햅틱 소자 적용을 위한 적층 액츄에이터용 압전체 및 이의 제조방법
    1.
    发明公开
    햅틱 소자 적용을 위한 적층 액츄에이터용 압전체 및 이의 제조방법 有权
    压电材料及其制造方法使用多层致动器

    公开(公告)号:KR1020130102222A

    公开(公告)日:2013-09-17

    申请号:KR1020120023283

    申请日:2012-03-07

    Abstract: PURPOSE: A piezoelectric material for a multilayer actuator in a haptic device and a fabrication method thereof are provided to minimize power consumption by performing a sintering process at a low temperature. CONSTITUTION: Copper oxide of 0.1 to 10 mole% is added to a compound. The compound is indicated as a chemical formula 1. A haptic device is laminated by using a piezoelectric material. A mixture is manufactured by a wet mixing process (S110). A first powder is formed by drying the mixture (S120). [Reference numerals] (S110) Step where a below-mentioned compound is produced by wet-mixing raw powder including PbO,ZrO_2,TiO_2,NiO,ZnO, and Nb_2O_5 according to a mol rate; (S120) Step where the compound is dried and calcined at around 700-1,000 °C in order to create a first powder; (S130) Step where copper oxide of 0.1 to 10 mole % is added to the first powder and the powder is wet-mixed and dried to produce a second powder; (S140) Step where the second powder is pressed and sintered at around 700-1,000 °C in order to create a piezoelectric body

    Abstract translation: 目的:提供一种用于触觉装置中的多层致动器的压电材料及其制造方法,以通过在低温下进行烧结工艺来最小化功率消耗。 构成:向化合物中加入0.1〜10摩尔%的氧化铜。 该化合物表示为化学式1.通过使用压电材料层压触觉装置。 通过湿式混合法制造混合物(S110)。 通过干燥混合物形成第一粉末(S120)。 (S110)根据摩尔比将包含PbO,ZrO_2,TiO_2,NiO,ZnO,Nb_2O_5的原料粉末混合,制造下述化合物的工序; (S120)步骤,其中将化合物干燥并在约700-1000℃下煅烧以产生第一粉末; (S130)向第一粉末中添加0.1〜10摩尔%的氧化铜的步骤,将粉末进行湿式混合干燥,得到第二粉末; (S140)为了形成压电体,将第二粉末压制并烧结在约700-1000℃的步骤

Patent Agency Ranking