公开(公告)号:JP5419231B2
公开(公告)日:2014-02-19
申请号:JP2011169523
申请日:2011-08-02
Applicant: 黒崎播磨株式会社
CPC classification number: B22D41/02 , C04B35/013 , C04B35/20 , C04B35/6269 , C04B35/6303 , C04B35/6306 , C04B35/6316 , C04B35/63452 , C04B35/63476 , C04B35/6348 , C04B35/63496 , C04B35/636 , C04B35/66 , C04B2235/3206 , C04B2235/3208 , C04B2235/3217 , C04B2235/3409 , C04B2235/3427 , C04B2235/3445 , C04B2235/3454 , C04B2235/365 , C04B2235/5427 , C04B2235/5472 , C04B2235/96 , C04B2235/9684 , C21C5/44 , F27D1/10 , F27D1/16 , F27D2001/1605
-
公开(公告)号:JP5283849B2
公开(公告)日:2013-09-04
申请号:JP2007055809
申请日:2007-03-06
Abstract: PROBLEM TO BE SOLVED: To provide a kneading method, a spraying construction method and its device capable of continuously performing direct kneading from a fireproofing material regarding a continuous kneading method for a monolithic refractory and its repair method. SOLUTION: The continuous kneading method for the refractory for continuously obtaining a slurry-like kneaded material while continuously supplying the fireproofing material and water, consists of a material conveying process and a material kneading process. In the material conveying process, the continuously supplied fireproofing material and water are conveyed downstream while being mixed/dispersed by a mixing means. In the material kneading process, a mixture of the fireproofing material and water conveyed from the material conveying process is fed downstream while being kneaded by a kneading means. COPYRIGHT: (C)2008,JPO&INPIT
-
-
9.
-
-
-
-
-
-
-
-
-