公开(公告)号:KR100036791B1
公开(公告)日:1990-10-18
申请号:KR1019860005544
申请日:1986-07-09
Applicant: 한국조폐공사
IPC: C09D11/033 , C09D11/02
-
公开(公告)号:KR1019900004227B1
公开(公告)日:1990-06-18
申请号:KR1019860005544
申请日:1986-07-09
Applicant: 한국조폐공사
IPC: C09D11/033 , C09D11/02
Abstract: Printing inks are prepd. by mixing pigments, epoxyresin varnish 25-50 wt.% [obtd. by (a) adding epoxyresin 17.2 wt.% (epoxy eq.= 800-1000, hydroxy eq.= 145-175, mol. wt.= 900-1400) to flax oil fatty acid 34.3 wt.%, (b) heating in the presence of inert gas and LiOH (catalyst) at 100-120 deg.C, (c) esterifying for 1.5-2 hr at 240-260 deg. C on a strrer, (d) cooling to 130 deg. C and reacting with trimethylolpropane 11.8 wt.% and phthalic anhydride 8.8 wt.% for 20- 30 min at 200-300 deg.C, (e) cooling to 130 deg. C at acid value 35- 40 and reacting with anhydrous mellitic acid 2.9 wt.% for 10-20 min at 200-230 deg. C, and (f) cooling and adding fatty hydrocarbon solvent (bp 230-320) 25.0 wt.% and diethyleneglycole monobutylether 1-10 wt.%.
Abstract translation: 印刷油墨已经准备好了。 通过混合颜料,25-50重量%的环氧树脂清漆[ 通过(a)将17.2重量%的环氧树脂(环氧当量= 800-1000,羟基当量= 145-175,摩尔重量= 900-1400)加入到34.3重量%的亚麻油脂肪酸中,(b)加热 在惰性气体和LiOH(催化剂)存在下,在100-120℃下,(c)在240-260℃下酯化1.5-2小时。 (d)冷却到130度。 并在200-300℃下与11.8重量%的三羟甲基丙烷和邻苯二甲酸酐8.8重量%反应20-30分钟,(e)冷却至130℃。 C,酸值35-40,并与无水苯氯酸反应,在200-230℃下反应2.9重量%,持续10-20分钟。 (f)冷却并加入25.0重量%的脂肪烃溶剂(沸点230-320)和二乙二醇单丁醚1-10重量%。
-
-
公开(公告)号:KR1019960013836B1
公开(公告)日:1996-10-10
申请号:KR1019930008517
申请日:1993-05-19
Applicant: 한국조폐공사
IPC: D21H21/42
Abstract: The antifalsification paper is produced by the steps of: carrying out dye exhaustion to a fiber yarn(1) having a denier of 10-30 as a security thread(4,5,6) at regular intervals in the isolated condition from the air by isolation region(2,3) of about 2-5 mm wide, and then subjecting the fiber(3) to move as much as expected distance from the isolation region(2,3), followed by doing the dye exhaustion again to undyed-exhaustion part of the fiber yarn to give two colors or more.
Abstract translation: 该防伪纸是通过以下步骤制造的:在与空气隔离的条件下,以规定的间隔,以10-30旦尼尔的纤维纱线(1)作为安全线(4,5,6)进行染色耗尽 隔离区域(2,3)约2-5mm宽,然后使纤维(3)从隔离区域(2,3)预期的距离移动,然后再次进行染色剂耗尽, 纤维纱的耗尽部分给出两种或更多种颜色。
-
公开(公告)号:KR1019940007294A
公开(公告)日:1994-04-27
申请号:KR1019920016096
申请日:1992-09-04
Applicant: 한국조폐공사
Abstract: 본 발명은 은화 중의 특정위치에 인쇄층을 형성시키는 방법과 그에 의해 제조된 용지에 관한 것으로 , 은화는 초지 공정중에서 형성시키는 것이므로 그 형상이나 위치가 일정치 못하여 은화중의 특정위치에 인쇄층을 형성시킨다는 것은 불가능하였던바, 본 발명은 초지기 출측에 설치한 은화형성장치(P)의 직하부에 인쇄롤(5)을 비롯한 인쇄장치를 설치하여, 은화전사롤(3)에 의해 전사형성된 은화(11)에 인쇄롤(5)에 의해 인쇄층을 형성시킨 후 건조하는 것을 특징으로 하는 것임.
-
-
-
公开(公告)号:KR1019950014485A
公开(公告)日:1995-06-16
申请号:KR1019930025561
申请日:1993-11-27
Applicant: 한국조폐공사
IPC: D21H21/44
Abstract: 본 발명은 10내지 30데니어의 천연섬유사나 합성섬유사에 가시적으로 판별이 가능하도록 청색계 또는 갈색계 산성염료나 식물성 추출천연색소를 염착시키고, 2차로 바탕색과는 다른 색상으로 발현되는 형광안료나 형광증백제를 2차염착하므로서 가시적으로 발현되는 색과 형광램프에 의해 발현되는 색이 다르게하여 위조감별이 용이하게 한 것임.
-
公开(公告)号:KR1019950014484A
公开(公告)日:1995-06-16
申请号:KR1019930025560
申请日:1993-11-27
Applicant: 한국조폐공사
IPC: D21H21/44
Abstract: 본 발명은 위조방지용지의 제조방법에 관한 것으로, 특히 선특허제 64258호의 개량발명인바, 금망(3)에 칩(6)을 설치하여 칩(6)의 상면에 지층이 형성되는 것을 방해하고, 쿠칭롤로 주변의 지층을 칩(6)의 상면부위로 밀어 칩(6)상면에 얇은 지층이 형성되게 하여 돌출은화(2)를 형성시킴에 있어서, 칩(6)에 무늬나 문자등의 모양을 가지는 관통부(7)를 형성시키므로서 통공(7)부위에 재료가 쌓이게 하여 돌출은화(2)내부중에서 관통부(7)에 대응하는 부위가 돌출부(8)를 형성시키게 함을 특징으로 하는 것임.
-
-
-
-
-
-
-
-
-