LbL 멀티레이어링 기술을 이용한 소수화된 펄프섬유의 제조 방법 및 이를 이용하여 제조된 종이
    1.
    发明公开
    LbL 멀티레이어링 기술을 이용한 소수화된 펄프섬유의 제조 방법 및 이를 이용하여 제조된 종이 有权
    通过LBL多层法制造疏水性纸浆纤维的方法及其使用

    公开(公告)号:KR1020110134744A

    公开(公告)日:2011-12-15

    申请号:KR1020100054493

    申请日:2010-06-09

    CPC classification number: D21H23/10 D21H17/33 D21H21/14 D21H27/30

    Abstract: PURPOSE: A method for fabricating hydrophobic pulp fiber using LbL multilayering is provided to enhance tensile strength. CONSTITUTION: A method for fabricating hydrophobic pulp fiber by LbL multilayering comprises: a step of diluting pulp fiber with distilled water in a reaction tank(S110); a step of adjusting pH concentration of the reaction tank by 8-12; a step of adding PAH(poly allyamine hydrochloride) to the reaction tank(S130); a step of adsorbing the PAH on the surface of the pulp fiber by static-electricity; a step of discharging the unattached PAH and adding distilled water to wash the pulp fiber(S140); a step of controlling pH concentration of the reaction tank by 6-8(S160); a step of adding saponified rosin and adsorbing the soponified rosin on the surface of the PAH by static-electricity; and a step of reinputting distilled water to the reaction tank and washing.

    Abstract translation: 目的:提供使用LbL多层制造疏水性纸浆纤维的方法,以提高拉伸强度。 构成:通过LbL多层制造疏水性纸浆纤维的方法包括:在反应槽中用蒸馏水稀释纸浆纤维的步骤(S110); 将反应釜的pH浓度调节8-12的步骤; 将PAH(盐酸聚烯丙胺)加入到反应槽中的步骤(S130); 通过静电将PAH吸附在纸浆纤维的表面上的步骤; 排出未附着的PAH并加入蒸馏水以洗涤纸浆纤维的步骤(S140); 将反应罐的pH浓度控制在6-8的步骤(S160); 加入皂化松香并通过静电吸附分散的松香在PAH表面上的步骤; 以及将蒸馏水重新输送到反应罐并洗涤的步骤。

    고분자 물질이 다중 흡착된 종이의 제조 방법 및 이를 이용하여 제조된 종이
    2.
    发明授权
    고분자 물질이 다중 흡착된 종이의 제조 방법 및 이를 이용하여 제조된 종이 有权
    通过聚合物多层制造纸张的方法和使用它的纸张

    公开(公告)号:KR101157351B1

    公开(公告)日:2012-06-15

    申请号:KR1020100054492

    申请日:2010-06-09

    Abstract: PURPOSE: A method for manufacturing polymeric material-adsorbed paper is provided to enhance tensile strength and internal tearing strength. CONSTITUTION: A method for manufacturing polymeric material-adsorbed paper comprises: a step of diluting pulp fiber with distilled water in a reaction tank(S110); a step of controlling pH concentration and adding cationic starch to the reaction tank(S130); a step of static-electrically adsorbing the cationic starch on the surface of the pulp fiber; a step of discharging the unadsorbed cationic starch; a step of washing the pulp fiber by reinputting distilled water to the reaction tank(S140); a step of controlling pH concentration by 6-8; a step of adding PSS(poly-sodium 4-styrene sulfonate)(S160); a step of static-electrically adsorbing PSS on the surface of the cationic starch; and a step of discharging undsorbed PSS(S170).

    LbL 멀티레이어링 기술을 이용한 소수화된 펄프섬유의 제조 방법 및 이를 이용하여 제조된 종이
    3.
    发明授权
    LbL 멀티레이어링 기술을 이용한 소수화된 펄프섬유의 제조 방법 및 이를 이용하여 제조된 종이 有权
    通过LbL多层制造疏水性纸浆纤维的方法及其使用的纸张

    公开(公告)号:KR101157387B1

    公开(公告)日:2012-06-20

    申请号:KR1020100054493

    申请日:2010-06-09

    Abstract: PURPOSE: A method for fabricating hydrophobic pulp fiber using LbL multilayering is provided to enhance tensile strength. CONSTITUTION: A method for fabricating hydrophobic pulp fiber by LbL multilayering comprises: a step of diluting pulp fiber with distilled water in a reaction tank(S110); a step of adjusting pH concentration of the reaction tank by 8-12; a step of adding PAH(poly allyamine hydrochloride) to the reaction tank(S130); a step of adsorbing the PAH on the surface of the pulp fiber by static-electricity; a step of discharging the unattached PAH and adding distilled water to wash the pulp fiber(S140); a step of controlling pH concentration of the reaction tank by 6-8(S160); a step of adding saponified rosin and adsorbing the soponified rosin on the surface of the PAH by static-electricity; and a step of reinputting distilled water to the reaction tank and washing.

    고분자 물질이 다중 흡착된 종이의 제조 방법 및 이를 이용하여 제조된 종이
    4.
    发明公开
    고분자 물질이 다중 흡착된 종이의 제조 방법 및 이를 이용하여 제조된 종이 有权
    通过聚合物多层纸制造纸张的方法及其使用

    公开(公告)号:KR1020110134743A

    公开(公告)日:2011-12-15

    申请号:KR1020100054492

    申请日:2010-06-09

    CPC classification number: D21H23/10 D21H17/29 D21H17/33 D21H21/14

    Abstract: PURPOSE: A method for manufacturing polymeric material-adsorbed paper is provided to enhance tensile strength and internal tearing strength. CONSTITUTION: A method for manufacturing polymeric material-adsorbed paper comprises: a step of diluting pulp fiber with distilled water in a reaction tank(S110); a step of controlling pH concentration and adding cationic starch to the reaction tank(S130); a step of static-electrically adsorbing the cationic starch on the surface of the pulp fiber; a step of discharging the unadsorbed cationic starch; a step of washing the pulp fiber by reinputting distilled water to the reaction tank(S140); a step of controlling pH concentration by 6-8; a step of adding PSS(poly-sodium 4-styrene sulfonate)(S160); a step of static-electrically adsorbing PSS on the surface of the cationic starch; and a step of discharging undsorbed PSS(S170).

    Abstract translation: 目的:提供吸收聚合物材料的方法,以提高拉伸强度和内部撕裂强度。 构成:用于制造聚合物吸附纸的方法包括:在反应罐中用蒸馏水稀释纸浆纤维的步骤(S110); 控制pH浓度并向反应槽中加入阳离子淀粉的步骤(S130); 在纸浆纤维的表面上静电吸附阳离子淀粉的步骤; 排出未吸附的阳离子淀粉的步骤; 通过将蒸馏水重新输送到反应罐中来清洗纸浆纤维的步骤(S140); 控制pH浓度6-8的步骤; 加入PSS(聚4-苯乙烯磺酸钠)(S160)的步骤; 在阳离子淀粉表面静电吸附PSS的步骤; 以及排出未吸附的PSS的步骤(S170)。