公开(公告)号:KR1020120045211A
公开(公告)日:2012-05-09
申请号:KR1020100106612
申请日:2010-10-29
CPC classification number: A01K59/00
Abstract: PURPOSE: An automatic honeybee separation device for bee keeping is provided to enhance work efficiency by reducing time and labor. CONSTITUTION: An automatic honeybee separation device for bee keeping comprises a base(10), a main frame(20), a supporting part(30), and a brush part. In the base, a plurality of grips is installed at a constant interval so that a user can grip a comb. The main frame forms a space so that the base can be placed inside. The supporting part is installed in the main frame to be reciprocated. The brush part is installed to be ascended and descended in the upper part of the base.
Abstract translation: 目的:提供一种用于养蜂的自动蜜蜂分离装置,通过减少时间和劳动来提高工作效率。 构成:用于蜜蜂保持的自动蜜蜂分离装置包括基座(10),主框架(20),支撑部件(30)和刷子部分。 在基座中,以一定的间隔安装多个把手,以便使用者可以握住梳子。 主框架形成一个空间,使底座可以放在里面。 支撑部件安装在主框架中以便往复运动。 刷子部分安装在基座的上部上升和下降。
-
公开(公告)号:KR1019930003662B1
公开(公告)日:1993-05-08
申请号:KR1019900008306
申请日:1990-06-07
Applicant: 박창엽
IPC: C04B35/46
Abstract: n electrostriction ceramics is composed of the powder mixture including lead oxide, niobium oxide, titanium oxide (titania), barium carbonate, zinc oxide, and 0.4 wt.% yttrium oxide (yttria) as an additive. The electrostrictive strain ceramics for a microdisplacement device has the general formula of 0.85Pb(Zn1/3Nb2/3)O3- 0.10BaTiO3-0.05PbTiO3. The additive increases the density of the electrostriction ceramic body and the permittivity by generating the space charge polarization between grain boundary layers.
Abstract translation: n电致伸缩陶瓷由包含氧化铅,氧化铌,氧化钛(二氧化钛),碳酸钡,氧化锌和0.4重量%氧化钇(氧化钇)作为添加剂的粉末混合物组成。 用于微位移器件的电致伸缩应变陶瓷具有0.85Pb(Zn1 / 3Nb2 / 3)O3-0.10BaTiO3-0.05PbTiO3的通式。 通过在晶界层之间产生空间电荷极化,添加剂增加了电致伸缩陶瓷体的密度和介电常数。
-
公开(公告)号:KR1019930012002B1
公开(公告)日:1993-12-23
申请号:KR1019910006516
申请日:1991-04-23
Applicant: 박창엽
IPC: C04B35/00
Abstract: A composition of piezoelectric ceramic for elastic surface wave device is 0.05Pb(Sn1/2Sb1/2)O3-0.35PbTiO3-0.6PbZrO3 + 0.4 wt.% MnO2 added with 0.05 1.2 wt.% Cr2O3. It is prepared by (1) weighing and mixing more than 99% of purity raw materials such as PbO, TiO2, ZrO2, SnO2, Sb2O3, MnO2 and Cr2O3 (2) ball milling the raw materials with zirconia media in distilled water for 24 hours, (3) calcining in an alumina crucible at 900≦̸C for 2 hours, (4) remilling and hot pressing under 600 kg/cm2 and (5) sintering in vacuum atmosphere, at 1,150≦̸C for 50 minutes.
Abstract translation: 用于弹性表面波器件的压电陶瓷组合物为0.05Pb(Sn1 / 2Sb1 / 2)O3-0.35PbTiO3-0.6PbZrO3 +添加0.05 1.2重量%Cr2O3的0.4重量%MnO2。 通过(1)称量和混合99%以上的纯度原料如PbO,TiO2,ZrO2,SnO2,Sb2O3,MnO2和Cr2O3(2),将原料与氧化锆介质在蒸馏水中球磨24小时 ,(3)在900℃下在氧化铝坩埚中煅烧2小时,(4)在600kg / cm2下再烧结和热压,和(5)在真空气氛中,在1,150℃下烧结50分钟。
-
-
公开(公告)号:KR1019930001349B1
公开(公告)日:1993-02-26
申请号:KR1019900008307
申请日:1990-06-07
Applicant: 박창엽
IPC: G10K9/12
Abstract: A electrostrictive buzzer consists of metal substrate (22) supported on ring-type supporter (10); press-junctioned ceramic plate (12) which is concentrically arrayed on the center of (11); electrode (13) attached to the side of (12) opposite to (11); AC power source (15) and capacitors (C1,C2) connected between (13) and (11); and DC bias power source (14) connected between (13) and (11). The ceramic plate (12) is composed of a ceramic of formula 0.85 Pb (Zn1/3Nb2/3)O3 - 0.10 BaTiO3 - 0.05 PbTiO3 + X wt.% Y2O3, where X= 0.2, 0.4, 0.6, 1, 1.2, 1.6 or 2.
Abstract translation: 电致伸缩蜂鸣器由支撑在环型支撑件(10)上的金属基底(22)组成。 同心排列在(11)的中心的压接陶瓷板(12); 附着在与(11)相对的(12)侧的电极(13); 连接在(13)和(11)之间的交流电源(15)和电容器(C1,C2) 和连接在(13)和(11)之间的直流偏压电源(14)。 陶瓷板(12)由式为0.85 Pb(Zn1 / 3Nb2 / 3)O3 - 0.10 BaTiO3 - 0.05 PbTiO3 + X重量%Y2O3的陶瓷构成,其中X = 0.2,0.4,0.6,1,1.2,1.6 或2。
-
-
公开(公告)号:KR1019890003508B1
公开(公告)日:1989-09-23
申请号:KR1019870003258
申请日:1987-04-06
Applicant: 박창엽
Inventor: 박창엽
IPC: C04B35/00
Abstract: A making method for a electric optical transparent ceramic with high transparency comprising thermal pressing of ceramic specimen made from oxidated lead powder, oxidated titanium powder, oxidated Zr powder and oxidated Ra with the composition Pb1-xLax (ZryTi1-y)1-x/ 4O3(x=0.07-0.09, y=0.65) under 200kg/cm2 in heating at a rate 200-400≦̸C/hr in a graphite mold until the mximum sintering temperature 1100- 1200≦̸C is maintained for 30-90 minutes and followed by cooling at a rate 200-400 C is characterized by high transparency and increase of hardness and density.
Abstract translation: 一种具有高透明度的电光透明陶瓷的制造方法,包括由氧化铅粉末,氧化钛粉末,氧化锆粉末和氧化的Ra与Pb1-xLax(ZryTi1-y)1-x / 4O3 (x = 0.07-0.09,y = 0.65)在200kg / cm2的加热条件下以200-400< 1lE; C / hr在石墨模具中直到最小烧结温度1100-1200< NlE; C保持30-90分钟,随后 通过以200-400℃的速度冷却,其特征在于高透明度和硬度和密度的增加。
-
-
-
-
-
-
-