리튬이차전지용 비수 전해액 첨가제
    2.
    发明公开
    리튬이차전지용 비수 전해액 첨가제 无效
    锂二次电池非电解电解质的添加剂

    公开(公告)号:KR1020140118517A

    公开(公告)日:2014-10-08

    申请号:KR1020130034595

    申请日:2013-03-29

    Abstract: The present invention relates to a non-aqueous electrolyte for a battery, and the non-aqueous electrolyte is formed by adding a compound of chemical formula 1 to a non-aqueous electrolyte for a battery, which comprises an organic solvent and a lithium salt. The present invention provides a non-aqueous electrolyte for a lithium secondary battery, which improves cycle characteristics and low-temperature output performances simultaneously. In chemical formula 1, n is 0-3 and R is CH_3 or CH(CH_3)_2.

    Abstract translation: 本发明涉及一种用于电池的非水电解质,非水电解质通过将化学式1的化合物加入到包含有机溶剂和锂盐的电池的非水电解质中而形成。 本发明提供了一种用于锂二次电池的非水电解质,其同时改善了循环特性和低温输出性能。 在化学式1中,n为0-3,R为CH 3或CH(CH 3)2。

    고순도 트리스(트리알킬실릴)포스파이트의 제조 방법
    3.
    发明授权
    고순도 트리스(트리알킬실릴)포스파이트의 제조 방법 有权
    高纯度三(三烷基甲硅烷基)亚磷酸酯的制备方法

    公开(公告)号:KR101249361B1

    公开(公告)日:2013-04-03

    申请号:KR1020100128770

    申请日:2010-12-16

    Abstract: 본 발명은 별도의 촉매 및 용매 없이 트리스(트리알킬실릴)포스파이트를 제조하는 방법에 관한 것으로, 상세하게는 아인산 및 헥사알킬디실라잔 유도체를 반응시킨 다음, 연속적으로 나트륨 금속을 첨가하여 고순도 트리스(트리알킬실릴)포스파이트를 제조하는 방법에 관한 것이다.
    촉매 및 용매없이 이용한 본 발명은 짧은 시간내에 합성하고, 나트륨 금속을 이용하여 정제 없이 한번 반응으로 고순도 화합물을 합성할 수 있다. 또한, 기존에 사용하는 촉매 및 용매 사용이 없기에 산업 공정상 용이하다는 장점을 가지고 있다. 따라서 화학 공업 분야에서 유용하게 활용될 수 있다.

    리튬 프탈라토보레이트 화합물을 함유하는 전해액 및 이를 이용한 이차 전지
    5.
    发明公开
    리튬 프탈라토보레이트 화합물을 함유하는 전해액 및 이를 이용한 이차 전지 有权
    包含对苯二酸酯化合物的电解质和使用其的二次电池

    公开(公告)号:KR1020140120174A

    公开(公告)日:2014-10-13

    申请号:KR1020130035936

    申请日:2013-04-02

    CPC classification number: H01M10/0567 H01M10/052 H01M2300/0025 Y02E60/122

    Abstract: 본 발명은 리튬 프탈라토보레이트 화합물을 함유하는 전해액에 관한 것으로서, 더욱 상세하게는 리튬염의 음이온 성분으로 프탈라토보레이트 또는 이의 유도체로 구성되는 리튬염을 포함하는 전해액을 구성하여 이를 이차 전지에 사용하는 경우 이차 전지의 안정성 및 저온 특성을 향상시킬 수 있어서 전지의 수명 향상의 효과와 함께 저온에서 출력이 상승된 효과를 얻을 수 있는 리튬 프탈라토보레이트 화합물을 함유하는 전해액 및 이를 이용한 이차 전지에 관한 것이다.

    Abstract translation: 本发明涉及包含邻苯二甲酸钴化合物的电解质,更具体地说,涉及包含邻苯二甲酸钴硼酸化合物的电解质和使用该锂的二次电池,其中包含邻苯二甲酸钴硼酸化合物的电解质包括由邻苯二甲酸钴或其衍生物组成的锂盐 锂盐的阴离子成分,并且当用于二次电池时可以提高二次电池的稳定性和低温性能,从而获得提高电池寿命并增加低温输出的效果。

    고순도의 트리스트리메틸실릴보레이트 제조방법
    6.
    发明公开
    고순도의 트리스트리메틸실릴보레이트 제조방법 有权
    高纯度TRIS(三甲基硅烷)硼酸盐的制备方法

