양자 개체 인증 장치 및 방법

    公开(公告)号:KR102222080B1

    公开(公告)日:2021-03-04

    申请号:KR1020200022326

    申请日:2020-02-24

    Abstract: 양자개체인증장치및 방법이개시된다. 본발명의일실시예에따른양자개체인증장치는개체와사전에공유된인증키에기반하여생성된인증양자상태를준비하는양자상태준비부; 기저장된고유연산자를상기인증양자상태에연산하여생성된양자상태를양자측정장치에게전송하고, 상기양자측정장치가상기양자상태에대해공개하는벨측정결과와상기인증양자상태로부터양자채널의안전성을검증하는양자채널검증부; 및상기양자채널의안전성이검증된경우, 상기벨측정결과와상기고유연산자를이용하여상기개체를인증하는양자개체인증부를포함한다.

    캐패시터 전극물질의 제조방법
    2.
    发明公开
    캐패시터 전극물질의 제조방법 无效
    电容器电极材料的制造方法

    公开(公告)号:KR1020130119833A

    公开(公告)日:2013-11-01

    申请号:KR1020120116702

    申请日:2012-10-19

    CPC classification number: C08L79/02 C08G73/0266 C08K3/04 H01G11/32

    Abstract: A capacitor electrode material provides a reaction solution including an activated charcoal, an anyline monomer, a dodecylbenzene sulfonate. A polymerization initiator is added to the reaction solution, so polyaniline surrounding the active charcoal can be manufactured from the aniline monomers. The dodecylbenzene sulfonate simultaneously functions as a doping acid and a surfactant. The concentration of dodecylbenezene sulfonate can be controlled in a manufacturing process to provide a capacitor electrode material with high electric capacity. [Reference numerals] (S10) Distribute active charcoal in a dodecylbenzene sulfonate;(S20) Add aniline monomers in the dodecylbenzene sulfonate where active charcoal is distributed;(S30) Synthesize polyaniline from the aniline monomers By adding a polymerization initiator

    Abstract translation: 电容器电极材料提供包含活性炭,丁烯单体,十二烷基苯磺酸盐的反应溶液。 向反应溶液中加入聚合引发剂,因此可以由苯胺单体制造活性炭周围的聚苯胺。 十二烷基苯磺酸盐同时用作掺杂酸和表面活性剂。 可以在制造工艺中控制十二烷基苯磺酸盐的浓度,以提供具有高电容的电容器电极材料。 (S10)在十二烷基苯磺酸盐中分配活性炭;(S20)在分散有活性炭的十二烷基苯磺酸盐中加入苯胺单体;(S30)从苯胺单体合成聚苯胺通过加入聚合引发剂

    슈퍼커패시터 전극 용 그래핀-이온성 액체 복합물의 제조 방법
    3.
    发明公开
    슈퍼커패시터 전극 용 그래핀-이온성 액체 복합물의 제조 방법 审中-实审
    制备超临界电极材料的石墨 - 离子液体复合材料的方法

    公开(公告)号:KR1020150009112A

    公开(公告)日:2015-01-26

    申请号:KR1020130082986

    申请日:2013-07-15

    CPC classification number: Y02E60/13 C01B32/23 B01J19/10 C01B2204/28 H01G11/32

    Abstract: 본 발명은 그래핀-이온성 액체 복합물의 제조 방법을 개시한다. 그의 제조 방법은, 그라파이트 산화물(graphite oxide)을 제조하는 것과 상기 그라파이트 산화물과 이온성 액체를 용매에 분산시키고 초음파 처리를 하여 단일 또는 복수층의 그라파이트 산화물-이온성 액체 복합물을 제조하는 것과 상기 그라파이트 산화물-이온성 액체 복합물에 수산화 붕소나트륨(NaBH
    4 )을 첨가하고 열에너지를 가하는 것을 포함한다.

