公开(公告)号:KR1020130029977A
公开(公告)日:2013-03-26
申请号:KR1020110093437
申请日:2011-09-16
Applicant: 한국과학기술원
IPC: C08L101/12 , C08K3/04 , C08K9/04 , C08J3/28
CPC classification number: C08K9/08 , C08J3/20 , C08J3/201 , C08J3/28 , C08K3/041 , C08L29/04 , C08L101/12
Abstract: PURPOSE: A carbon nanotube-polymer nanocomposite with improved tensile strength and elongation is provided to have high strength and electric conductivity by using a melt-mixing method. CONSTITUTION: A manufacturing method of a carbon nanotube-polymer nanocomposite comprises as follows: a step of forming the solution mixture of a hydrophilic polymer, carbon nanotube, and solvent; a step of forming a dispersant by applying external energy to the solution mixture; a step of removing the solvent from the dispersant and obtaining carbon nanotube powder coated with the hydrophilic polymer; and a step of melt-mixing the powder with the polymer. The carbon nanotube-polymer nanocomposite comprises 100.0 parts by weight of a polymer matrix, 0.1-5 parts by weight of a polyvinyl alcohol, and 0.1-20 parts by weight of carbon nanotube which is dispersed in the polymer matrix and coated with the polyvinyl alcohol.
Abstract translation: 目的:提供拉伸强度和伸长率提高的碳纳米管 - 聚合物纳米复合材料,通过使用熔融混合法具有高强度和导电性。 构成:碳纳米管 - 聚合物纳米复合材料的制造方法包括以下步骤:形成亲水性聚合物,碳纳米管和溶剂的溶液混合物的步骤; 通过向溶液混合物施加外部能量形成分散剂的步骤; 从分散剂中除去溶剂并获得涂覆有亲水性聚合物的碳纳米管粉末的步骤; 以及将粉末与聚合物熔融混合的步骤。 碳纳米管聚合物纳米复合材料包含100.0重量份的聚合物基质,0.1-5重量份的聚乙烯醇和0.1-20重量份的分散在聚合物基体中并用聚乙烯醇涂覆的碳纳米管 。