Abstract: In the present invention, provided is a soil material composition for ramming soil, comprising 100 parts by weight of soil including an amount of sand capable of making porosity while content and moisture content of silt are respectively not more than 10% and 5%; and 5-200 parts by weight of high strength lime and light-weight aggregate or 0.1-50 parts by weight of fiber materials, which has 5MPa or more compressive strength 28 days after aging. The soil material composition has an outstanding strength and workability, leading to construction efficiency in construction sites.
Abstract translation: 在本发明中,提供了一种用于夯实土壤的土壤材料组合物,其包含100重量份的土壤,包括一定量的能够产生孔隙率的砂,同时淤泥含量和含水量分别不大于10%和5%; 和5-200重量份的高强度石灰和轻质骨料或0.1-50重量份纤维材料,其老化后28天具有5MPa或更高的抗压强度。 土壤材料成分具有突出的实力和可操作性,导致施工现场施工效率高。
-
公开(公告)号:KR101049769B1
公开(公告)日:2011-07-19
申请号:KR1020100048856
申请日:2010-05-25
Applicant: 목포대학교산학협력단
Abstract: PURPOSE: A stomped earth wall and earth for the stomped earth wall are provided to enable original earth to be immediately applied to a construction process. CONSTITUTION: A form is assembled. Earth is collected. 10wt%~50wt% of lime complex and 50wt%~90wt% of earth are mixed. The water is mixed with raw materials. 60wt%~90wt% of raw material and 60wt%~90wt% of water are mixed. Earth for a stomped earth wall is filled in the form. The earth is stomped by pressure. The earth is cured for a given time.
Abstract translation: 目的:提供踩踏土墙的踩踏土墙和地球,以使原始地球立即施加施工过程。 构成:组合表格。 收集地球 10重量%〜50重量%的石灰复合物和50重量%〜90重量%的土壤混合。 水与原料混合。 60wt%〜90wt%的原料和60wt%〜90wt%的水混合。 地球填满了一块踩踏的土墙。 地球被压力踩踏。 地球被治好了一段时间。
-