公开(公告)号:KR1020090093702A
公开(公告)日:2009-09-02
申请号:KR1020080019389
申请日:2008-02-29
Applicant: 재단법인서울대학교산학협력재단
CPC classification number: C01B13/14 , B22F9/24 , B22F2301/15 , B22F2301/255 , B22F2304/054 , B82Y30/00 , B82Y40/00 , C01P2004/64
Abstract: A method for manufacturing a metal oxide-metal heterojunction nanoparticle is provided to vary the shapes of metal oxide-metal heterojunction nanoparticles such as a dumbbell shape and a flower shape. A method for manufacturing a metal oxide-metal heterojunction nanoparticle comprises the following steps of: mixing a metal precursor solution and an organic acid metal salt composite solution, wherein the metal precursor solution consists of a metal precursor, a surfactant and an organic solvent and the organic acid metal salt composite solution consists of an organic acid metal salt composite, the surfactant and the organic solvent; and pyrolyzing the mixture. The metal precursor is selected from the group consisting of HAuCl4.nH2O, H2PtCl6.nH2O, NiCl2 and AgNO3. The surfactant is selected among C1-C18 alkyl amines.
Abstract translation: 提供金属氧化物 - 金属异质结纳米颗粒的制造方法,以改变金属氧化物 - 金属异质结纳米颗粒的形状,例如哑铃形状和花形状。 金属氧化物 - 金属异质结纳米颗粒的制造方法包括以下步骤:将金属前体溶液和有机酸金属盐复合溶液混合,其中金属前体溶液由金属前体,表面活性剂和有机溶剂组成, 有机酸金属盐复合溶液由有机酸金属盐复合物,表面活性剂和有机溶剂组成; 并热解混合物。 金属前体选自HAuCl4.nH2O,H2PtCl6·6H2O,NiCl2和AgNO3。 表面活性剂选自C1-C18烷基胺。