개선된 염색성을 갖는 폴리트리메틸렌테레프탈레이트섬유의제조방법
    1.
    发明公开
    개선된 염색성을 갖는 폴리트리메틸렌테레프탈레이트섬유의제조방법 失效
    生产具有改善的可染性的聚对苯二甲酸乙二醇酯纤维

    公开(公告)号:KR1020030021969A

    公开(公告)日:2003-03-15

    申请号:KR1020010055567

    申请日:2001-09-10

    Abstract: PURPOSE: A process of improving dyeability of polytrimethylene terephthalate fiber by instantly heat treating polytrimethylene terephthalate fiber at high temperature is provided which improves dyeability as compared to non-treatment and thus permits effective dyeing to be achieved at low temperature. CONSTITUTION: To dye polytrimethylene terephthalate fiber at lower temperature, it is subject to heat treatment at 180 to 200deg.C for 0.1 to 1.0sec. For an example, polytrimethylene terephthalate fiber articles are passed through a contact type heating apparatus at 180deg.C for 0.15 to 0.8sec and then dyed with a disperse dye(C.I. DISPERSE BLUE 79) at 25 to 95deg.C while elevating the temperate at a rate of 2deg.C/min.

    Abstract translation: 目的:提供通过在高温下立即热处理聚对苯二甲酸丙二醇酯纤维来提高聚对苯二甲酸丙二醇酯纤维的染色性的方法,其与非处理相比改善了染色性,从而允许在低温下实现有效染色。 构成:在较低温度下染色聚对苯二甲酸丙二醇酯纤维,在180〜200℃下进行0.1〜1.0秒的热处理。 例如,将聚对苯二甲酸丙二醇酯纤维制品在180℃下通过接触式加热装置进行0.15至0.8秒,然后在分散染料(CI DISPERSE BLUE 79)中以25至95℃进行染色,同时将温带升温至 速度2deg.C / min。

    개선된 염색성을 갖는 폴리트리메틸렌테레프탈레이트섬유의제조방법
    2.
    发明授权
    개선된 염색성을 갖는 폴리트리메틸렌테레프탈레이트섬유의제조방법 失效
    具有改善染色性能的聚对苯二甲酸丙二醇酯纤维的制造方法

    公开(公告)号:KR100490192B1

    公开(公告)日:2005-05-17

    申请号:KR1020010055567

    申请日:2001-09-10

    Abstract: 본 발명은 폴리트리메틸렌테레프탈레이트 섬유의 염색성을 향상시키는 방법에 관한 것으로서, 폴리트리메틸렌테레프탈레이트 섬유를 고온에서 순간 열처리하는 것을 특징으로 하며, 본 발명에 따라 순간 열처리한 폴리트리메틸렌테레프탈레이트 섬유는 처리하지 않은 섬유에 비해 염색성이 향상되어 훨씬 낮은 온도에서 염색이 가능하기 때문에 에너지를 절감할 수 있을 뿐만아니라 저온 염색이 요구되는 폴리트리메틸렌테레프탈레이트 섬유 제품의 제조에 매우 유용하다.