    公开(公告)号:KR1020100090152A

    公开(公告)日:2010-08-13

    申请号:KR1020090009471

    申请日:2009-02-05

    CPC classification number: C07F19/00 C01B35/1054 C07F7/10

    Abstract: PURPOSE: A method for preparing Tris(trimethylsilyl)borate is provided to perform the reaction under mild condition without additional process. CONSTITUTION: A method for preparing Tris(trimethylsilyl)borate comprises: a step of reacting boric acid, hexamethyldisilazane and quaternary ammonium salt at 90-150°C for 5-20 hours to obtain crude Tris(trimethylsilyl)borate; and a step of purifying crude Tris(trimethylsilyl)borate to obtain Tris(trimethylsilyl)borate. The quaternary ammonium salt is F-, Cl-. Br- or I-.

    Abstract translation: 目的:提供一种制备三(甲基甲硅烷基)硼酸盐的方法,在温和条件下进行反应,无需额外的工艺。 构成:制备三(甲基甲硅烷基)硼酸盐的方法包括:在90-150℃下使硼酸,六甲基二硅氮烷和季铵盐反应5-20小时,得到粗三(甲硅烷基)硼酸盐; 和纯化三(甲基甲硅烷基)硼酸三钠以获得三(三甲基甲硅烷基)硼酸盐的步骤。 季铵盐是F-,Cl-。 Br-或I-。

    고순도 트리스(트리알킬실릴)포스파이트의 제조 방법
    9.
    发明公开
    고순도 트리스(트리알킬실릴)포스파이트의 제조 방법 有权
    高纯度TRIS(TRIALKYLSILYL)磷酸盐的制造工艺

    公开(公告)号:KR1020120067398A

    公开(公告)日:2012-06-26

    申请号:KR1020100128770

    申请日:2010-12-16

    CPC classification number: C07F19/00 B01D3/14 B01J2219/0059

    Abstract: PURPOSE: A method for preparing tris(trialkylsilyl)phosphate without separate catalyst and solvent is provided to quickly synthesize the compounds without purification. CONSTITUTION: A method for preparing tris(trialkylsilyl)phosphite of chemical formula 1 comprises: a step of reacting hypophosphoric acid and hexaalkyldisilazane of chemical formula 2 without separate catalyst and solvent; and a step of continuously adding metallic sodium. The amount of the hexaalkydisilazane derivative of chemical formula 2 is 1-3 equivalent based o 1 equivalent of hypophosphoric acid.

    Abstract translation: 目的:提供无需单独催化剂和溶剂的三(三烷基甲硅烷基)磷酸酯的制备方法,可快速合成化合物而无需纯化。 构成:制备化学式1的三(三烷基甲硅烷基)亚磷酸酯的方法包括:使化学式2的次磷酸和六烷基二硅氮烷与单独的催化剂和溶剂反应的步骤; 和连续加入金属钠的步骤。 化学式2的六氢二硅氮烷衍生物的量为基于0当量的次磷酸1-3当量。

    고순도의 트리스트리메틸실릴포스페이트 제조방법
    10.
    发明公开
    고순도의 트리스트리메틸실릴포스페이트 제조방법 有权
    高纯度TRIS(三甲基硅烷)磷酸盐的制造工艺

    公开(公告)号:KR1020100090150A

    公开(公告)日:2010-08-13

    申请号:KR1020090009468

    申请日:2009-02-05

    CPC classification number: C07F19/00 B01D3/143

    Abstract: PURPOSE: A method for preparing Tris(trimethylsilyl)phosphate is provided to obtain Tris(trimethylsilyl) phosphate of high purity at low temperature without solvent. CONSTITUTION: A method for preparing Tris(trimethylsilyl)phosphate comprises: a step of reacting phosphoric acid, hexamethyldisilazaen, quaternary ammonium salt, phosphonium salt and mixture thereof at 100-160°C for 5-20 hours to obtain crude Tris(trimethylsilyl)phosphate; and a step of purifying the crude Tris(trimethylsilyl)phosphate.

    Abstract translation: 目的:提供一种制备三(三甲基甲硅烷基)磷酸酯的方法,以在低温下无溶剂获得高纯度的三(三甲基甲硅烷基)磷酸酯。 构成:制备三(三甲基甲硅烷基)磷酸酯的方法包括:在100-160℃下使磷酸六甲基二硅氮烷,季铵盐,鏻盐及其混合物反应5-20小时,得到粗的三(三甲基甲硅烷基)磷酸酯 ; 和纯化粗三(三甲基甲硅烷基)磷酸酯的步骤。