公开(公告)号:KR1019900001098B1
公开(公告)日:1990-02-26
申请号:KR1019850008534
申请日:1985-11-14
Applicant: 삼성전자주식회사
Inventor: 안동훈
IPC: C22C38/22
Abstract: A carbon steel with high hardenability is characterized by being composed of about 0.8% C, 0.1-0.25% Mo, 0.4-0.6% Cr, 0.4-0.6% Si and inevitably added impurites. Si induces synergistic effect with Mo and Cr, so the carbon steel needs less alloying element but doesn't lose its own properties.
Abstract translation: 具有高淬透性的碳钢的特征在于由约0.8%的C,0.1-0.25%的Mo,0.4-0.6%的Cr,0.4-0.6%的Si和不可避免的添加的杂质组成。 Si引起Mo和Cr的协同效应,因此碳钢需要较少的合金元素,但不会失去其自身特性。
-
-
公开(公告)号:KR1019890003346B1
公开(公告)日:1989-09-18
申请号:KR1019840008430
申请日:1984-12-27
Applicant: 삼성전자주식회사
IPC: C22C21/06
Abstract: Cu 2.0-4.7, Mg 0.7-2.1, Ni 0.9-2.7, Si 0.3-0.9, Fe 0.1-0.6, Ti and/or B 0.001-0.04 and Al the balance and has a coefft. of expansion below 20.0X10-6/deg.C, hardness after heat treatment of above 145 Hv and uniformity of dispersion of ppts. smaller than 7.5 micro, above 95%. Alloy may also contain; Cr 0.1- 0.3. Alloy has good mechanical properties, cold forgeability, thermal expansion pption. properties and corrosion and abrasion resistance.
Abstract translation: Cu 2.0-4.7,Mg 0.7-2.1,Ni 0.9-2.7,Si 0.3-0.9,Fe 0.1-0.6,Ti和/或B 0.001-0.04,Al余量为Coe。 的膨胀低于20.0X10-6 /℃,热处理后的硬度高于145 Hv,ppts分散均匀。 小于7.5微米,高于95%。 合金还可能含有 Cr 0.1- 0.3。 合金具有良好的机械性能,冷锻性,热膨胀性。 性能和耐腐蚀和耐磨性。
-
4.
公开(公告)号:KR1020170013712A
公开(公告)日:2017-02-07
申请号:KR1020150106772
申请日:2015-07-28
Applicant: 삼성전자주식회사
CPC classification number: G10L15/063 , G06F17/2705 , G10L15/02 , G10L15/197 , G10L2015/025 , G10L2015/027 , G10L2015/0635
Abstract: 적어도하나의단어를포함하는코퍼스(corpus)를획득하고, 코퍼스로부터적어도하나의단어를획득하고, 획득된단어를적어도하나의세그먼트로분할하고, 분할된세그먼트를단어로재조합하기위한힌트를생성하고, 힌트를포함하는적어도하나의세그먼트를이용하여, 문법모델을갱신하는음성인식시 이용되는문법모델을갱신하는방법이개시된다.
Abstract translation: 一种更新在语音识别期间使用的语法模型的方法,包括获得包括至少一个单词的语料库,从语料库中获得至少一个单词,将至少一个获得的单词分解成至少一个分段,产生用于重新组合的提示 至少一个段到所述至少一个单词中,以及通过使用至少一个包括所述提示的段来更新所述语法模型。
-
-
公开(公告)号:KR1019880001083B1
公开(公告)日:1988-06-22
申请号:KR1019850004249
申请日:1985-06-15
Applicant: 삼성전자주식회사
Inventor: 안동훈
Abstract: A BaTiO3 ceramic semiconductor is obtained by adding to a basic compsn., mixed by the mol ratio (1:1) with BaCo3 and TiO2 having 98-99% purity, 4 mol% SnO2, 0.02-0.06 mol% Nb2O5, 0.0270.08 mol% Mn (NO3)2, 2.365-3.94 mol% SiO2 and 1-1.5 mol% TiO2. The ceramic semiconductor has specific resistance 70-300Ω.cm, increment ratio of resistance 5X1O5 and withstand voltage 250-300V. This material can be used as a degaussing element esp. a noncontact switch for high voltages.
Abstract translation: 通过添加碱性组分,通过与BaCo 3和纯度为98-99%的TiO 2,4mol%SnO 2,0.02-0.06mol%Nb 2 O 5,0.0270.08的摩尔比(1:1)混合来获得BaTiO 3陶瓷半导体 mol%Mn(NO 3)2,2.365-3.94mol%SiO 2和1-1.5mol%TiO 2。 陶瓷半导体具有电阻70-300Ω.cm,电阻增量比5X1O5,耐压250-300V。 这种材料可以用作消磁元件。 用于高电压的非接触式开关。
-
-
-
公开(公告)号:KR1019900001099B1
公开(公告)日:1990-02-26
申请号:KR1019850008096
申请日:1985-10-31
Applicant: 삼성전자주식회사
IPC: C22C38/30
Abstract: A making process of permanent magnet composed of 20-30 wt.% Cr, 12.5- 15.7 wt.% Co, 1-5 wt.% forming element (Ti, V, Al, Zr, Si, W etc) and bal. Fe is characterized by having 2-6 MGOe of (BH) max resulted from stress-aging at a stress 1 kgf/mm2-9.5 kgf/mm2 for 15-45 minutes at a temperature range from 600oC to 710oC.
Abstract translation: 永磁体的制造过程由20-30重量%的Cr,12.5-15.7重量%的Co,1-5重量%的成形元素(Ti,V,Al,Zr,Si,W等)和bal组成。 Fe的特征在于,在600℃至710℃的温度范围内,在应力为1kgf / mm 2 -9.5kgf / mm 2的情况下,由应力老化引起的(BH)max为2-6MOOe为15-45分钟。
-
-
-
-
-
-
-
-
-