公开(公告)号:JPH03207636A
公开(公告)日:1991-09-10
申请号:JP26295890
申请日:1990-09-29
Applicant: 3 D SYSTEMS INC
Inventor: POORU FURANSHISU JIEIKOBUZU , JIYAN RIKUTAA
IPC: B29C67/00 , B29C35/08 , B29K105/24
Abstract: PURPOSE: To reduce a stress crack generated by a heat by emitting a light having a strong chemical action of a spectral range having a narrow wavelength to a partly cured stereoscopic molding, thereby lowering a postcuring temperature to reduce a warp. CONSTITUTION: In the case of selecting a radiation wavelength for curing a photosensitive polymer resin in an optimum state, it is necessary to obtain a terminating end of an absorption curve of a photopolymerization initiator or to position a terminating end curing radiation of a long wavelength not a point that an absorption becomes zero but its near position. For example, in the case of Irgacure 184, it is a wavelength range near 370 nm, in the case of Irgacure 651, a wavelength range near 390 nm, and in the case of other photopolymerization initiator Lucerin normally used for a stereoscopic molding, a wavelength range near 415 nm. Accordingly, an optimum postcuring radiation source radiates most of its output in a narrow limited spectral range with very small absorption of the initiator. A tubular low pressure mercury vapor fluorescent lamp for emitting an ultraviolet radiation (black light) having a long wavelength is ideal here.