Abstract:
A threaded joint for steel pipes having excellent galling resistance, rust preventing properties, and airtightness without using a compound grease comprises a pin and a box each having a threaded portion and an unthreaded metal-to-metal contact portion serving as contact surfaces. The contact surfaces of at least one of the pin and the box are coated with a multi-layered structure comprising, from the bottom, a first layer formed from a first metal or alloy, a second layer formed from a second metal or alloy which is softer than the first metal or alloy, and an uppermost layer of a solid lubricating coating comprising a lubricating powder in an organic or inorganic binder.
Abstract:
A threaded joint for steel pipes comprised of a pin 1 and a box 2 each having a threaded portion (1a, 2a) and an unthreaded metal contact portion (1b, 2b) exhibits adequate leakage resistance and galling resistance when used for makeup of oil country tubular goods with application of a green dope or even without any dope. The threaded joint has a first plating layer of Sn—Bi alloy plating or Sn—Bi—Cu alloy plating formed on the contact surface of at least one of the pin 1 and the box 2. The first plating layer may have a second plating layer selected from Sn plating, Cu plating, and Ni plating on its lower side and at least one layer of a lubricating coating, and particularly a solid lubricating coating, on its upper side.
Abstract:
A method of making a thermal spray powder is provided. The method comprises: providing a powder comprising a plurality of porous particles; infiltrating a mixture comprising a solvent and a plurality of solid lubricant particles into the porous particles; and heating the powder to a temperature sufficient to evaporate the solvent. The method of forming a wear-resistant coating is provided. The method comprises: providing a thermal spray powder; heating the thermal spray powder; and accelerating the thermal spray powder from a thermal spray gun onto the substrate, to form a deposit. Yet another embodiment provides a wear resistant coating. The wear resistant coating is formed by thermally spraying the thermal spray powder.
Abstract:
A process is disclosed for manufacturing a lubricant composition comprising combining a superabsorbent polymer with a material for decreasing friction between moving surfaces. The superabsorbent polymer absorbs from about 25 to greater than 100 times its weight in water and may comprise a polymer of acrylic acid, an acrylic ester, acrylonitrile or acrylamide, including co-polymers thereof or starch graft co-polymers thereof or mixtures thereof. A product produced by the process includes the material for decreasing friction comprising a petroleum lubricant containing an additive, water containing an additive, synthetic lubricant, grease, solid lubricant or metal working lubricant, wherein the synthetic lubricant, grease, solid lubricant or metal working lubricant optionally contain an additive. A process comprising controlling the delivery of a lubricant to at least one of two moving surfaces in order to decrease friction between said moving surfaces, is also disclosed. This process includes applying the lubricant composition to at least one of the surfaces. The lubricant composition in this instance comprises a superabsorbent polymer combined with a material for decreasing friction between moving surfaces, wherein the material for decreasing friction comprises a petroleum lubricant, water, synthetic lubricant, grease, solid lubricant or metal working lubricant, and optionally an additive.
Abstract:
Systems, compositions, methods, etc., that provide significantly enhanced tribological properties to a target substrate such as metal, plastic, wood, glass, etc., by bombarding or showering the target material with bombardment particles substantially saturated with a desirable lubricant composition, typically comprising at least one primary lubricant such as a molybdenum disulphide (MoS2) and at least one polymeric lubricant, such as polytetrafluoroethylene (PTFE), such that the lubricant composition imbeds into the surface of the target material (also called a target substrate).
