公开(公告)号:KR101267224B1
公开(公告)日:2013-05-24
申请号:KR1020100139389
申请日:2010-12-30
Applicant: 성균관대학교산학협력단
Abstract: 본발명은셀룰로오즈및 계면활성제를함유하는혼합물을기둥형태의상단및 하단으로구성되고, 상기상기상단및 하단의중량비가 3 : 1 내지 8 : 1인분쇄기로분쇄하는단계를포함하는셀룰로오즈입자의제조방법에관한것으로, 본발명에의해제조된셀룰로오즈입자는나노사이즈를가지고, 열가소성수지와혼련이가능하여건축자재등의특성을향상시키기위한소재로사용될수 있다.
-
公开(公告)号:KR101211948B1
公开(公告)日:2012-12-13
申请号:KR1020100041012
申请日:2010-04-30
Applicant: 성균관대학교산학협력단
IPC: C07G1/00 , C09D197/00 , C08J5/18
Abstract: 본발명은목질계원료로부터저분자리그닌을제조하는방법에관한것이다. 본발명에서는종래와달리, 목질계원료로부터고분자리그닌을제조하는것이아니라, 중량평균분자량이 100 내지 500인저분자리그닌을효율적으로제조할수 있으며, 상기제조된저분자리그닌을함유하는코팅제를제조함으로써, 항균성및 코팅성이우수한코팅필름을제공할수 있다.
-
公开(公告)号:KR1020120077438A
公开(公告)日:2012-07-10
申请号:KR1020100139389
申请日:2010-12-30
Applicant: 성균관대학교산학협력단
Abstract: PURPOSE: A manufacturing method of cellulose particle is provided to provide cellulose particle having nano size, to mull with a thermoplastic resin, to provide cellulose particles, and to recycle wood raw material. CONSTITUTION: A manufacturing method of cellulose particle comprises a step of pulverizing a mixture containing cellulose and surfactant by a pulverizer which consists of an upper part and a lower part of pillar shape, and has the weight ration of the upper part and the lower part of 3:1-8:1. The cellulose is manufactured by purifying wood based raw material. The surfactant is one or more alkoxysilane selected from a group consisting of tetramethoxysilane, tetraethoxysilane, tetrapropoxysilane, and tetrabutoxysilane.
Abstract translation: 目的:提供纤维素颗粒的制造方法,以提供具有纳米尺寸的纤维素颗粒,与热塑性树脂一起研磨以提供纤维素颗粒,以及回收木材原料。 构成:纤维素颗粒的制造方法包括通过由柱状上部和下部构成的粉碎机粉碎含有纤维素和表面活性剂的混合物的步骤,并且具有上部和下部的重量比 3:1-8:1。 纤维素通过纯化木材原料制造。 表面活性剂是一种或多种选自四甲氧基硅烷,四乙氧基硅烷,四丙氧基硅烷和四丁氧基硅烷的烷氧基硅烷。
-
公开(公告)号:KR1020110121423A
公开(公告)日:2011-11-07
申请号:KR1020100041012
申请日:2010-04-30
Applicant: 성균관대학교산학협력단
IPC: C07G1/00 , C09D197/00 , C08J5/18
CPC classification number: C07G1/00 , C08J5/18 , C09D197/005
Abstract: PURPOSE: A producing method of low molecular weight lignin using a wood composite raw material is provided to prevent the environmental contamination, and to produce a coating film having antibacterial property. CONSTITUTION: A producing method of low molecular weight lignin using a wood composite raw material comprises the following steps: refining high molecule weight lignin from the wood composite raw material; decomposing the high molecule weight lignin to obtain the low molecular weight lignin; and extracting the obtained low molecular weight lignin. The average molecular weight of the high molecule weight lignin is greater than 5,000. The average molecular weight of the low molecule weight lignin is 100-500.
Abstract translation: 目的:提供使用木材复合原料的低分子量木质素的制造方法,以防止环境污染,并制造具有抗菌性的涂膜。 构成:使用木材复合原料制备低分子量木质素的方法包括以下步骤:从木材复合原料中精制高分子量木质素; 分解高分子量木质素得到低分子量木质素; 并提取所得到的低分子量木质素。 高分子量木质素的平均分子量大于5,000。 低分子量木质素的平均分子量为100-500。
-
-
-