보행로 포장재 조성물
    1.
    发明授权
    보행로 포장재 조성물 有权
    路面构成的组成

    公开(公告)号:KR100938212B1

    公开(公告)日:2010-01-22

    申请号:KR1020090068585

    申请日:2009-07-27

    Inventor: 전상무 설태윤

    Abstract: PURPOSE: A pavement composition of a pedestrian path is provided to prevent the sliding accident by improving the skid resistance with eco-friendly aggregate, to buffer the shock added to feet of a pedestrian in walking after construction, and to prevent the injury of a pedestrian in an accident. CONSTITUTION: A pavement composition of a pedestrian path comprises a main material composed of modified epoxy pre-polymer resin of 20~40 weight%, eco-friendly aggregate of 22~27 weight%, recycled chips of 22~27 weight%, filler of 13~18 weight%, pigment of 1.5~5 weight%, and additive of 1.5~3 weight%, and polyurethane pre-polymer of 2~20 weight parts having isocyanate-end group as a hardener.

    Abstract translation: 目的:提供行人通道的路面构成,以防止滑行事故,通过改善耐环保骨料的抗滑性,缓解行人在步行后施加的冲击增加的冲击,防止行人受伤 在事故中 构成:人行道路面构成包括由20〜40重量%的改性环氧树脂预聚物树脂,22〜27重量%的环保骨料,22〜27重量%的回收芯片,填料 13〜18重量%,1.5〜5重量%的颜料,1.5〜3重量%的添加剂,2〜20重量份的聚氨酯预聚物,具有异氰酸酯端基作为硬化剂。

    자전거 전용 도로용 포장재 조성물
    2.
    发明授权
    자전거 전용 도로용 포장재 조성물 有权
    BICYCLE路径的组合

    公开(公告)号:KR100937181B1

    公开(公告)日:2010-01-19

    申请号:KR1020090068584

    申请日:2009-07-27

    Inventor: 전상무 설태윤

    CPC classification number: E01C15/00 E01C7/30 E01C7/356 E01C13/065

    Abstract: PURPOSE: Paving composition for a bicycle path is provided to improve the shock resistance and the durability without a crack or omission. CONSTITUTION: Paving composition for a bicycle path is composed of quick-hardening resin 30~60 weight%, aggregate 20~30 weight%, filler 15~25 weight%, paint 2~5%, anti-foaming agent 1~3 weight%, UV blocking agent 1~4 weight%, and oxygen barrier agent 1~3 weight%. The quick-hardening resin is manufactured by mixing low-viscosity methyl methacrylate resin 50~80 weight%, thermosetting resin or synthetic resin selected from high-viscosity methyl methacrylate 19.5~48 weight%, and hardening accelerator 0.5~2%.

    Abstract translation: 目的:提供用于自行车路径的铺路组合物,以提高抗冲击性和耐久性,而不会产生裂缝或遗漏。 规定:自行车路径的铺路组合物由快硬硬化树脂30〜60重量%,骨料20〜30重量%,填料15〜25重量%,涂料2〜5%,消泡剂1〜3重量% ,紫外线阻断剂1〜4重量%,氧气阻隔剂1〜3重量%。 通过混合低粘度甲基丙烯酸甲酯树脂50〜80重量%,热固性树脂或选自高粘度甲基丙烯酸甲酯19.5〜48重量%的合成树脂和硬化促进剂0.5〜2%制造快速硬化树脂。