저 품위 철광석을 사용한 식생 콘크리트블록 제조방법
    1.
    发明公开
    저 품위 철광석을 사용한 식생 콘크리트블록 제조방법 有权
    使用低等级铁矿石生产木质混凝土块的制造方法

    公开(公告)号:KR1020100025438A

    公开(公告)日:2010-03-09

    申请号:KR1020080084174

    申请日:2008-08-27

    Abstract: PURPOSE: A method of manufacturing planting concrete block using low grade iron ore is provided to replace gravel as a planting block, and to improve durability and environment-friendly property. CONSTITUTION: A method of manufacturing planting concrete block using low grade iron ore comprises the following steps: mixing 60~80wt% of low grade iron ore, 20~35wt% of portland cement, and 3~10wt% of water to prepare iron ore mortar(S10); pouring the iron ore mortar and a water-soluble light aggregate in a volume ratio of 100:10~15 into a block molding frame and curing to manufacture a concrete block with pores(S20); and completing the concrete block by neutralizing the strong alkali nature of the block using autoclave curing.

    Abstract translation: 目的:提供一种使用低品位铁矿石生产种植混凝土块的方法,以取代砾石作为种植块,提高耐久性和环境友好性。 构成:使用低品位铁矿石生产混凝土块的方法包括:将60〜80wt%的低品位铁矿石,20〜35wt%的波特兰水泥和3〜10wt%的水混合制备铁矿砂浆 (S10); 将铁矿砂浆和体积比为100:10〜15的水溶性轻骨料倒入块状成型框中,固化,制成具有孔隙的混凝土块(S20); 并通过使用高压釜固化中和块的强碱性来完成混凝土块。

    저 품위 철광석을 사용한 식생 콘크리트블록 제조방법
    2.
    发明授权
    저 품위 철광석을 사용한 식생 콘크리트블록 제조방법 有权
    低品位铁矿石生产混凝土块的制造方法

    公开(公告)号:KR101021525B1

    公开(公告)日:2011-03-16

    申请号:KR1020080084174

    申请日:2008-08-27

    Abstract: 본 발명은 제철의 재료로 부적절하여 폐광에 적치되어 환경 문제를 야기하는 저 품위 철광석을 이용하여 충분한 공극을 제공하고, 콘크리트가 지닌 강알칼리성을 중성화처리하여 장기적으로 중성을 성질을 유지하여 식생환경을 지속적으로 유지시키고, 내구성과, 내마모성이 개선된 저 품위 철광석을 사용한 식생 콘크리트블록 제조방법에 관한 것으로, 이를 위해 60중량% 내지 75중량%를 갖는 저 품위 철광석과, 20중량% 내지 35중량%를 갖는 포틀랜드시멘트와, 3중량% 내지 10중량%를 갖는 물을 혼합하여 철광석모르타르를 제조하는 단계;(S10)와, 블록성형틀에 철광석모르타르의 부피 100에 대해 수용성 중공경량골재를 10 내지 15부피비로 타설하고 양생하는 과정을 거쳐 일정공극이 형성된 콘크리트블록을 제조하는 단계;(S20)와, 상기 콘크리트블록을 오토클레이브 양생을 통해 중성화시켜 완성하는 단계;(S30)를 포함하여 구성되는 것을 특징으로 한다.
    저 품위 철광석, 식생, 콘크리트, 블록,