Abstract:
A striking typed dissociating apparatus for dry fiber and a dissociating method using the same are provided to improve properties of the fiber by increasing a bulk value, yield, average fiber length, and tensile strength. A striking typed dissociating apparatus for dry fiber includes the followings: a plane wing portion of a flat pattern type; a blow blade(160) having a slant wing portion(164) installed on an end side of the plane wing portion; dissociation room(180) in which an upper end is opened while accommodating the blow blade; a motor providing rotation power for the blow blade; a driving pulley connected in the motor; a sub pulley delivered the power of the driving pulley; a power transmission shaft connecting the sub pulley and the blow blade.
Abstract:
본 발명은 α-아밀라아제의 첨가에 의해 형광 증백제의 함량이 감소된 제지 및 그 제조 방법에 관한 것이다. 형광증백제가 포함된 종이를 원료로 하여 재생지를 만드는 과정에 있어서, 원료 펄프의 해리과정에서 α-아밀라아제를 첨가함으로써, 재활용 폐지 내에 포함되어 있는 형광증백제의 약 50% 이상을 제거할 수 있다. 또한, 화합물을 사용하지 않고 효소를 사용하였으므로 친환경적인 방법으로 형광증백제의 함량이 감소된 제지를 제조할 수 있다. 형광증백제, 원료 펄프, 해리, α-아밀라아제
Abstract:
A paper with a reduced content of a fluorescent whitening agent and a manufacturing method thereof are provided to separate a remaining content of a fluorescent whitening agent from a paper and remove the remaining content by green technology using enzymes. In a method for manufacturing a paper with a reduced content of a fluorescent whitening agent, an endosperm layer is separated from raw material pulp in a pulper and/or a beater while carrying out hydrolysis for an endosperm layer containing a fluorescent whitening agent by adding enzymes such as amylase, cellulase, xylanase, and mixture thereof to the raw material pump, wherein the raw material pulp is treated with the endosperm layer. Impurities are removed from the beaten raw material pulp through a cleaner and/or a screen, so that perfect pulp stuff is screened from the raw material pulp. The pulp stuff is compressed, dried and wound on a winder.
Abstract:
본 발명은 스티렌-부타디엔계 라텍스, 이의 제조방법 및 이를 포함하는 코팅액에 관한 것으로, 보다 상세하게는 잉크젯 용지 바인더용 스티렌-부타디엔계 라텍스로서 에틸렌성 불포화산 단량체를 0.1 내지 1.5 중량부 포함하여 표면음전하밀도가 낮은 잉크젯 용지 바인더용 스티렌- 부타디엔계 라텍스, 이의 제조방법 및 이를 포함하는 코팅액에 관한 것이다. 본 발명에 따르면, 가격경쟁력과 도공작업성이 우수하고, 건조에너지 비용을 절감할 수 있는 잉크젯 용지용 코팅액 및 인쇄품질이 우수한 잉크젯 용지를 제공하는 효과가 있다. 잉크젯 용지, 바인더, 라텍스, 에틸렌성 불포화산 단량체, 표면음전하밀도, 유리전이온도
Abstract:
본 발명은 양성 팜(PAM)을 이용한 충전물 선응집이 적용된 종이 제조방법에 관한 것으로서, 1백만 ~ 8백만 g/mol인 분자량과 0.1 ~ 5.0 meq/g인 전하밀도를 갖는 양이온성 PAM을 첨가하여 충전제를 선응집시키고, 기존의 DDJ를 축소 제작한 filler mixing cell과 입도분석 장치인 DSD를 이용하여 충전물의 응집현상을 확인하고, 충전물 응집 시 양성 고분자의 투입량과 응집 시간 및 전단력을 조절하여 충전물 응집체의 입도와 분포를 적절히 조절하고, 상기 충전물 선응집체를 펄프를 함유하는 지료에 첨가하여 종이를 제조하고, 섬유 원료를 절감할 수 있는 양성 PAM을 이용한 충전물 선응집이 적용된 종이 제조방법에 관한 것이다. 선응집, 충전물, 양성 고분자, PAM, 백색도, 보류도, DDJ, 종이, DSD
Abstract:
Paper and a method for manufacturing the same are provided to remove fluorescence whitening agents of more than 50% from raw pulp in an eco-friendly method, thereby producing paper having excellent quality. Raw pulp is treated with a starch layer containing fluorescence whitening agents at a temperature of 65-85°C and a pH of 7-9. The treated pulp is dissociated using a pulper or a beater while alpha-amylase is added into the treated pulp to hydrolyze the treated pulp. The dissociated raw pulp is passed through a cleaner or a screen to remove external particles and refine a paper material from the dissociated raw pulp. The refined paper material is compressed, and wound around a winder.
Abstract:
A method for manufacturing paper applied filler preflocculation technology with cationic PAM is provided to increase the amount of the filler without degradation of strength of paper according to shear force and input of a polymer. A method for manufacturing paper applied filler preflocculation technology with cationic PAM comprises the following steps of: adding the cationic PAM having 0.1 ~ 5.0 meq/g of charge density and 1 million ~ 8 million g/mol of molecular weight; preflocculating the filler; and adding a piller aggregate containing pulp. A rate of cationic PAM and the filler is 99.09:0.01 ~ 99.00:1.00(W/W).
Abstract:
A styrene-butadiene latex binder for ink-jet paper is provided to ensure low negative charge density and predetermined glass transition temperature, to exhibit excellent price competitiveness and paint workability, and to save a drying energy cost. A styrene-butadiene latex binder for ink-jet paper comprises 20-85 parts by weight of a styrene-based monomer, 10-70 parts by weight of a butadiene-based monomer, 0.5-15 parts by weight of a vinyl cyan monomer, 0.1-1.5 parts by weight of an ethylenically unsaturated acid monomer, and 1-25 parts by weight of a monomer copolymerizable with the monomers, and has a glass transition temperature of 20-50 °C. The ethylenically unsaturated acid monomer is at least one selected from the group comprising unsaturated carboxylic acids and unsaturated polycarboxylic acid alkyl esters having at least one carboxylic acid group.
Abstract:
본 발명은 형광 증백제의 함량이 감소된 제지 및 그 제조 방법에 관한 것이다. 형광증백제가 포함된 종이를 원료로 하여 재생지를 만드는 과정에 있어서, 원료 펄프의 해리과정에서 아밀라아제, 셀룰라아제, 자일라네이즈 복합 효소등을 첨가함으로써, 재활용 폐지 내에 포함되어 있는 형광증백제의 약 50% 이상을 제거할 수 있다. 또한, 화합물을 사용하지 않고 효소를 사용하였으므로 친환경적인 방법으로 형광증백제의 함량이 감소된 제지를 제조할 수 있다. 형광증백제, 원료 펄프, 해리, 아밀라아제, 셀룰라아제, 자일라네이즈