公开(公告)号:KR100958551B1
公开(公告)日:2010-05-18
申请号:KR1020090068079
申请日:2009-07-24
Applicant: 서울대학교산학협력단
CPC classification number: C08J3/205 , C08J2323/10 , C08K3/346 , C08K2201/011 , C08L23/10 , Y10S977/783
Abstract: PURPOSE: A soundproofing material and a manufacturing method thereof are provided to use a PP resin for improving the soundproof property of the material, and to prevent the productivity degradation. CONSTITUTION: A manufacturing method of a soundproofing material comprises the following steps: forming a mixture by dissolving a PP resin and nanoclay into a solvent; and evaporating the solvent from the mixture. The formation process for the mixture is performed by mixing 2~10wt% of nanoclay for the total amount of the mixture. The mass ratio of the PP resin and the solvent is 1:3~1:5. The content rate of the solvent is under 0.5~2wt%.
Abstract translation: 目的:提供隔音材料及其制造方法,以使用PP树脂来改善材料的隔音性能,并且防止生产率降低。 构成:隔音材料的制造方法包括以下步骤:通过将PP树脂和纳米粘土溶解在溶剂中形成混合物; 并从混合物中蒸发溶剂。 混合物的形成过程是通过混合2〜10重量%的纳米粘土混合物的总量来进行的。 PP树脂和溶剂的质量比为1:3〜1:5。 溶剂含量为0.5〜2wt%。