    Abstract: The improved method comprises (A) synthesizing liquid phase generated powder (3BaCuO2+2CuO) by mixing Ba and Cu in a ratio of 3:5, followed by calcining the mixture at 870 deg.C for 26 hours, (B) synthesizing Y2BaCuO5 powder by mixing Y, Ba and Cu in a ratio of 2:1:1, followed by calcinating the mixture at 925 deg.C for 23 hours and sintering the cold pressure moulded Y2BaCuO5 powder at 1,050 deg.C for 15 hours, and (C) surrounding Y2BaCuO5 sintered body with the liquid-phase generated powder and thermal-treating at 800-1,000 deg.C for 15-50 hours under the oxygen atmosphere.

    Abstract translation: 改进的方法包括(A)通过混合比例为3:5的Ba和Cu合成液相产生的粉末(3BaCuO2 + 2CuO),然后在870℃下煅烧26小时,(B)合成Y2BaCuO5粉末 通过将Y,Ba和Cu以2:1:1的比例混合,然后在925℃下煅烧该混合物23小时,并将冷压成型的Y2BaCuO5粉末在1050℃下烧结15小时,和(C )将Y2BaCuO5烧结体与液相产生粉末并在氧气氛下在800-1,000℃热处理15-50小时。

    YBa₂Cu₃O_7-x 초전도체의 개선된 제조 방법

    公开(公告)号:KR1019940011363A

    公开(公告)日:1994-06-21

    申请号:KR1019920021432

    申请日:1992-11-14

    Abstract: 본 발명은 Y : Ba : Cu의 비가 2:1:1인 소결체를 액상 형성 분말로 둘러싸서 압분체를 만들고 이를 YBa
    2 Cu
    3 O
    7-x 의 포정 반응 온도 이하의 온도에서 등온 열처리하는 것으로 이루어지는 YBa
    2 Cu
    3 0
    7-x 초전도체의 제조 방법이 제공된다. 이 방법에 의해 제조된 YBa
    2 Cu
    3 0
    7-x 초전도체는 입자들이 한 방향으로 배열되어 높은 임계 전류 밀도를 갖는다.