나노 세공을 갖는 금속 함유 VSB-5 분자체 조성물과이의 제조방법
    1.
    发明公开
    나노 세공을 갖는 금속 함유 VSB-5 분자체 조성물과이의 제조방법 有权
    金属纳入的纳米VSB-5分子筛组合物及其使用无机碱或有机碱作为PH调节材料制备其的方法

    公开(公告)号:KR1020050019530A

    公开(公告)日:2005-03-03

    申请号:KR1020030057350

    申请日:2003-08-19

    Abstract: PURPOSE: To provide a noble VSB-5 molecular sieve composition containing metal components and a method for preparing a VSB-5 molecular sieve, which is able to prepare the VSB-5 molecular sieve through an economic and efficient method using an inexpensive inorganic base or mono-amine. CONSTITUTION: In the method for preparing nanoporous VSB-5 molecular sieve by crystallizing a raw material consisting of a nickel compound and a phosphorous compound using a base, one or two metals selected from the group consisting of transition metals, typical metals, noble metals, and lanthanium are contained in the raw material, an inorganic base or an organic amine is added to the raw material, and the crystallization is performed under pH of 7.0-12.0 and at the temperature of 50-350 deg.C.

    Abstract translation: 目的:提供一种含有金属成分的高分子VSB-5分子筛组合物和制备VSB-5分子筛的方法,该方法能够通过经济有效的方法制备VSB-5分子筛,使用廉价的无机碱或 单胺。 构成:在使用碱使由镍化合物和磷化合物构成的原料结晶而制备纳米多孔VSB-5分子筛的方法中,选自过渡金属,典型金属,贵金属, 原料中含有镧,在原料中加入无机碱或有机胺,在7.0〜10.0的pH和50〜350℃的温度下进行结晶。

    나노 세공을 갖는 VSB-5 분자체의 제조방법
    4.
    发明公开
    나노 세공을 갖는 VSB-5 분자체의 제조방법 有权
    使用无机碱或单胺加热处理步骤制备纳米VSB-5分子筛的方法

    公开(公告)号:KR1020050019340A

    公开(公告)日:2005-03-03

    申请号:KR1020030057002

    申请日:2003-08-18

    Abstract: PURPOSE: To provide a method for preparing a VSB-5 molecular sieve, which is able to prepare the VSB-5 molecular sieve having good physical properties through an economic and efficient method using an inexpensive inorganic base or mono-amine. CONSTITUTION: In the method for preparing nanoporous VSB-5 molecular sieve by crystallizing a nickel compound and a phosphorous compound using a base, an inorganic base or a mono-amine is used as the base, and the crystallization is performed under pH of 7.0-12.0 and at the temperature of 50-350 deg.C.

    Abstract translation: 目的:提供一种制备VSB-5分子筛的方法,该方法能够通过使用便宜的无机碱或单胺的经济有效的方法制备具有良好物理性能的VSB-5分子筛。 构成:在通过使用碱使镍化合物和磷化合物结晶而制备纳米多孔VSB-5分子筛的方法中,使用无机碱或单胺作为碱,结晶在pH 7.0〜 12.0℃,温度为50-350℃。