公开(公告)号:KR1020080095981A
公开(公告)日:2008-10-30
申请号:KR1020070040714
申请日:2007-04-26
Applicant: 삼성코닝 주식회사
CPC classification number: H01J61/305 , G02F1/133604 , H01J61/10
Abstract: A surface light source device and a backlight unit having the same are provided to improve the uniformity of contrast even though the surface light source device is made of plural surface light source modules. A surface light source device comprises a light source body(110) containing a discharge space(140) into which the discharge gas is injected; a plurality of surface light source modules having an electrode(150) which applies a discharge voltage to the discharge gas; a light guide member guiding the light, which is emitted from the plural surface light source modules to downwards, to the border area between the surface light source modules. The light guide member is mounted at the bottom side of surface light source modules.
Abstract translation: 提供一种表面光源装置和具有该表面光源装置的背光单元以提高对比度的均匀性,即使表面光源装置由多个表面光源模块制成。 面光源装置包括:容纳放电空间的放电空间的光源体, 多个表面光源模块,具有向放电气体施加放电电压的电极; 导光构件,其将从多个面光源模块发射的光向下引导到表面光源模块之间的边界区域。 导光构件安装在表面光源模块的底侧。
-
公开(公告)号:KR1020000019512A
公开(公告)日:2000-04-15
申请号:KR1019980037636
申请日:1998-09-11
Applicant: 삼성코닝 주식회사
Abstract: PURPOSE: Is provided a water repellent glass coated with an agitated silica solution without a haze or a rainbow phenomenon. The solution thereof is obtained by mixing silica solution into the solution of acetic acid and alcohol as an essential step. CONSTITUTION: The fabrication method of a water repellent glass contains; obtaining an agitated silica solution by mixing 10-90 wt% of silica solution which has a hydrolysis of tetraethoxysilane(Si2(C2H5O)4) via ammonia water of pH 9-13 at 30°C for 24hrs., followed by acidifying of pH 1-3 with hydrochloride and agitating at 5°C for 1hr. with a mixed solution of 10-90 wt% acetic acid and alcohol; coating a cleaned glass with the solution thereof by a spray method; heat treatment in at 300°C for 30 min. after drying.
Abstract translation: 目的:提供涂有搅拌的二氧化硅溶液的防水玻璃,没有雾度或彩虹现象。 其溶液是通过将二氧化硅溶液作为必需步骤将乙酸和醇的溶液混合而获得的。 构成:防水玻璃的制造方法包括: 通过将10-90重量%的具有四乙氧基硅烷(Si 2(C 2 H 5 O)4水解)的二氧化硅溶液通过pH 9-13的氨水在30℃下混合24小时获得搅拌的二氧化硅溶液,然后酸化pH 1 -3与盐酸盐混合,并在5℃下搅拌1小时。 与10-90重量%乙酸和醇的混合溶液; 用喷雾法用其溶液涂覆清洁过的玻璃; 在300℃下热处理30分钟。 干燥后。
-
公开(公告)号:KR1019980066464A
公开(公告)日:1998-10-15
申请号:KR1019970002042
申请日:1997-01-24
Applicant: 삼성코닝 주식회사
IPC: C03C3/112
Abstract: 유리 기재의 어느 한 면에 금속알콕시드 화합물과 무기염을 포함하는 혼합 용액을 도포하여 제1층을 형성하고, 상기 제1층의 위에 플루오로알킬실란 화합물을 포함하는 혼합 용액을 도포하여 제2층을 형성하여 제조되는 내구성을 가지는 발수 유리의 제조 방법은 금속산화물층 형성을 위한 용액의 제조 방법이 간단하고, 그 열처리 온도가 일반 소다라임 유리의 연화점 혹은 기존의 방법보다 낮아서 제조 비용이 저렴한 동시에 유리 기재의 변형을 예방할 수 있으며, 고가의 장비를 사용한다거나 공정상의 번거로움이 없으며, 이러한 제조 방법에 의하여 제조된 발수 유리는 막강도가 높고, 우수한 내구성을 가진다.
