公开(公告)号:KR1019930000594B1
公开(公告)日:1993-01-25
申请号:KR1019900006860
申请日:1990-05-14
Applicant: 대한민국(관리부서:과학기술부장관)
IPC: G21F9/28
Abstract: This method pulverizes the organic ion-exchange resin having the average diameter of 300-1500μm into the extent of 10-150μm, pref. 5-50μm. The method comprises (1) adjusting the water content of the organic ion-exchange resin to 30-60 wt.%, (b) uniformly mixing the resin with dry ice and (c) continuously pulverizing the resultant mixture using a stone mill at the room temperature.
Abstract translation: 该方法将平均直径为300-1500μm的有机离子交换树脂粉碎成10-150μm的范围。 5-50μm。 该方法包括(1)将有机离子交换树脂的含水量调节至30-60重量%,(b)将树脂与干冰均匀混合,(c)使用石磨机连续粉碎所得混合物 室内温度。
-
-
公开(公告)号:KR1019910020749A
公开(公告)日:1991-12-20
申请号:KR1019900006860
申请日:1990-05-14
Applicant: 대한민국(관리부서:과학기술부장관)
IPC: G21F9/28
Abstract: 내용 없음
-
-
-
公开(公告)号:KR100061490B1
公开(公告)日:1993-04-19
申请号:KR1019900006860
申请日:1990-05-14
Applicant: 대한민국(관리부서:과학기술부장관)
IPC: G21F9/28
-
-
-
-
-
-
-