公开(公告)号:KR1020100090377A
公开(公告)日:2010-08-16
申请号:KR1020090009598
申请日:2009-02-06
Applicant: 충남대학교산학협력단
CPC classification number: C01B32/956 , C01P2004/64 , C01P2006/90
Abstract: PURPOSE: A porosity nano silicon carbide and a manufacturing method thereof are provided to simplify processing conditions and prevent cracks. CONSTITUTION: A porosity nano silicon carbide manufacturing method includes next steps. A polymer precursor and silicone compound are mixed with solvent. The compound which is obtained in the stage is electro-spined in a sphere or fiber form. A heat-treatment process is executed for the electrospinning result. The polymer precursor is selected among petroleum pitch, coal type pitch, polyimide, polybenzimidazole, poly acrylonitrile, polyaramide, polyaniline, mesophase pitch, furfuryl alcohol, phenol, cellulose, sucrose, polyvinylchloride and their mixture.
Abstract translation: 目的:提供孔隙度纳米碳化硅及其制造方法,以简化加工条件并防止裂纹。 构成:孔隙度纳米碳化硅制造方法包括以下步骤。 将聚合物前体和硅氧烷化合物与溶剂混合。 在舞台中获得的化合物以球形或纤维形式电纺丝。 执行静电纺丝结果的热处理工艺。 聚合物前体选自石油沥青,煤型沥青,聚酰亚胺,聚苯并咪唑,聚丙烯腈,聚芳酰胺,聚苯胺,中间相沥青,糠醇,苯酚,纤维素,蔗糖,聚氯乙烯及其混合物。
-
公开(公告)号:KR101118213B1
公开(公告)日:2012-03-16
申请号:KR1020090009598
申请日:2009-02-06
Applicant: 충남대학교산학협력단
Abstract: 고온에서 내산화성을 갖는 다공성 나노 탄화규소 및 그 제조방법이 개시된다.
본 발명에 따른 내산화성을 갖는 다공성 나노 탄화규소의 제조방법은, (1) 폴리머 전구체와 실리콘다이옥사이드를 용매와 혼합하는 단계; (2) 상기 '단계 (1)'의 과정을 통하여 얻어진 혼합물을 구형상 또는 섬유형상으로 전기방사하는 단계; 및 (3) 상기 '단계 (2)'의 과정을 통하여 얻어진 전기방사 결과물에 열처리를 하는 단계를 포함하여 이루어진다.
다공성, 탄화규소, 전기방사, 내산화성
-