-
公开(公告)号:KR100519109B1
公开(公告)日:2005-11-30
申请号:KR1019980013562
申请日:1998-04-16
Applicant: 삼성코닝 주식회사
IPC: B60J1/00
Abstract: 본 발명은 다기능성 자동차 유리에 관한 것으로서, 더욱 상세하게는 자동차유리 내면에는 결정형 TiO
2 입자가 고르게 분산된 광촉매성 코팅막이 형성되어 있어서 표면에 수막이 형성되도록하여 자동차 안팎의 기온차에도 김이 서리지 않도록 친수기능을 부여하고, 또한 유리 외면에는 실리카막과 표면에너지가 낮은 발수막이 2중으로 도포되어 있어서 우천시 물방울이 표면에 젖지 않고 구형으로 흘러내리게하여 물방울이 유리표면을 적시지 않아 우천시에도 시야의 왜곡됨 없이 안전한 시계확보가 가능하도록 발수기능을 부여한 다기능성 자동차 유리에 관한 것이다.-
公开(公告)号:KR100433203B1
公开(公告)日:2004-07-16
申请号:KR1019970034648
申请日:1997-07-24
Applicant: 삼성코닝 주식회사
IPC: C03C27/00
Abstract: PURPOSE: A process for producing water-repellent glass is provided, which can improve water-repellency and abrasion resistance by forming a silica layer having surface roughness on a glass substrate under a special coating condition. CONSTITUTION: The water-repellent glass is produced by forming the silica layer on the surface of the glass substrate(2) and then forming a water-repellent layer on the silica layer. The silica layer having surface roughness is formed by spraying specially prepared silica sol solution on the glass substrate(2) by a spray coating method, wherein a pressure(applied to a solution tank(3)) of the silica coating solution is 0.4-1.0kgf/cm2, an air pressure passed through an air transfer line(13) is 0.5-2.5kgf/cm2, and the distance between the glass substrate(2) and a spray nozzle is 5-20cm. The spray nozzle attached to the spray gun(11) moves at a velocity of 10-40cm/sec.
-
公开(公告)号:KR1020000013595A
公开(公告)日:2000-03-06
申请号:KR1019980032548
申请日:1998-08-11
Applicant: 삼성코닝 주식회사
IPC: C09D5/16
CPC classification number: C09D5/1618 , C03C17/00 , C09D1/00
Abstract: PURPOSE: A stain-proofing coating composition is provided to have a good coating property for glass, resin, ceramic and metal materials and hence large thickness of the coating, which causes no degradation of the coating product under heat treatment at a high temperature and effectively prevents a stain on the surface of a substrate. CONSTITUTION: The coating composition comprises boron and sodium carbonate at a molar ratio of 1:0.01 to 1:2, the total content of the boron and sodium carbonate being 1 to 10 wt.% based on the total weight of the aqueous solution. The glass product contains a coating comprising the stain-proofing coating composition. The coating has a thickness of 500 to 2,000 angstroms.
Abstract translation: 目的:提供防污涂料组合物,以对玻璃,树脂,陶瓷和金属材料具有良好的涂层性能,因此涂层厚度大,不会在高温下有效地在热处理下降解涂层产品 防止基板表面上的污渍。 构成:涂料组合物包含摩尔比为1:0.01至1:2的硼和碳酸钠,基于水溶液的总重量,硼和碳酸钠的总含量为1-10重量%。 玻璃制品含有包含防污涂料组合物的涂层。 该涂层的厚度为500至2000埃。
-
公开(公告)号:KR100396371B1
公开(公告)日:2003-11-20
申请号:KR1019960047649
申请日:1996-10-23
Applicant: 삼성코닝 주식회사
Inventor: 홍병선 , 이혜용 , 조윤주 , 한주헌 , 발사미안구에오르구이
IPC: B05D7/04
Abstract: PURPOSE: A process for modifying surface of a substrate is provided to economically and stably modify the surface by contacting the surface with XeF2 (xenon difluoride) then graft-bonding single molecules by contacting the surface with polymerable fluoro monomer in vapor status. CONSTITUTION: The process comprises steps of reacting the surface with gaseous xenon difluoride at 0 to 50 deg.C for 1 minute to 20 hours; reacting polymerable monomer in a gas status on the surface under a pressure of 50 to 150 torr and at 20 to 200 deg.C for 10 seconds to 72 hours; and reacting the gaseous xenon difluoride on the surface. The polymerable monomer is selected from a group consisting of tetrafluoroethylene and hexafluoropropene(HTP). The substrate is selected from any one consisting of glass, plastic, rubber ceramic and metal.
