폴리에틸렌 왁스의 분자량 분획정제방법 및 그 장치
    1.
    发明授权
    폴리에틸렌 왁스의 분자량 분획정제방법 및 그 장치 失效
    폴리에틸렌왁스의분자량분획정제방법및그장치

    公开(公告)号:KR100417059B1

    公开(公告)日:2004-02-05

    申请号:KR1020010022578

    申请日:2001-04-26

    Abstract: PURPOSE: Provided is a method for crystallizing polyethylene wax and fractionating the wax according to average molecular weight with narrow molecular weight distribution, so as to purify the wax in high purity. CONSTITUTION: The method comprises the steps of (i) mixing a crystallizing solvent having concentration of 1-95% and a raw material in a crystallizer(S1); (ii) elevating temperature of the mixture so as to liquidize the raw material(S2); (iii) cooling temperature of the mixture at supercooling temperature of 30-110 deg.C and cooling velocity of 0.1-10 deg.C/minute(S3); crystallizing the cooled raw material(S4); and filtrating the crystallized material(S5). The crystallizing solvent is selected from the group consisting of saturated hydrocarbon, ketone, monocyclic aromatic hydrocarbon, polycyclic aromatic hydrocarbon, olefinic hydrocarbon, and mixture thereof.

    Abstract translation: 用途:提供一种使聚乙烯蜡结晶并按照平均分子量分级并且分子量分布窄的方法,从而以高纯度纯化蜡的方法。 组成:该方法包括以下步骤:(i)在结晶器(S1)中混合浓度为1-95%的结晶溶剂和原料; (ii)升高混合物的温度以便使原料(S2)液化; (iii)在30-110℃的过冷温度和0.1-10℃/分钟的冷却速度下混合物的冷却温度(S3); 结晶冷却的原料(S4); 并过滤结晶材料(S5)。 结晶溶剂选自饱和烃,酮,单环芳烃,多环芳烃,烯烃和它们的混合物。

    폴리에틸렌 왁스의 분자량 분획정제방법 및 그 장치
    2.
    发明公开
    폴리에틸렌 왁스의 분자량 분획정제방법 및 그 장치 失效
    通过分子量分解聚乙烯泡沫的方法

    公开(公告)号:KR1020020083226A

    公开(公告)日:2002-11-02

    申请号:KR1020010022578

    申请日:2001-04-26

    Abstract: PURPOSE: Provided is a method for crystallizing polyethylene wax and fractionating the wax according to average molecular weight with narrow molecular weight distribution, so as to purify the wax in high purity. CONSTITUTION: The method comprises the steps of (i) mixing a crystallizing solvent having concentration of 1-95% and a raw material in a crystallizer(S1); (ii) elevating temperature of the mixture so as to liquidize the raw material(S2); (iii) cooling temperature of the mixture at supercooling temperature of 30-110 deg.C and cooling velocity of 0.1-10 deg.C/minute(S3); crystallizing the cooled raw material(S4); and filtrating the crystallized material(S5). The crystallizing solvent is selected from the group consisting of saturated hydrocarbon, ketone, monocyclic aromatic hydrocarbon, polycyclic aromatic hydrocarbon, olefinic hydrocarbon, and mixture thereof.

    Abstract translation: 目的:提供聚乙烯蜡结晶方法,按照分子量分布窄的平均分子量对蜡进行分馏,以纯化蜡。 方法:该方法包括以下步骤:(1)在结晶器中混合浓度为1-95%的结晶溶剂和原料(S1); (ii)提高混合物的温度以使原料液化(S2); (iii)过冷却温度为30-110℃,冷却速度为0.1-10℃/分钟的混合物的冷却温度(S3); 使冷却的原料结晶(S4); 并过滤结晶物(S5)。 结晶溶剂选自饱和烃,酮,单环芳烃,多环芳烃,烯烃,及其混合物。