메조 기공 구조의 복합분말 제조 방법 및 이를 이용한 고체산화물 연료전지 제조 방법
    1.
    发明公开
    메조 기공 구조의 복합분말 제조 방법 및 이를 이용한 고체산화물 연료전지 제조 방법 审中-实审
    使用相同方法制备多孔复合粉末和固体氧化物燃料电池

    公开(公告)号:KR1020130134799A

    公开(公告)日:2013-12-10

    申请号:KR1020120058579

    申请日:2012-05-31

    CPC classification number: Y02P70/56 H01M8/12 B01J19/00 H01M8/02

    Abstract: Provided is a manufacturing method of composite powder enabling to manufacture an electrode for a solid oxide fuel cell in a mesoporous structure with a low temperature sintering. The manufacturing method of composite powder according to the present invention comprises that a surfactant ethanol solution in which Pluronic^R F127 surfactant is added to ethanol is formed, and that a sol solution is formed by mixing a metallic salt of nickel, a metallic salt of gadolinium and a metallic salt of cerium in the surfactant ethanol solution. The sol solution is synthesized to a gel state by using the hydrothermal synthesis at 100°C or less, and dried powder is obtained by drying the synthesized gel state solution. Then, calcinated powder is obtained by calcinating the dried powder. [Reference numerals] (AA) Add F127 surfactant in aqueous hydrochloric acid and ethanol;(BB) Material mixing (Cerium nitrate hexahydrate + Gadolinium nitrate hexahydrate +Nickel nitrate hexahydrate);(CC) Stiring;(DD) Gelation (Stirring at 80°C for 1 hour);(EE) Hydrothermal synthesis (80°C for 7 days);(S1) Mixing;(S2) Synthesis;(S3) Dry - Heating at 70°C in air;(S4) Calcination - 450-650°C for 2 hours at the atmosphere of air in furnace

    Abstract translation: 提供一种复合粉末的制造方法,其能够制造具有低温烧结的介孔结构中的固体氧化物型燃料电池用电极。 根据本发明的复合粉末的制造方法包括:将形成PluronicRF127表面活性剂的表面活性剂乙醇溶液加入到乙醇中,并且溶胶溶液通过将镍的金属盐, 钆和铈的金属盐在表面活性剂乙醇溶液中。 通过使用100℃以下的水热合成将溶胶溶液合成为凝胶状,通过干燥合成的凝胶状溶液得到干燥粉末。 然后,通过煅烧干燥的粉末获得煅烧粉末。 (AA)添加F127表面活性剂在盐酸水溶液和乙醇中;(BB)混合物(硝酸铈六水合物+硝酸钆六水合物+硝酸镍六水合物);(CC)烧结;(DD)凝胶(80℃搅拌 C)1小时);(EE)水热合成(80℃7天);(S1)混合;(S2)合成;(S3)在70℃干燥空气中加热;(S4)煅烧 - 650℃,炉中空气气氛2小时

Patent Agency Ranking