-
公开(公告)号:KR1020030074211A
公开(公告)日:2003-09-19
申请号:KR1020030013600
申请日:2003-03-05
Applicant: 삼성코닝 주식회사
IPC: C03C17/28
CPC classification number: C03C17/28
Abstract: PURPOSE: Provided is a water soluble coating composition comprising salts, surfactant, sugar alcohol which has pollution prevention, good coating for glass, ceramic and metal materials and easy cleaning. CONSTITUTION: The coating composition comprises the components of: 0.01-1wt.% of water soluble salt such as carbonate, nitrate, sulfate, phosphate, silicate, etc., and preferably Na2B4O7; 0.0001-1wt.% of anionic or non-ionic surfactant such as sodium alkyl sulfonate, sodium polyacrylic acid, polyethylene glycol, etc.; 0.01-5wt.% of sugar alcohols such as sorbitol, xylitol and mannitol; and aqueous medium. The coating film is formed on the substrate in a thickness of 600-5000angstrom by conventional methods such as dip coating, spray coating, and flow coating.
Abstract translation: 目的:提供一种含有盐,表面活性剂,糖醇的水溶性涂料组合物,其具有防污染,对玻璃,陶瓷和金属材料的良好涂层和易于清洁。 构成:涂料组合物包含:0.01-1重量%的水溶性盐如碳酸盐,硝酸盐,硫酸盐,磷酸盐,硅酸盐等,优选为Na 2 B 4 O 7; 0.0001-1重量%的阴离子或非离子表面活性剂如烷基磺酸钠,聚丙烯酸钠,聚乙二醇等; 0.01-5重量%的糖醇如山梨糖醇,木糖醇和甘露糖醇; 和水介质。 通过常规方法如浸涂,喷涂和流涂,在基底上形成厚度为600-5000的涂膜。
-
公开(公告)号:KR100281993B1
公开(公告)日:2001-04-02
申请号:KR1019970027532
申请日:1997-06-26
Applicant: 삼성코닝 주식회사
IPC: C03C3/04
Abstract: 본 발명은 내구성이 우수한 발수유리와 그 제조방법에 관한 것으로서, 더욱 상세하게는 자동차 안전유리, 건물용 유리, 거울등과 같은 다양한 유리의 기판재료 위에 먼저 내구성 부여를 위해 염기성 및 산성 촉매하에서 숙성된 실리카용액을 코팅하여 미세결정의 실리카 입자를 갖고 표면거칠기가 만들어진 실리카 하지층을 형성하고 그 위에 플루오로알킬실란(FAS)을 도포하여 발수층을 형성하므로써, 발수성과 동시에 내구성을 부여하여 오랫동안 사용하더라고 외관상의 변형은 물론 성능상의 저하가 없도록 개선된 내구성 발수유리와 그를 제조하는 방법에 관한 것이다.
-
公开(公告)号:KR100216869B1
公开(公告)日:1999-09-01
申请号:KR1019970002042
申请日:1997-01-24
Applicant: 삼성코닝 주식회사
IPC: C03C3/112
CPC classification number: C03C2217/45 , C03C2217/478
Abstract: 유리 기재의 어느 한 면에 금속알콕시드 화합물과 무기염을 포함하는 혼합 용액을 도포하여 제1층을 형성하고, 상기 제1층의 위에 플루오로알킬실란 화합물을 포함하는 혼합 용액을 도포하여 제2층을 형성하여 제조되는 내구성을 가지는 발수 유리의 제조 방법은 금속산화물층 형성을 위한 용액의 제조 방법이 간단하고, 그 열처리 온도가 일반 소다라임 유리의 연화점 혹은 기존의 방법보다 낮아서 제조 비용이 저렴한 동시에 유리 기재의 변형을 예방할 수 있으며, 고가의 장비를 사용한다거나 공정상의 번거로움이 없으며, 이러한 제조 방법에 의하여 제조된 발수 유리는 막강도가 높고, 우수한 내구성을 가진다.
-
-
-
-
-
-
-
-
-