公开(公告)号:KR1020000017855A
公开(公告)日:2000-04-06
申请号:KR1019990060701
申请日:1999-12-18
Applicant: 강병희
IPC: C04B16/08
CPC classification number: C04B18/023 , C04B16/08 , C04B28/02 , C04B2111/40 , Y02W30/94 , C04B18/20 , C04B2201/50 , Y02W30/96 , C04B14/00 , C04B18/146 , C04B40/0028
Abstract: PURPOSE: A preparation method of lightweight concrete by using an ingot fused waste of expanded polystyrene is provided which improves compression strength. CONSTITUTION: A process for making lightweight concrete comprises: (a)a process for producing an ingot by fusing waste of expanded polystyrene with a frictional heat of 80-100°C through a miniature instrument of expanded polystyrene and extruding; b)a process for crushing the ingot in a plastic crusher mill of rotary-type; c)a process for adjusting grading of the crushed ingot where the biggest ingot is about 20 mm; d)a process for blending the ingot with cement powder, water, an additive, and silica hume for 6 min in a forced mixer. The weight of lightweight concrete by using the reclaimed aggregate of waste expanded polystyrene is reduced to 40-45%.
Abstract translation: 目的:提供通过使用发泡聚苯乙烯的锭熔融废料制备轻质混凝土的制备方法,其提高抗压强度。 构成:制造轻质混凝土的方法包括:(a)通过发泡聚苯乙烯和挤出的微型仪器,通过使80-100℃的摩擦热熔化发泡聚苯乙烯的废料来生产锭的方法; b)在旋转式塑料破碎机中破碎锭的方法; c)调整最大锭约20毫米的压块的分级的方法; d)在强制混合器中将锭与水泥粉末,水,添加剂和硅橡胶混合6分钟的方法。 通过使用废弃聚苯乙烯的回收骨料,轻质混凝土的重量减少到40-45%。
-
公开(公告)号:KR1020000006973A
公开(公告)日:2000-02-07
申请号:KR1019990050957
申请日:1999-11-16
Applicant: 강병희
IPC: B29B17/00
CPC classification number: C04B28/00 , C04B2201/00 , C04B14/00 , C04B16/08 , C04B38/061 , C04B40/0028 , C04B40/0067
Abstract: PURPOSE: A concrete brick is provided to remarkably decrease the weight of a brick by manufacturing a brick using ingot which is made by melting the waste styrofoam, and to promote the thermal insulating effectiveness. CONSTITUTION: The concrete brick is manufactured by: mixing usual aggregate with the waste styrofoam reproduced aggregate which having its particle sized to be modulated according to the standard of aggregate about concrete bricks by pulverizing and processing the waster styrofoam ingot using a crusher; mixing cement to have 1:7 of ratio of the waste styrofoam to the reproduced aggregate; pressurizing using a vibrating press. Therefore, the concrete brick using the waste styrofoam reproduced aggregate meets the standard of KS F 4004, and particularly having 1120-2100 kg/m¬3 of unit volume weight, 93-320 kg/cm¬2 of compressing strength; 6.2-11.7 % of absorption rate, and 0.28-1.35 kcal/mh°C of heat conduction rate.
Abstract translation: 目的:提供一种混凝土砖,通过使用通过熔化废发泡胶制成的锭来制造砖,显着降低砖的重量,并提高隔热效果。 构成:混凝土砖的制造方法是:使用破碎机粉碎和处理废发泡胶锭,将通常的聚集体与废聚苯乙烯泡沫塑料再生骨料混合,将其粒径根据混凝土骨料的标准调整; 混合水泥以废弃聚苯乙烯与废弃聚苯乙烯的比例为1:7; 使用振动压力机进行加压。 因此,使用废发泡聚苯乙烯再生骨料的混凝土砖满足KS F 4004的标准,特别是具有1120-2100kg / m 3的单位体积重量,93-320kg / cm 2的压缩强度; 吸收率为6.2-11.7%,导热率为0.28-1.35 kcal / mh。
-