公开(公告)号:KR1020110064329A
公开(公告)日:2011-06-15
申请号:KR1020090120870
申请日:2009-12-08
Applicant: 전남대학교산학협력단
CPC classification number: C01B6/23 , C01B3/0031 , C01B6/24 , C01G17/00
Abstract: PURPOSE: A method for preparing a hydrogen storage complex is provided to confirm storage and release of hydrogen by color change and to suppress rapid exothermic reaction. CONSTITUTION: A method for preparing a hydrogen storage complex comprises: a step of preparing an alkali borohydride solution; and a step of reacting the solution with germanium oxide. The alkali borohydride is selected among sodium borohydride, potassium borohydride, and lithium borohydride. The method further comprises a step of centrifuging and washing.
Abstract translation: 目的:提供一种制备储氢络合物的方法,用于通过变色确定氢的储存和释放,并抑制快速放热反应。 构成:一种制备储氢络合物的方法,包括:制备碱金属硼氢化物溶液的步骤; 以及使溶液与氧化锗反应的步骤。 碱式硼氢化钠选自硼氢化钠,硼氢化钾和硼氢化锂。 该方法还包括离心和洗涤步骤。
-
公开(公告)号:KR101119466B1
公开(公告)日:2012-03-20
申请号:KR1020100001511
申请日:2010-01-08
Applicant: 전남대학교산학협력단
IPC: C07F7/20
Abstract: 본 발명은 유기 관능기를 함유하는 유기실리카 미립자 및 이의 제조방법에 관한 것으로, 오디오, 비디오, 포장용 등에 사용되는 각종 필름의 점착 방지제(안티-블록킹제), 도료의 소광제, 치약의 점증제 및 연마제, 플라스틱 및 고무의 보강재, 식품 및 의약품의 첨가제, 광섬유 제조 원료, 크로마토그래피 충진제, 건조제, 촉매담체 등에 사용하기 적합한 유기실리카 미립자를 제공한다. 또한 본 발명은 졸-겔 공법에 의한 유기실리카 미립자의 제조방법에 있어서, 물에 알칼리 금속염 촉매와 수소화 실레인 전구체를 첨가하여 가수분해 및 중합 시키는 단계를 포함하는 유기실리카 미립자의 친환경적인 제조방법을 제공한다.
-
公开(公告)号:KR101113748B1
公开(公告)日:2012-02-27
申请号:KR1020090120870
申请日:2009-12-08
Applicant: 전남대학교산학협력단
Abstract: 본 발명은 수소저장 착물의 제조방법에 관한 것으로, 소듐보로하이드라이드, 칼륨보로하이드라이드, 리튬보로하이드라이드 중 어느 하나에서 선택되는 알칼리 붕소수소화물 수용액을 제조하는 단계; 상기 수용액과 게르마늄 산화물을 반응하는 단계;를 포함하는 안정한 수소저장 착물의 제조방법을 제공하는 것이다.
이산화게르마늄, 소듐보로하이드라이드, 수소저장, 수소방출-
公开(公告)号:KR1020110081380A
公开(公告)日:2011-07-14
申请号:KR1020100001511
申请日:2010-01-08
Applicant: 전남대학교산학협력단
IPC: C07F7/20
CPC classification number: C07F7/0849
Abstract: PURPOSE: An organic silica fine particle containing an organic functional group and a method for preparing the same are provided to enhance pore size. CONSTITUTION: A method for preparing organic silica fine particles by a sol-gel method comprises a step of adding alkali metal salt catalyst and hydrogenation silane precursor to the water. The alkali metal salt catalyst is denoted by chemical formula 1(MX), In chemical formula 1, M is Li, Na, K, Rb, or Cs, and X is F, Cl, Br, or I. The alkali metal salt catalyst is added in 10-30 weight parts based on 100 weight parts of hydrogenation silane precursor. The method for further comprises polymerization, isolation, washing, drying, and pulerizing.
Abstract translation: 目的:提供含有有机官能团的有机二氧化硅微粒及其制备方法,以增加孔径。 构成:通过溶胶 - 凝胶法制备有机二氧化硅细颗粒的方法包括向水中加入碱金属盐催化剂和加氢硅烷前体的步骤。 碱金属盐催化剂由化学式1(MX)表示,在化学式1中,M是Li,Na,K,Rb或Cs,X是F,Cl,Br或I.碱金属盐催化剂 加入10-30重量份的加氢硅烷前体100重量份。 进一步包括聚合,分离,洗涤,干燥和粉碎的方法。
-
-
-