公开(公告)号:KR101405517B1
公开(公告)日:2014-06-11
申请号:KR1020130057995
申请日:2013-05-22
Applicant: 한국과학기술연구원
IPC: B01J37/08 , B01J37/02 , B01J23/755
CPC classification number: B01J23/755 , B01J21/04 , B01J23/83 , B01J35/002 , B01J35/08 , B01J35/1019 , B01J35/1038 , B01J35/1061 , B01J37/0207 , B01J37/08 , C01B3/04 , C01B3/40 , C01B2203/0233 , C01B2203/0238 , C01B2203/1058 , C01B2203/1082 , Y02P20/52
Abstract: The present invention relates to a method for manufacturing a nickel-based catalyst for steam carbon dioxide reforming reaction (SCR) of natural gas and, more particularly, to a method for manufacturing a nickel-based catalyst that is represented by Ni/η-Al_2O_3 manufactured by repeatedly impregnating nickel into a spherical eta-alumina support, which has many acid points formed thereon, and drying the impregnated product dozens of times, thus supporting the nickel at high density. A catalyst manufactured by the manufacturing method according to the present invention exhibits excellent catalytic activity even under the severe conditions of high temperature and high pressure when applied to steam carbon dioxide reforming reaction, and has little carbon deposited thereon owing to the excellent durability of the catalyst.
Abstract translation: 本发明涉及天然气的蒸汽二氧化碳重整反应(SCR)的镍系催化剂的制造方法,更具体地说,涉及由Ni /η-Al_2O_3表示的镍系催化剂的制造方法 通过将镍重复浸渍到其上形成有许多酸点的球形等离子体 - 氧化铝载体上,并干燥浸渍的产物数十次,从而以高密度支撑镍。 通过本发明的制造方法制造的催化剂,即使在高温高压条件下,即使在蒸汽二氧化碳重整反应中也显示出优异的催化活性,由于催化剂的耐久性优异,因此在其上沉积少量碳 。