Abstract: PURPOSE: A manufacturing method of a metallic catalyst for synthesizing carbon nano-tubes and a manufacturing method of the carbon nano-tubes using the same are provided to suppress the generation of carbon impurities in the process of synthesizing the carbon nano-tubes by using nickel or cobalt as a catalytic metal. CONSTITUTION: A manufacturing method of a metallic catalyst for synthesizing carbon nano-tubes includes the following: a catalyst mixed solution containing a catalytic metal, molybdenum(Mo), and magnesium(Mg) at the molar ratio of 1:0.25:8.75 is prepared; the catalyst mixed solution is heated at a temperature between 400 and 500 deg C to prepare a catalytic material; and the catalytic material is pulverized to obtain catalytic powder. The catalytic metal is nickel(Ni) or cobalt(Co). A manufacturing method of the carbon nano-tubes includes the following: the metallic catalyst is prepared; the metallic catalyst is positioned on a substrate to be reacted with carbon source gas in a chamber in order to synthesize the carbon nano-tubes; and oxygen gas is further arranged in the chamber in the process of synthesizing the carbon nano-tubes.
Abstract translation: 目的:提供一种用于合成碳纳米管的金属催化剂的制造方法和使用该纳米管的碳纳米管的制造方法,以通过使用镍来抑制碳纳米管合成过程中的碳杂质的产生 或钴作为催化金属。 构成:用于合成碳纳米管的金属催化剂的制造方法包括:制备含有摩尔比为1:0.25:8.75的催化剂金属,钼(Mo)和镁(Mg)的催化剂混合溶液 ; 催化剂混合溶液在400-500℃的温度下加热以制备催化材料; 将催化剂粉碎,得到催化剂粉末。 催化金属是镍(Ni)或钴(Co)。 碳纳米管的制造方法包括:制备金属催化剂; 金属催化剂位于基板上,与室内的碳源气体反应,以便合成碳纳米管; 在合成碳纳米管的过程中,室内进一步设置氧气。