Abstract translation:系统,组合物,方法等通过用理想的润滑剂组合物基本上饱和的轰击颗粒轰击或淋浴目标材料,为目标基材(例如金属,塑料,木材,玻璃等)提供显着增强的摩擦学性能, 通常包括至少一种主要润滑剂,例如二硫化钼(MoS 2 H 2)和至少一种聚合物润滑剂,例如聚四氟乙烯(PTFE),使得润滑剂组合物嵌入目标材料的表面 (也称为靶基板)。
Abstract:
A method for protecting a metal surface from galling and corrosion includes a step of providing a protective dry film on the metal surface. The film includes a solid lubricant and a conducting polymer, the conducting polymer having lubricant properties and being capable of binding the solid lubricant to the metal surface. Threaded metal joint surfaces coated with the film are capable of resisting galling under high pressure and high torque conditions, even after several fastening and unfastening operations or over a long period of time. Protection from corrosion is also provided by the film. The method and film are economical in that only a single layer of protective compound need be applied in order to provide metal surfaces with both lubrication and protection against corrosion, and problems such as removal or leakage, which are associated with protective compounds that use oils, are avoided. Additionally, the dry film is advantageous because it does not contain heavy metals that are harmful to the environment.
Abstract:
A sliding bearing having excellent initial conformability and seizure resistance as well as high durability and heat resistance is provided. A sliding bearing comprising a coating layer containing a resin and a solid lubricant formed on a bearing alloy layer, characterized in that the resin of said coating layer is a resin having a glass transition temperature of from 150° C. to 250° C. which has a great elongation at high temperatures.
Abstract:
The production of solid lubricant agglomerates by combining solid lubricant powder, an inorganic binder, other fillers if optionally desired, and a liquid to form a mixture, and driving off the liquid to form dry agglomerates which are subsequently classified by size or milled and classified by size to yield agglomerates of a desired size range. These agglomerates are then treated to stabilize the binder, thereby strengthening the binder and rendering it nondispersible in the liquid. The undesired size ranges can be readily recycled because the agglomerates with untreated binder can be reprocessed, thereby promoting high recovery rates.
Abstract:
A process is disclosed for manufacturing a lubricant composition comprising combining a superabsorbent polymer with a material for decreasing friction between moving surfaces. The superabsorbent polymer absorbs from about 25 to greater than 100 times its weight in water and may comprise a polymer of acrylic acid, an acrylic ester, acrylonitrile or acrylamide, including co-polymers thereof or starch graft co-polymers thereof or mixtures thereof. A product produced by the process includes the material for decreasing friction comprising a petroleum lubricant containing an additive, water containing an additive, synthetic lubricant, grease, solid lubricant or metal working lubricant, wherein the synthetic lubricant, grease, solid lubricant or metal working lubricant optionally contain an additive. A process comprising controlling the delivery of a lubricant to at least one of two moving surfaces in order to decrease friction between said moving surfaces, is also disclosed. This process includes applying the lubricant composition to at least one of the surfaces. The lubricant composition in this instance comprises a superabsorbent polymer combined with a material for decreasing friction between moving surfaces, wherein the material for decreasing friction comprises a petroleum lubricant, water, synthetic lubricant, grease, solid lubricant or metal working lubricant, and optionally an additive.
Abstract:
A process is disclosed for manufacturing a lubricant composition comprising combining a superabsorbent polymer with a material for decreasing friction between moving surfaces. The superabsorbent polymer absorbs from about 25 to greater than 100 times its weight in water and may comprise a polymer of acrylic acid, an acrylic ester, acrylonitrile or acrylamide, including co-polymers thereof or starch graft co-polymers thereof or mixtures thereof. A product produced by the process includes the material for decreasing friction comprising a petroleum lubricant containing an additive, water containing an additive, synthetic lubricant, grease, solid lubricant or metal working lubricant, wherein the synthetic lubricant, grease, solid lubricant or metal working lubricant optionally contain an additive. A process comprising controlling the delivery of a lubricant to at least one of two moving surfaces in order to decrease friction between said moving surfaces, is also disclosed. This process includes applying the lubricant composition to at least one of the surfaces. The lubricant composition in this instance comprises a superabsorbent polymer combined with a material for decreasing friction between moving surfaces, wherein the material for decreasing friction comprises a petroleum lubricant, water, synthetic lubricant, grease, solid lubricant or metal working lubricant, and optionally an additive.