마이크로 에멀젼 공정을 이용한 Ag 나노 분말의 제조방법
    1.
    发明公开
    마이크로 에멀젼 공정을 이용한 Ag 나노 분말의 제조방법 失效
    使用微乳法制备尺寸为5-10nm的银纳米尺寸粉末的方法

    公开(公告)号:KR1020040093911A

    公开(公告)日:2004-11-09

    申请号:KR1020030027780

    申请日:2003-04-30

    CPC classification number: B22F9/24 B22F1/0044 B82Y40/00

    Abstract: PURPOSE: Provided is a method for preparing silver nano-sized powder having controlled particle size distribution of up to 100 nm by using micro-emulsion process. CONSTITUTION: The method for preparing Ag nano-sized powders comprises the steps of: mixing an aqueous solution of silver with a surfactant in an organic solvent to obtain a reverse micelle micro-emulsion; reducing silver by adding a reducing agent to the emulsion and agglutinating to obtain silver powder; and washing the powder to isolate from the organic solvent. Particularly, the organic solvent is at least one selected from cyclohexane and isooctane, and the surfactant is at least one selected from polyoxyethylene nonylphenyl ether and sodium bis(2-ethylhexyl) sulfonate. Further, the reducing agent may be 0.1-2 wt% of N2H4.xH2O.

    Abstract translation: 目的:提供一种通过使用微乳液法制备具有高达100nm的可控粒度分布的银纳米尺寸粉末的方法。 构成:制备Ag纳米尺寸粉末的方法包括以下步骤:将银水溶液与表面活性剂在有机溶剂中混合,得到反胶束微乳液; 通过向乳液中加入还原剂并凝集得到银粉来还原银; 并洗涤粉末与有机溶剂分离。 特别地,有机溶剂是选自环己烷和异辛烷中的至少一种,表面活性剂是选自聚氧乙烯壬基苯基醚和双(2-乙基己基)磺酸钠中的至少一种。 此外,还原剂可以为0.1〜2重量%的N 2 H 4·xH 2 O.

Patent Agency Ranking