염료 감응 태양 전지 및 그 제조 방법
    2.
    发明公开
    염료 감응 태양 전지 및 그 제조 방법 有权
    DYE SENSITIZED SOLAR CELL AND METHOD OF FABRICATING THE SAME

    公开(公告)号:KR1020090038631A

    公开(公告)日:2009-04-21

    申请号:KR1020070104023

    申请日:2007-10-16

    Abstract: A dye-sensitized solar cell and a manufacturing method thereof are provided to maximize photoelectric energy conversion efficiency by minimizing a moving path of an electron in an electrode structure. An electrode structure of a dye-sensitized solar cell includes a conductor layer(120), an oxide semiconductor layer(122), and a dye layer(124). The conductor layer includes regularly arranged holes. The oxide semiconductor layer is formed on a surface of the conductor layer by using one method selected among a deep coating method, an electrophoretic method, and an electroplating method. The oxide semiconductor layer includes a titanium oxide. The dye layer is formed on a surface of the oxide semiconductor layer.

    Abstract translation: 提供染料敏化太阳能电池及其制造方法,以通过使电极结构中的电子的移动路径最小化来最大化光电转换效率。 染料敏化太阳能电池的电极结构包括导体层(120),氧化物半导体层(122)和染料层(124)。 导体层包括规则排列的孔。 通过采用深涂法,电泳法,电镀法等一种方法,在导体层的表面形成氧化物半导体层。 氧化物半导体层包括氧化钛。 染料层形成在氧化物半导体层的表面上。

    염료감응 태양전지 및 그 제조 방법
    3.
    发明公开
    염료감응 태양전지 및 그 제조 방법 有权
    致密的太阳能电池及其制造方法

    公开(公告)号:KR1020090019485A

    公开(公告)日:2009-02-25

    申请号:KR1020070083952

    申请日:2007-08-21

    Abstract: A die-sensitized solar cells and method for manufacturing the same is provided to prevent electronic loss by interaction with the electronics from dyes and oxidation/deoxidation electrolyte on the surface of the surface of the metal oxide layer or the conductive substrate. In a die-sensitized solar cells and method for manufacturing the same, the dye-sensitized solar cell comprises a semiconductor electrode(10), an opposing electrode, and electrolyte solution. The semiconductor electrode includes a first conductive substrate and an electron transport layer(13) on the first conductive substrate. The electron transport layer comprises the dye molecule layer(16) absorbed to the surface of the metal oxide layer and the metal oxide layer(14) formed on the first conductive substrate. The insulating protection layer(18) is formed on a part of surface on the metal oxide layer not covering with the dye molecule layer or a part of the surface of the conductive substrate not contacting with the metal oxide layer.

    Abstract translation: 提供了一种模具增感太阳能电池及其制造方法,以通过与金属氧化物层或导电性基体的表面的染料和氧化/脱氧电解质的电子元件的相互作用来防止电子损失。 在模具增感太阳能电池及其制造方法中,染料敏化太阳能电池包括半导体电极(10),相对电极和电解质溶液。 半导体电极在第一导电衬底上包括第一导电衬底和电子传输层(13)。 电子传输层包括被吸收到金属氧化物层的表面上的染料分子层(16)和形成在第一导电衬底上的金属氧化物层(14)。 绝缘保护层(18)形成在金属氧化物层的不被染料分子层覆盖的表面的一部分上,或导电性基材的与金属氧化物层不接触的部分表面。

    나노 복합체의 제조방법 및 이를 이용한 염료감응 태양전지의 제조방법
    6.
    发明公开
    나노 복합체의 제조방법 및 이를 이용한 염료감응 태양전지의 제조방법 有权
    纳米复合材料及其制造方法,以及透明的太阳能电池

    公开(公告)号:KR1020090033713A

    公开(公告)日:2009-04-06

    申请号:KR1020070098887

    申请日:2007-10-01

    Abstract: A nanocomposite is provided to increase a surface area of nanoparticles in order to improve the amount of dye molecule absorbed and allow electron to move freely using nanotubes. A nanocomposite(120) comprises a plurality of nanotubes formed in a perpendicular direction of a substrate and a plurality of nanoparticles(110) dispersed between the nanotubes(100). The nanotubes and the nanoparticles contain titanium oxide(TiO2), tin oxide(SnO2), zinc oxide(ZnO) and tungsten oxide(WO3) or a mixture thereof. An outer diameter of nanotube is 50nm to 300nm. An inner diameter of nanotube shows 50nm to 200nm. A size of the nanoparticle is 2nm to 50nm. The nanoparticle has a formation of sphere, tube, rod or tubular shape.

