전기방사법을 이용한 코어-쉘 구조 나노섬유 리튬이차전지용 양극활물질의 제조방법 및 이에 의해 제조된 양극활물질
    1.
    发明授权

    公开(公告)号:KR101373538B1

    公开(公告)日:2014-03-13

    申请号:KR1020120124631

    申请日:2012-11-06

    Abstract: The present invention relates to a manufacturing method of positive electrode active material which has a shape of nanofiber having a large superficial dimension by using an electric radiation method. The present invention comprises: a first step of manufacturing a core viscous solution by mixing a source material measured as stoichiometric ratio according to an empirical formula which is represented as: LiFe1-xMxPO4 (0

    Abstract translation: 本发明涉及通过使用电辐射法具有大的表面尺寸的纳米纤维的形状的正极活性物质的制造方法。 本发明包括:第一步骤,通过混合根据经验公式测量的化学计量比的源材料来制造芯粘稠溶液,所述经验公式表示为:LiFe1-xMxPO4(0≤X≤1,M = Ni,Mn ,Co,V,Cr,Cu,Ti,Zr)和螯合剂与溶剂; 通过将根据以下经验公式测量的化学计量比的源材料混合制造壳粘稠溶液的第二步:其表示为:Li'N'O2(N = Mn,Fe,Co,Ni,Cu,Cr,V, Ti,Zn)和螯合剂与溶剂; 通过使用双喷嘴排出核心粘性溶液和外部粘稠溶液在核心粘稠溶液和壳粘性溶液中辐射电制造纳米纤维前体的第三步骤; 干燥纳米纤维前体的第四步骤; 以及使干燥的纳米纤维前体增塑的第五步骤。 本发明具有通过双喷嘴进行电辐射而提供具有增加的稳定性的正极活性物质的效果,由此制造核 - 壳结构的正极活性物质,其中磷酸铁锂铁芯的表面被稳定地覆盖 锂金属氧化物壳。 (标号)(AA)制造LiFe_1-XM_XPO_4芯粘性溶液; (BB)制造Li [N] O_2壳粘稠溶液; (CC)制造双喷嘴电辐射纳米纤维前体; (DD)干燥纳米纤维前体; (EE)增塑纳米纤维前体

Patent Agency Ranking