    Abstract translation: 本发明涉及石墨烯离子液体复合材料的制造方法。 制造石墨烯离子液体复合材料的方法制造石墨烯氧化物,通过将氧化石墨和离子液体分散在溶剂中并进行超声波处理,制造单层或多层氧化石墨离子液体复合物,加入硼氢化钠(NaBH_4) 到石墨氧化物离子液体复合材料并施加热能。

    무기 필러를 포함하는 고분자 블렌드를 이용한 고체 고분자 전해질과 그 제조방법
    4.
    发明公开
    무기 필러를 포함하는 고분자 블렌드를 이용한 고체 고분자 전해질과 그 제조방법 无效
    聚合物共混固体聚合物电解质含有有机填料及其制造方法

    公开(公告)号:KR1020120096712A

    公开(公告)日:2012-08-31

    申请号:KR1020110015974

    申请日:2011-02-23

    Abstract: PURPOSE: A solid polymer electrolyte is provided to be manufactured by a simple and economic method, and to have high ion conductivity at room temperature by comprising inorganic filler and a high dielectric carbonate compound. CONSTITUTION: A solid polymer electrolyte comprises a blend of polyethylene oxide and polyethylene imine, a lithium salt, a high dielectric carbonate compound, and inorganic filler. Based on 100.0 parts by weight of the polyethylene oxide, comprised amount of the polyethylene imine, the lithium salt, the carbonate compound and the inorganic filler is respectively 10-40 parts by weight, 3-10 parts by weight, 50-30 parts by weight and 5-30 parts by weight. The lithium salt is one or more kinds selected from LiClO4, LiBF4 and LiPF6, the carbonate compound is one or more kinds selected from PC, EC, DMC, DEC and EMC, and the inorganic filler is one or more kinds selected from SiO2, TiO2, and RuO2.

    Abstract translation: 目的:提供一种固体聚合物电解质,通过简单经济的方法制造,并通过包含无机填料和高介电常数碳酸酯化合物在室温下具有高离子传导性。 构成:固体聚合物电解质包括聚环氧乙烷和聚乙烯亚胺的共混物,锂盐,高电介质碳酸盐化合物和无机填料。 基于100.0重量份的聚环氧乙烷,聚乙烯亚胺,锂盐,碳酸酯化合物和无机填料的含量分别为10〜40重量份,3-10重量份,50-30重量份 重量和5-30重量份。 锂盐是选自LiClO 4,LiBF 4和LiPF 6中的一种或多种,​​碳酸酯化合物是选自PC,EC,DMC,DEC和EMC中的一种或多种,​​无机填料是选自SiO 2,TiO 2中的一种或多种 ,和RuO 2。

    폴리아닐린-금속 복합체 제조방법
    5.
    发明公开
    폴리아닐린-금속 복합체 제조방법 无效
    制备聚氨酯金属复合材料的方法

    公开(公告)号:KR1020120092288A

    公开(公告)日:2012-08-21

    申请号:KR1020110012234

    申请日:2011-02-11

    Abstract: PURPOSE: A manufacturing method of a polyaniline-metal composite is provided to manufacture a polyaniline-metal composite with uniform size and low resistance without additional process. CONSTITUTION: A manufacturing method of a polyaniline-metal composite uses 0.05-0.2 mole oxidizer as a starting material based on 1 mole of an aniline monomer and 0.04-0.5 mole of a dopant. The dopant is an inorganic acid, organic acid, or a mixture thereof. The oxidizer is a water-soluble metal precursor of one or more kinds selected from a group consisting of H2PtCl6, K2PtCl6, and K2AuCl6.

    Abstract translation: 目的:提供聚苯胺 - 金属复合材料的制造方法,制造均匀尺寸和低电阻的聚苯胺 - 金属复合材料,无需附加工艺。 构成:聚苯胺 - 金属复合体的制造方法使用基于1摩尔苯胺单体和0.04-0.5摩尔掺杂剂的0.05-0.2摩尔氧化剂作为原料。 掺杂剂是无机酸,有机酸或其混合物。 氧化剂是选自H2PtCl6,K2PtCl6和K2AuCl6中的一种或多种的水溶性金属前体。