마르텐사이트 조직을 가진 초고강도 용융아연도금 강판 및 그 제조 방법
    3.
    发明公开
    마르텐사이트 조직을 가진 초고강도 용융아연도금 강판 및 그 제조 방법 无效
    具有极高强度的马氏体结构的热镀锌钢化片及其制造方法

    公开(公告)号:KR1020100034118A

    公开(公告)日:2010-04-01

    申请号:KR1020080093085

    申请日:2008-09-23

    Abstract: PURPOSE: An ultimate strength molten galvanized steel plate with a martensite structure and a manufacturing method thereof are provided to protect passengers when an accident occurs by improving the intensity of covering parts of a vehicle. CONSTITUTION: An ultimate strength molten galvanized steel plate with a martensite structure contains a steel plate and a molten galvanized steel layer. The steep plate includes the martensite structure. The steep plate contains 0.05wt%~0.20wt% of C, 0.5wt%~3.5wt% of Mn, 0.1wt%~0.8wt% of Si, 0.01wt%~1.5wt% of Al, 0.01wt%~1.5wt% of Cr, 0.01wt%~1.5wt% of Mo, 0.001wt%~0.05wt% of Ti, 20ppm~80ppm of N, 5ppm~50ppm of B remnant Fe and impurities.

    Abstract translation: 目的:提供具有马氏体结构的极限强度熔融镀锌钢板及其制造方法,以通过提高车辆的覆盖部件的强度来保护乘客。 构成:具有马氏体结构的极限强度熔融镀锌钢板包含钢板和熔融镀锌钢层。 陡板包括马氏体结构。 陡板含有0.05wt%〜0.20wt%的C,0.5wt%〜3.5wt%的Mn,0.1wt%〜0.8wt%的Si,0.01wt%〜1.5wt%的Al,0.01wt%〜1.5wt ,Cr的0.01wt%〜1.5wt%,Ti为0.001wt%〜0.05wt%,N为20ppm〜80ppm,B为残余Fe为5ppm〜50ppm。

    판상 재료의 구멍확장 방법
    4.
    发明公开
    판상 재료의 구멍확장 방법 无效
    如何延长板材的孔

    公开(公告)号:KR1020170060264A

    公开(公告)日:2017-06-01

    申请号:KR1020150164422

    申请日:2015-11-24

    Abstract: 본발명은구멍주변에생성된버의형성방향과반대방향으로펀칭하여직경을확장시킴에따라구멍주변에형성된버가밀려올라가는동안구멍주변에형성된미세한결함들이크랙의시발점이되어두께방향으로파단이발생하게되는것을지연시키면서구멍의직경을확장시키도록하여기존공정에비해재료의구멍확장성비를획기적으로증가시킬수 있음은물론산업적으로재료를성형함에있어성형성을증가시킬수 있는판상재료의구멍확장방법에관한것이다. 이를위한본 발명의판상재료의구멍확장방법은, a) 판상재료에구멍을형성하는단계; 및 b) 펀칭공정으로제작된 구멍주변에생성된버의형성방향과구멍확장공정시 펀치가올라오는방향을반대로두고구멍을확장시킴에따라버가밀려올라가는동안구멍주변에형성된미세한결함들이크랙의시발점이되어두께방향으로파단이발생하게되는것을지연시키며상기구멍의직경을확장시키는단계;를포함하는판상재료의구멍확장방법;를포함한다.

    Abstract translation: 与成形方向和细小缺陷,本发明断裂是在厚度方向是形成在所述周边孔爆破根据锡金在孔周围形成推毛刺的裂纹的起点在相反的方向上延伸冲裁孔周围所产生的飞边的直径 而发生在这里,以这样的延迟扩展形成,所述材料,所述孔的直径,以及工业可提高材料的扩孔率显着地相对于传统的过程,这可以增加板状材料的可模塑性方法扩孔 Lt。 为此,本发明的用于扩展板材的孔的方法包括以下步骤:a)在板材中形成孔; 和b)在使得形成在孔的周边而服务器是按照锡金与未来打孔的方向上隆起驱动的裂缝微细缺陷的形成方向和围绕此后冲压过程相反的孔所产生的毛刺的孔膨胀步骤中弹出延伸孔 并且通过延迟在厚度方向上发生破裂的起点来扩大孔的直径。