콘크리트 노면의 재포장방법
    1.
    发明公开
    콘크리트 노면의 재포장방법 有权
    混凝土再填充方法

    公开(公告)号:KR1020100013817A

    公开(公告)日:2010-02-10

    申请号:KR1020080075517

    申请日:2008-08-01

    CPC classification number: E01C7/142 E01C19/025 E01C19/12

    Abstract: PURPOSE: A concrete pavement re-surfacing method is provided to reduce the repair time for a large area of pavement and to improve the uniformity and quality of concrete placed on the pavement by mixing the concrete components at the accurate ratio. CONSTITUTION: A concrete pavement re-surfacing method is as follows. Coarse aggregate, fine aggregate, fly ash based cement, and water are mixed with a twin shaft scheme to form semi-processed concrete(15)(S10). The semi-processed concrete is transported to a work site(S20). An activator causing hydration is put in the carried semi-processed concrete and mixed again to obtain concrete(35)(S30). The concrete is poured on the pavement being repaired to a fixed thickness(S40).

    Abstract translation: 目的:提供混凝土路面重铺方法,减少大面积路面的修复时间,并通过混合混凝土构件以准确的比例提高铺设在路面上的混凝土的均匀性和质量。 构成:混凝土路面重铺方法如下。 将粗骨料,细骨料,飞灰基水泥和水与双轴方案混合以形成半加工混凝土(15)(S10)。 半加工混凝土被运送到工地(S20)。 引起水化的活化剂放入运载的半加工混凝土中,再混合得到混凝土(35)(S30)。 将混凝土浇注在修复的固定厚度的路面上(S40)。

    콘크리트 노면의 재포장방법
    2.
    发明授权
    콘크리트 노면의 재포장방법 有权
    混凝土路面重铺方法

    公开(公告)号:KR101035405B1

    公开(公告)日:2011-05-20

    申请号:KR1020080075517

    申请日:2008-08-01

    Abstract: 본 발명은 콘크리트 노면의 재포장방법에 관한 것으로서, 그 주요 구성은 조골재, 세골재, 플라이애시계 시멘트, 물을 트윈 샤프트(twin shaft) 방식으로 혼합하여 콘크리트 반제품을 만드는 1차 비빔단계; 상기 1차 비빔단계에서 만든 콘크리트 반제품을 작업현장까지 운반하는 운반단계; 상기 운반단계에서 작업현장으로 운반되어 온 콘크리트 반제품에 수화작용을 일으키는 활성화제를 투입하고 재혼합하여 콘크리트를 만드는 2차 비빔단계; 및 상기 2차 비빔단계에서 만든 콘크리트를 보수할 노면 위에 부어 일정한 두께의 포장면을 형성하는 포설단계;로 이루어져 있는 것을 특징으로 하며, 위와 같은 구성에 따르면, 활성화제가 제거된 플라이애시계 시멘트에 의해 콘크리트 반제품을 만들기 때문에 1차 비빔을 원격지의 콘크리트 배치설비에 의해 할 수 있으므로, 콘크리트 구성물의 혼합비를 중량에 의해 정확하게 유지할 수 있어 콘크리트 반제품은 물론 노면에 타설되는 콘크리트의 물성 즉, 품질을 균일하게 유지할 수 있게 된다.
    콘크리트, 노면, 보수, 재포장, 초속경, 저슬럼프, 활성화제