公开(公告)号:KR1020100129430A
公开(公告)日:2010-12-09
申请号:KR1020090047991
申请日:2009-06-01
Applicant: 아주대학교산학협력단
IPC: B21D26/02
Abstract: PURPOSE: A method for manufacturing a magnesium frame using hydroforming, capable of hydro formation of magnesium or magnesium alloy, is provided to improve the elongation ratio and moldability of magnesium material by keeping the temperature of pressurized fluids between 230~300°C. CONSTITUTION: A method for manufacturing a magnesium frame using hydroforming comprises next steps. Magnesium or magnesium alloy tube is loaded on a mold(S100). Pressure fluid is injected into the magnesium or magnesium alloy tube(S120). Pressure is added to the fluid of the magnesium or magnesium alloy tube(S140). A material tube in which molding is completed is taken out from the mold(S160).
Abstract translation: 目的:提供一种能够加氢形成镁或镁合金的使用液压成形的镁框架的制造方法,以通过将加压流体的温度保持在230〜300℃之间来提高镁材料的伸长率和成形性。 构成:使用液压成型制造镁框架的方法包括以下步骤。 将镁或镁合金管装载在模具上(S100)。 将压力流体注入到镁或镁合金管中(S120)。 向镁或镁合金管的流体中加入压力(S140)。 从模具中取出完成成型的材料管(S160)。
-
公开(公告)号:KR101094460B1
公开(公告)日:2011-12-15
申请号:KR1020090047991
申请日:2009-06-01
Applicant: 아주대학교산학협력단
IPC: B21D26/02
Abstract: 본 발명은 하이드로 포밍을 이용한 마그네슘 프레임의 제조 방법에 관한 것으로서, 마그네슘 또는 마그네슘 합금 소재 튜브를 금형에 로딩하는 단계; 마그네슘 또는 마그네슘 합금 소재 튜브의 내부에 압력 유체를 주입하는 단계; 및 마그네슘 또는 마그네슘 합금 소재 튜브 내부의 유체에 압력을 가하여 금형에 맞게 성형하여 성형이 완료된 소재 튜브를 취출하는 단계를 포함하는 것을 특징으로 한다.
본 발명에 의하면, 고온의 가압 유체가 열전달 작용에 의하여 150℃ ~ 600℃, 바람직하게는 180℃ ~ 400℃, 더욱 바람직하게는 230℃ ~ 300℃의 특성을 지니게 됨으로서, 상기 온도에 근접한 마그네슘 소재는 연신율이 증가하여 높은 성형성을 얻게 되어 소성 가공이 가능해진다.
-