    Abstract: 본발명은피셔-트롭쉬합성용촉매의제조방법에관한것으로, a) 코발트함유화합물과, 에테르기를 2개이상함유하는폴리에테르화합물의용액을제조하는단계, b) 상기용액을실리카담체에함침시키는단계, c) 상기용액이함침된실리카담체를건조하는단계, 및 d) 건조후의실리카담체를소성하는단계를포함하며, 상기촉매전구체에포함된코발트함량이상기실리카담체의중량을기준으로약 12중량% 내지약 25중량%인피셔-트롭쉬합성용촉매전구체의제조방법을제공한다.

    Abstract translation: 本发明涉及一种用于Fisher-Tropsch合成的催化剂的制备方法。 更具体地说,制备方法包括以下步骤:a)制备含钴化合物的溶液和包含至少两个醚基团的聚醚化合物; b)将溶液浸渍在二氧化硅载体中; c)干燥浸渍溶液的二氧化硅载体; 和d)使干燥后获得的二氧化硅载体增塑。 包含在催化剂前体中的钴组分基于二氧化硅载体的重量构成约12至25重量%。

    고활성 피셔-트롭쉬 촉매의 제조방법
    2.
    发明公开
    고활성 피셔-트롭쉬 촉매의 제조방법 无效
    制备具有高活性的渔具 - 催化剂催化剂的方法

    公开(公告)号:KR1020150137733A

    公开(公告)日:2015-12-09

    申请号:KR1020140066125

    申请日:2014-05-30

    CPC classification number: B01J23/75 B01J37/02 B01J37/08 B01J37/16

    Abstract: 본발명은피셔-트롭쉬합성용촉매의제조방법에관한것으로, a) 코발트함유화합물과, 에테르기를 2개이상함유하는폴리에테르화합물의용액을제조하는단계, b) 상기용액을실리카담체에함침시키는단계, c) 상기용액이함침된실리카담체를건조하는단계, 및 d) 건조후의실리카담체를소성하는단계를포함하며, 상기촉매전구체에포함된코발트함량이상기실리카담체의중량을기준으로약 12중량% 내지약 25중량%인피셔-트롭쉬합성용촉매전구체의제조방법을제공한다.

    Abstract translation: 本发明涉及一种用于费 - 托合成的催化剂的制备方法。 另外,本发明提供了一种费 - 托合成用催化剂前体的制造方法,其特征在于,包括以下工序:a)制造由含钴化合物和含有2个以上醚基的聚醚化合物构成的溶液 ; b)将溶液浸渍到二氧化硅载体中; c)干燥浸渍有溶液的二氧化硅载体; 和d)使干燥的二氧化硅载体增塑,其中催化剂前体中所含的钴的含量相对于二氧化硅载体的重量为约12-25重量%。

    피셔-트롭쉬 촉매의 제조방법
    3.
    发明授权
    피셔-트롭쉬 촉매의 제조방법 有权
    制备捕鱼催化剂的方法

    公开(公告)号:KR101298783B1

    公开(公告)日:2013-08-26

    申请号:KR1020130068338

    申请日:2013-06-14

    CPC classification number: B01J23/75 B01J37/08 C10G2/00 C10G2/332

    Abstract: PURPOSE: A catalyst produced by using the manufacturing method of fisher-tropsch catalysts is provided to increase the yield of hydrocarbon with high-boiling point and light olefin because the catalyst is used in the fischer-tropsch synthesis to increase the conversion ratio of carbon monoxide and decrease the selectivity of methane as a main by-product. CONSTITUTION: A manufacturing method of a catalyst precursor for the fischer-tropsch synthesis comprises the steps of: a) producing a solution containing polyester compound with two or more type 1 transition metal compound and ether groups; b) immersing the solution into a carrier; c) drying the carrier with the solution; and d) sintering the dried carrier.

    Abstract translation: 目的:提供通过使用费托催化剂的制造方法生产的催化剂,以提高烃与高沸点和轻烯烃的收率,因为催化剂用于费 - 托合成以增加一氧化碳的转化率 并降低甲烷作为主要副产物的选择性。 构成:费 - 托合成的催化剂前体的制造方法包括以下步骤:a)制备含有两种或更多种1种过渡金属化合物和醚基的聚酯化合物的溶液; b)将溶液浸入载体中; c)用溶液干燥载体; 和d)烧结干燥的载体。