피엔에이 함유 잉크 및 이의 확인방법
    1.
    发明公开
    피엔에이 함유 잉크 및 이의 확인방법 无效
    含有PNA的INK及其识别方法

    公开(公告)号:KR1020080060744A

    公开(公告)日:2008-07-02

    申请号:KR1020060135203

    申请日:2006-12-27

    CPC classification number: C09D11/03 C12Q1/68

    Abstract: An ink containing a small amount of peptide nucleic acid is provided to identify authenticity of a peptide nucleic acid in a matter printed with the ink while realizing improved durability of the ink. A printing ink comprises 0.000007-0.02 wt% of peptide nucleic acid for identifying authenticity. In a variant, a paint or coating solution comprises 0.000007-0.02 wt% of peptide nucleic acid for identifying authenticity. To detect peptide nucleic acid for identifying authenticity in a product using the printing ink, paint or coating solution, the peptide nucleic acid(PNA) is contacted with a PNA chip, in which a single spiral PNA complementary to the PNA and one to three optional single spiral PNAs are integrated, and then with a phosphor.

    Abstract translation: 提供含有少量肽核酸的油墨,以识别印刷有油墨的物质中的肽核酸的真实性,同时实现油墨的改善的耐久性。 印刷油墨包含0.000007-0.02重量%的用于鉴定真实性的肽核酸。 在一个变体中,涂料或涂料溶液包含0.000007-0.02重量%的用于鉴定真实性的肽核酸。 为了检测使用印刷油墨,油漆或涂层溶液鉴定产品真实性的肽核酸,肽核酸(PNA)与PNA芯片接触,其中与PNA互补的单螺旋PNA和一至三个可选的 单螺旋PNA被整合,然后与磷光体。

    위조방지용 기능성 섬유
    2.
    发明授权
    위조방지용 기능성 섬유 有权
    功能纤维预防

    公开(公告)号:KR100808651B1

    公开(公告)日:2008-02-29

    申请号:KR1020060135258

    申请日:2006-12-27

    CPC classification number: D01D5/32 B42D25/378

    Abstract: A forgery preventive functional fiber is provided to mix the specific pigment into the complex fiber with a side-by-side type, thereby displaying the functionality. A first and a second components as the synthetic polymer chip are heated, mixed and spun so that the forgery preventive functional fiber is manufactured. The forgery preventive functional fiber is dyed by the specific pigment. Polyester, nylon, polypropylene, polyethylene and polyurethane are used as the mixing polymer of the first component and the second component. The same polymer or different mixing polymers are used as the mixing polymer of the first and second components according to the mixing property of the specific pigment. Colored pigment, fluorescent pigment, infrared pigment and the like are used as the specific pigment and added differently to the first and second components so that various effects are represented.

    Abstract translation: 提供防伪功能性纤维,以将并排型的特定颜料混合到复合纤维中,从而显示功能性。 加热,混合和纺丝作为合成聚合物芯片的第一和第二组分,从而制造防伪功能性纤维。 防伪功能纤维由特定颜料染色。 聚酯,尼龙,聚丙烯,聚乙烯和聚氨酯用作第一组分和第二组分的混合聚合物。 根据特定颜料的混合性质,使用相同的聚合物或不同的混合聚合物作为第一和第二组分的混合聚合物。 使用着色颜料,荧光颜料,红外线颜料等作为特定颜料,并且不同地添加到第一和第二组分,从而表现出各种效果。

    발광체 및 이의 제조방법
    3.
    发明授权
    발광체 및 이의 제조방법 有权
    LUMINESCENT材料及其制备方法

    公开(公告)号:KR100779237B1

    公开(公告)日:2007-11-28

    申请号:KR1020060135194

    申请日:2006-12-27

    Abstract: A method for preparing a luminescent material is provided to obtain a luminescent material having excellent stability and printability and suitable for a printing ink for preventing forgery. A method for preparing a luminescent material comprises the steps of mixing and pulverizing lanthanum trifluoride as a host material, holmium chloride, holmium nitrate or holmium oxide as an activator, and lithium oxide, lithium chloride, lithium hydroxide, potassium chloride or sodium chloride as a flux; and putting the obtained one in an electric furnace, increasing the temperature to 300 deg.C over 1 hour, maintaining the temperature for 1 hour, increasing the temperature to 1,100 deg.C over 3 hours, maintaining the temperature for 2 hours, and cooling the temperature to a room temperature to prepare a luminescent material represented by LaF3:Ho^3+, M, wherein M is Li^+, K^+ or Na^+.

    Abstract translation: 提供一种制备发光材料的方法以获得具有优异的稳定性和可印刷性的发光材料,并且适用于防止伪造的印刷油墨。 制备发光材料的方法包括将作为主体材料的三氧化镧混合和粉碎,作为活化剂的氯化钬,硝酸钬或氧化钬以及作为活化剂的氧化锂,氯化锂,氢氧化锂,氯化钾或氯化钠的步骤 通量; 并将所得到的装置放入电炉中,在1小时内将温度升高至300℃,保持温度1小时,3小时内将温度升高至1100℃,保持温度2小时,冷却 温度至室温以制备由LaF 3:Ho 3+,M表示的发光材料,其中M为Li +,K +或Na +。