    Abstract translation: 提供纳米复合材料以增加纳米颗粒的表面积,以改善吸收的染料分子的量,并允许电子使用纳米管自由移动。 纳米复合材料(120)包括在基底的垂直方向上形成的多个纳米管和分散在纳米管(100)之间的多个纳米颗粒(110)。 纳米管和纳米颗粒含有氧化钛(TiO 2),氧化锡(SnO 2),氧化锌(ZnO)和氧化钨(WO 3)或其混合物。 纳米管的外径为50nm至300nm。 纳米管内径为50nm〜200nm。 纳米颗粒的尺寸为2nm至50nm。 纳米颗粒具有球形,管状,棒状或管状形状。

    염료감응 태양전지 및 그 제조 방법
    7.
    发明授权
    염료감응 태양전지 및 그 제조 방법 有权
    염료감응전지및그제조방법

    公开(公告)号:KR100932901B1

    公开(公告)日:2009-12-22

    申请号:KR1020070083952

    申请日:2007-08-21

    Abstract: 전해질 용액에 용해된 유기 분자가 자기조립되어 형성된 절연 보호막이 형성된 반도체 전극을 구비하는 염료감응 태양 전지 및 그 제조 방법에 관하여 개시한다. 본 발명에 따른 염료감응 태양전지는 제1 전도성 기판상에 형성된 금속산화물층과, 금속산화물층의 표면에 흡착되어 있는 염료 분자층과, 금속산화물층의 표면에서 염료 분자층으로 덮이지 않은 제1 부분 및 제1 전도성 기판의 표면에서 금속산화물층이 접촉하고 있지 않은 제2 부분 중 적어도 하나의 부분 위에 형성된 절연 보호막을 포함한다. 반도체 전극과 대향 전극과의 사이의 공간에는 금속산화물 위에 자기조립될 수 있는 작용기를 가지는 유기 분자들이 용해되어 있는 전해질 용액이 채워져 있다. 반도체 전극과 대향 전극과의 사이에 전해질 용액을 주입하면 전해질 용액이 전자 전달층에 접촉되면서 유기분자들이 제1 부분 또는 제2 부분에 자기조립되어 절연 보호막이 형성된다.
    염료감응, 태양전지, 자기조립, 절연 보호막, 금속산화물, 전해질

    Abstract translation: 本发明提供染料敏化太阳能电池和染料敏化太阳能电池的制造方法,该半导体电极上形成有通过自组装有机分子而形成的绝缘保护层,该染料敏化太阳能电池具有染料敏化太阳能电池, 单元包括:半导体电极,包括:形成在第一导电衬底上的金属氧化物层; 吸附在金属氧化物层的表面上的染料分子层; 以及绝缘保护层,所述绝缘保护层形成在所述金属氧化物层的未被所述染料分子层覆盖的所述表面的第一部分和所述第一导电衬底的不接触所述金属氧化物的表面的第二部分中的至少一个上 层; 设置在第二导电衬底上并且面向所述半导体电极的相对电极; 以及填充在半导体电极和相对电极之间的空间中的电解质溶液,所述电解质溶液包含具有官能团的有机分子,所述官能团可以通过化学键与金属氧化物上的金属氧化物选择性地自组装。 一旦电解质溶液注入到半导体电极和相对电极之间,电解质溶液接触电子传输层,并且因此有机分子在第一部分或第二部分上自组装以形成绝缘保护层。

    염료감응 태양전지 및 그의 제조 방법
    9.
    发明公开
    염료감응 태양전지 및 그의 제조 방법 有权
    透明的太阳能电池及其制造方法

    公开(公告)号:KR1020090065177A

    公开(公告)日:2009-06-22

    申请号:KR1020070132642

    申请日:2007-12-17

    Abstract: A dye-sensitized solar cell and a manufacturing method thereof are provided to maximize efficiency by preventing effectively recombination of an electrolyte and electrons transmitted to a conductor. A semiconductor electrode(110) includes a conductive substrate(112), an oxide semiconductor-conductor structure(115), and a dye molecule layer(117). The oxide semiconductor-conductor structure is formed on an upper surface of the conductive substrate. The dye molecule layer is absorbed in a surface of an oxide semiconductor(114). The conductive substrate is electrically connected with the oxide semiconductor-conductor structure. A conductor(113) of the oxide semiconductor-conductor structure is electrically connected with the conductive substrate.

    Abstract translation: 提供染料敏化太阳能电池及其制造方法,以通过防止电解质和传输到导体的电子的有效复合来最大化效率。 半导体电极(110)包括导电基板(112),氧化物半导体 - 导体结构(115)和染料分子层(117)。 氧化物半导体 - 导体结构形成在导电基板的上表面上。 染料分子层被吸收在氧化物半导体(114)的表面中。 导电基板与氧化物半导体 - 导体结构电连接。 氧化物半导体 - 导体结构的导体(113)与导电基板电连接。