industrial water systems.
Abstract translation: 聚合的磷酸盐防腐剂通过混合60-90重量%的NaH 2 PO 4,0-10重量%的Na 2 H 2 PO 4,0-20重量%的碳酸锌(ZnCO 3),1-5重量%的碳酸钙(CaCO 3),1 -5重量%的氧化铝(Al 2 O 3)和0-5重量%的二氧化硅,干燥混合物,加热至800-1000℃和10℃/分钟加热速率,并在850℃聚合 0.5-1小时。 防腐蚀具有良好的防腐效果,适用于饮用水和工业用水系统。
-
公开(公告)号:KR1019920010304B1
公开(公告)日:1992-11-26
申请号:KR1019900012093
申请日:1990-08-07
Applicant: 한국과학기술연구원
IPC: C23F11/18
Abstract: A rustproofing agent containing polymerized phosphate is manufactured by (A) mixing raw materials in a proper ration, (B) drying and high-temperature polymerizing mixed raw materials in a S- type cylindrical polymerization reactor, (C) molding the polymerized mixture in the form of glass beads in a molder of which the temperature is kept at 150-300 deg.D, and (D) cooling the product to a constant temperature. The polymerization reactor, which is equipped with a distributor to uniformly distribute melt product successively downwards, consists of four heating zones of temperatures of 700-800 deg.C, 800-850 deg.C, 800-900 deg.C, and 800-1000 deg.C.
Abstract translation: 含有聚合磷酸盐的防锈剂是通过(A)以适当的比例混合原料,(B)在S-型圆柱形聚合反应器中的干燥和高温聚合混合原料,(C)将聚合的混合物在 在其中温度保持在150-300度的成型机中的玻璃珠的形式,和(D)将产物冷却至恒定温度。 装配有分配器以均匀分布熔体产物的聚合反应器连续向下包括温度为700-800℃,800-850℃,800-900℃和800℃的四个加热区, 1000摄氏度
-
-