公开(公告)号:KR1020140032756A
公开(公告)日:2014-03-17
申请号:KR1020120099429
申请日:2012-09-07
Applicant: 서울대학교산학협력단
CPC classification number: H01F7/00 , A61K9/0009 , A61K9/5094 , B82Y25/00 , H01F1/0045 , H01F1/0054 , A61K9/16 , A61K9/14 , A61K47/50 , A61K49/08
Abstract: The present invention provides a selective activation method of a magnetic nanoparticle having a magnetic vortex structure. The selective activation method of the magnetic nanoparticle by an embodiment of the present invention comprises the following steps: a step of providing the magnetic nanoparticle with the magnetic vortex structure; a step of applying a first magnetic field to the magnetic nanoparticle for the magnetic nanoparticle to have resonant frequency; and a step of applying a second magnetic field to the magnetic nanoparticle with the resonant frequency for activating the magnetic nanoparticle. [Reference numerals] (S110) Providing a magnetic nanoparticle with magnetic vortex structure; (S120) Applying a first magnetic field to the magnetic nanoparticle for the magnetic nanoparticle to have resonant frequency; (S130) Activating the magnetic nanoparticle by applying a second magnetic field to the magnetic nanoparticle with the resonant frequency
Abstract translation: 本发明提供具有磁涡旋结构的磁性纳米颗粒的选择性活化方法。 本发明实施方案的磁性纳米颗粒的选择性活化方法包括以下步骤:向磁性纳米颗粒提供磁涡旋结构的步骤; 向所述磁性纳米颗粒施加第一磁场以使所述磁性纳米颗粒具有共振频率的步骤; 以及使用具有用于激活磁性纳米颗粒的共振频率的磁性纳米颗粒施加第二磁场的步骤。 (S110)提供具有磁涡旋结构的磁性纳米粒子; (S120)将磁性纳米颗粒的第一磁场施加到磁性纳米颗粒以具有共振频率; (S130)通过以具有共振频率的磁性纳米颗粒施加第二磁场来激活磁性纳米颗粒
-
公开(公告)号:KR101409296B1
公开(公告)日:2014-06-24
申请号:KR1020120099429
申请日:2012-09-07
Applicant: 서울대학교산학협력단
CPC classification number: H01F7/00 , A61K9/0009 , A61K9/5094 , B82Y25/00 , H01F1/0045 , H01F1/0054
Abstract: 본 발명은, 자기 소용돌이 구조를 가지는 자성 나노 입자의 선택적 활성화 방법을 제공한다. 본 발명의 일실시예에 따른 자성 나노 입자의 선택적 활성화 방법은, 자기 소용돌이 구조를 가지는 자성 나노 입자를 제공하는 단계; 자성 나노 입자가 공진 주파수를 가지도록, 제1 자기장을 자성 나노 입자에 인가하는 단계; 및 공진 주파수를 가지는 제2 자기장을 자성 나노 입자에 인가하여, 자성 나노 입자를 활성화시키는 단계;를 포함한다.
-